PL32874B1 - A method of decolorizing black or dark sulfuric acid - Google Patents

A method of decolorizing black or dark sulfuric acid Download PDF

Info

Publication number
PL32874B1
PL32874B1 PL32874A PL3287438A PL32874B1 PL 32874 B1 PL32874 B1 PL 32874B1 PL 32874 A PL32874 A PL 32874A PL 3287438 A PL3287438 A PL 3287438A PL 32874 B1 PL32874 B1 PL 32874B1
Authority
PL
Poland
Prior art keywords
acid
sulfuric acid
dark
gases
black
Prior art date
Application number
PL32874A
Other languages
Polish (pl)
Filing date
Publication date
Application filed filed Critical
Publication of PL32874B1 publication Critical patent/PL32874B1/en

Description

Wynalazek dotyczy sposobu odbarwiania czarnego lub ciemnego kwasu siarkowego.Zdarza sie czesto, ze niektórymi sposo¬ bami, zwlaszcza katalicznymi, wytwarza sie kwas siarkowy o bardzo ciemnym za¬ barwieniu, czasami nawet czarnym, np. gdy wytwarza sie go z niektórych gazów, otrzy¬ mywanych przez prazanie rud albo kon¬ centratów, zawierajacych substancje orga¬ niczne, w aparacie Dwight Lloyda lub po¬ dobnym.Zabarwienie to jest niepozadane, ponie¬ waz najwiekszy popyt jest na kwas jasny lub przezroczysty. Próbowano juz odbar¬ wiac zabarwiony kwas przez stosowanie srodków utleniajacych, np. wody utlenio¬ nej, kwasu nadsiarkowego lub nadsiarcza¬ nów, albo Pb02, jednak sposoby te sa kosztowne.Wedlug wynalazku czarny lub ciemny kwas siarkowy odbarwia sie przez dziala¬ nie ciepla.Wedlug jednej z odmian wykonania wy¬ nalazku stosuje sie w tym celu wysoka temperature, a równoczesnie dziala sie SO3 w postaci H2SO4 dymiacego lub w postaci gazowej.W razie ogrzewania czarnego lub ciem¬ nego kwasu siarkowego odbarwianie roz¬ poczyna sie w temperaturze okolo 260° C, a konczy sie w temperaturze okolo 300° C.W tej temperaturze proces odbarwiania trwa w przyblizeniu 90 min.Proces odbarwiania jest wykonywany w dowolnym odpowiednim urzadzeniu, w któ¬ rym kwas moze byc poddawany dzialaniu ciepla lub ciepla i SOs. Urzadzenie takie moze stanowic np. wieza z przegrodami lub ze wsadem z materialu odpornego na dziala¬ nie kwasów, np. z kwarcytu. Urzadzenie takie jest proste' i ekonomiczne, przy czym zbedne jest stosowanie specjalnych odczyn¬ ników.W razie odbarwiania kwasu, otrzymane¬ go z gazów powstalych przy prazeniu rud albo koncentratów w aparacie Dwight Lloyda, korzystne okazalo sie stosowanie temperatur okolo 300° C.W razie wytwarzania kwasu siarkowego sposobem katalitycznym do odbarwiania nadaja sie wedlug wynalazku zwlaszcza gazy bogate w SO3 , otrzymane z katalizy w temperaturze okolo 400° C.Gazy te sa skierowywane do wymienni¬ ka ciepla w celu obnizenia ich temperatu¬ ry do okolo 300° C, a nastepnie sa prowa¬ dzone do urzadzenia, w którym przepro¬ wadza sie odbarwianie (urzadzenia odbar¬ wiajacego) . -. Gazy te moga takze czesciowo omijac wymiennik ciepla, tak iz czesc ga¬ zów goracych skierowuje sie wprost z ka¬ talizy do urzadzenia odbarwiajacego.W znanych urzadzeniach, - stosowanych do katalicznego wytwarzania kwasu siar¬ kowego, gazy musza byc ochlodzone do okolo 60° C przed doprowadzeniem ich do aparatu absorpcyjnego. Po oddaniu w wy¬ mienniku ciepla pewnej ilosci ciepla ga¬ zom, doprowadzanym do komