PL2248B1 - A method of vulcanizing rubber, rubber and similar materials. - Google Patents

A method of vulcanizing rubber, rubber and similar materials. Download PDF

Info

Publication number
PL2248B1
PL2248B1 PL2248A PL224820A PL2248B1 PL 2248 B1 PL2248 B1 PL 2248B1 PL 2248 A PL2248 A PL 2248A PL 224820 A PL224820 A PL 224820A PL 2248 B1 PL2248 B1 PL 2248B1
Authority
PL
Poland
Prior art keywords
rubber
solution
benzene
similar materials
sulfur dioxide
Prior art date
Application number
PL2248A
Other languages
Polish (pl)
Filing date
Publication date
Application filed filed Critical
Publication of PL2248B1 publication Critical patent/PL2248B1/en

Description

Wynalazek niniejszy dotyczy sposobu wulkanizacji kauczuku, gumy i podobnych materjalów i zwyklego traktowania uprzed¬ niego, polegajacego na niestosowaniu na¬ grzewania (wysokiej temperatury), W mysl wynalazku traktuje sie kauczuk, gume i podobne ciala, w postaci arkuszy lub wsteg (film) lub tez w stanie rozpuszczonym lub pólrozpuszczonym dwutlenkiem siarki oraz siarkowodorem. Kauczuk wchlania oba te gazy, a wzajemne ich oddzialywanie do¬ prowadza do stosunkowo predkiej wulka¬ nizacji nawet w zwyklej temperaturze.Wiadomo, ze dwutlenek siarki i weglowo¬ dór dzialaja na siebie w obecnosci naj¬ mniejszych sladów wilgoci, przyczem wy¬ twarza sie rodzaj alotropowej siarki, róz¬ niacej sie pod wzgledem fizycznych wla¬ snosci od rodzajów, uzywanych zazwyczaj do wulkanizacji kauczuku. Niezaleznie od tego nieznanem bylo wyzyskanie wzajem* nego oddzialywania wspomnianych ga&ów do wulkanizacji kauczuku przy zwyklej temperaturze. Wulkanizacja przy pomocy zwyklych gatunków siarki mozliwa j^st tylko w podwyzszonej temperaturze, gdy tymczasem wytworzona w powyzszy spo¬ sób alotropowa siarka, powstajac we¬ wnatrz samej substancji kauczuku, zdolna jest do laczenia sie z nim w momencie swe¬ go powstawania, t, j, „iii statu nascendi'\ Laczenie to odbywa sie przy zwyklej tem¬ peraturze, wytwarzajac nader skuteczna wulkanizacje. Nie Jest wylaczone, ze po-wstaja przytem uprzednio produkty przej¬ sciowe, jak np. kwas tionowy, biorace u- dzialw procesie przeksztalcania, którego koncowym rezultatem jest zamierzone na- siarkowanie kauczuku. W tym celu wysta¬ wia sie kauczuk przez pewien czas, zalez¬ ny od grubosci arkusza, na dzialanie dWu- tlenku siarki lub atmosfery, ten gaz zawie¬ rajacej, Stan wilgotnosci kauczuku odpo¬ wiada przytem stanowi wilgotnosci powie¬ trza; zawiera tedy kauczuk pewien zasób x wilgoci;; nie,ulega jednak uprzedniemu mo- yw cieniu w- gródku rozpuszczajacym, jak np. w benzolu. Nastepnie wystawia sie wulka¬ nizowany kauczuk na dzialanie siarkowo¬ doru lub atmosfery, nasiaknietej tym ostat¬ nim, w której trzyma sie go az do zaniku zapachu dwutlenku siarki. W razie potrze¬ by mozna powtórzyc kolejno poddawanie przerabianego ciala wplywowi tych dwóch gazów, az do osiagniecia pozadanego stop¬ nia wulkanizacji. Kolejnosc te mozna równiez zmienic traktujac kauczuk z po¬ czatku siarkowodorem, a potem dopiero dwutlenkiem siarki, uprzedniemu jednak sposobowi nalezy sie pierwszenstwo. Wy¬ konanie tego procesu odbywac sie moze w najrozmaitszy sposób, np. przez wysta¬ wienie kauczuku na dzialanie atmosfery, przesyconej dwutlenkiem siarki i przez na¬ stepne pograzenie (zanurzenie) go w roz¬ tworze siarkowodoru w benzolu lub innym srodku rozpuszczajacym. Obydwie te czyn¬ nosci powtarza sie do ukonczenia wulka¬ nizacji. Stosowac je mozna pod zwyklem lub zwiekszonem cisnieniem; kauczuk znaj¬ dowac sie moze w stanie czystym lub z domieszkami, barwnikami i t. d. Jeszcze lepiej dziala powyzszy sposób w razie u- zycia do wulkanizacji kauczuku rozpuszczo¬ nego. Rozczyn kauczuku w benzolu np. nasyca sie czesciowo lub calkowicie dwu¬ tlenkiem siarki wchlanianym wówczas z nadzwyczajna latwoscia. Roztwór podda¬ je sie nastepnie dzialaniu siarkowodoru, w stanie lotnym, albo tez miesza sie go z ta- kimze roztworem, nasyconym czesciowe* lub calkowicie siarkowodorem, albo wresz¬ cie jeszcze prosciej z roztworem siarko¬ wodoru w benzolu. Odwrotnie mozna zmieszac benzolowy roztwór kauczuku, na¬ sycony czesciowo lub calkowicie siarko¬ wodorem, z odpowiednia iloscia roztworu dwutlenku siarki równiez w benzolu lub czems podobnem. W obydwóch wypad¬ kach zwieksza sie stopniowo tezyzna cie¬ czy w zwyklej temperaturze i stosunkowo krótkim czasie, wreszcie zsiada sie ona w galaretowata mase, nie rozpuszczajaca sie wiecej w benzolu i przedstawiajaca zwul- kanizowany (zahartowany) kauczuk. Po wyparowaniu tej masy na powietrzu otrzy¬ muje sie kauczuk w stanie suchym. Teze¬ niu cieczy towarzyszy czesto wydzielanie sie czesci srodka rozpuszczajacego, który odprowadza sie przed poddaniem reszty cieczy wyparowywaniu. Zastosowywane srodki rozpuszczajace wolne mtisza byc od domieszki pyrydyn oraz innych substancyj zasadowych, obecnosc których opóznia proces wulkanizacji. Nastepujace przykla¬ dy pozwalaja orjentowac sie, mniej wiecej, w ilosciowych stosunkach skladników: Przyklad 1. 100 g roztworu benzolo¬ wego, zawierajacego 2,5% surowego kau* czuku, traktuje sie dwutlenkiem siarki, do¬ póki nie nastapi wchloniecie 0,17 g gazu.Takaz ilosc roztworu w tej samej propor¬ cji poddaje sie dzialaniu weglowodoru, przyczem absorbeji ulega 0,2 g tego ga¬ zu. Obydwa roztwory miesza sie z soba, a po stezeniu wyparowywa sie srodek ioz- puszczajacy (benzol).Przyklad II. 100 g 8 procentowego roztworu gniecionego kauczuku w benzolu nasyca sie czesciowo 0,28 g siarkowodo¬ ru, poczem dodaje sie 26,8 g \% roztwo¬ ru dwutlenku siarki w benzolu. Dalszy spo* sób postepowania, jak wyze].Przyklad III. 100 g 12%-ego roz- — 2 —tworu gniecionego kauczuku w benzolu na¬ syca sie siarkowodorem; poczem dodaje sie 40,2 g 1% roztworu dwutlenku siar¬ ki w benzolu lub solventnafcie. Jeden z ga¬ zów, albo i obydwa, mozna równiez wpro¬ wadzac w zwiazek z kauczukiem pod ci¬ snieniem. Stan kauczuku moze byc staly lub rozpuszczony. Wskutek zwiekszonej kon¬ centracji, gaz przenika lepiej kauczuk sta¬ ly; absorbcja jednak odbywa sie szybciej w wypadku rozpuszczonego kauczuku. PL PLThis invention relates to a method for vulcanizing rubber, gum, and similar materials, and to a conventional pretreatment method that involves the absence of heat (high temperature). According to the invention, rubber, gum, and similar materials are treated, in the form of sheets or ribbons (films), or in a dissolved or semi-dissolved state, with sulfur dioxide and hydrogen sulfide. Rubber absorbs both gases, and their interaction leads to relatively rapid vulcanization even at ordinary temperatures. It is known that sulfur dioxide and hydrocarbon interact in the presence of the slightest trace of moisture, producing a type of allotropic sulfur whose physical properties differ from those typically used for rubber vulcanization. Regardless of this, it was unknown to utilize the interaction of the above-mentioned branches to vulcanize rubber at ordinary temperatures. Vulcanization with ordinary grades of sulfur is only possible at elevated temperatures, while the allotropic sulfur produced in this way, being formed within the rubber substance itself, is capable of combining with it at the moment of its formation, i.e., "nascent state." This combination takes place at ordinary temperatures, producing a very effective vulcanization. It is not excluded that intermediate products, such as thionic acid, are formed beforehand, which participate in the transformation process, the final result of which is the intended sulfurization of the rubber. For this purpose, the rubber is exposed for a certain time, depending on the thickness of the sheet, to the action of sulfur dioxide or the atmosphere; this gas contains The rubber's moisture content corresponds to the air humidity; therefore, it contains a certain amount of moisture; however, it is not subjected to prior exposure to a solvent, such as benzene. The vulcanized rubber is then exposed to hydrogen sulfide or an atmosphere saturated with the latter, where it is kept until the odor of sulfur dioxide disappears. If necessary, the treatment of the body under treatment with these two gases can be repeated until the desired degree of vulcanization is achieved. This order can also be changed by treating the rubber first with hydrogen sulfide and then with sulfur dioxide, but the former method is preferred. This process can be carried out in a variety of ways. by exposing the rubber to an atmosphere saturated with sulfur dioxide and then immersing it in a solution of hydrogen sulfide in benzene or another solvent. Both these operations are repeated until the vulcanization is completed. They can be used under normal or increased pressure; the rubber can be in a pure state or with additives, dyes, etc. The above method works even better when dissolved rubber is used for vulcanization. The solution of rubber in benzene, for example, becomes partially or completely saturated with sulfur dioxide, which is then absorbed with extraordinary ease. The solution is then exposed to the action of hydrogen sulfide in the gaseous state, or it is mixed with Such a solution, partially or completely saturated with hydrogen sulfide, or finally, even more simply, with a solution of hydrogen sulfide in benzene. Conversely, one can mix a benzene solution of rubber, partially or completely saturated with hydrogen sulfide, with a corresponding amount of a sulfur dioxide solution also in benzene or something similar. In both cases, the liquid's strength gradually increases at ordinary temperature and in a relatively short time, until it finally solidifies into a gelatinous mass, no longer soluble in benzene and representing vulcanized (hardened) rubber. After evaporation of this mass in air, the rubber is obtained in a dry state. The hardening of the liquid is often accompanied by the release of some of the solvent, which is removed before the rest of the liquid is subjected to the hardening. evaporation. The solvents used must be free from pyridines and other alkaline substances, the presence of which retards the vulcanization process. The following examples provide an approximate guide to the quantitative ratios of the components: Example 1. 100 g of a benzol solution containing 2.5% raw rubber is treated with sulfur dioxide until 0.17 g of the gas is absorbed. An equal amount of the solution is treated with a hydrocarbon in the same proportion, absorbing 0.2 g of this gas. The two solutions are mixed, and after concentrating, the solvent (benzol) is evaporated. Example II. 100 g of an 8% kneaded solution The rubber in benzene is partially saturated with 0.28 g of hydrogen sulfide, then 26.8 g of a 1% solution of sulfur dioxide in benzene is added. The further procedure is as above. Example III. 100 g of a 12% solution of the crushed rubber in benzene is saturated with hydrogen sulfide; then 40.2 g of a 1% solution of sulfur dioxide in benzene or solvent naphtha is added. One or both of the gases can also be introduced into the rubber under pressure. The state of the rubber can be solid or dissolved. Due to the increased concentration, the gas penetrates the solid rubber better; however, absorption takes place faster in the case of dissolved rubber.

PL2248A 1920-10-30 A method of vulcanizing rubber, rubber and similar materials. PL2248B1 (en)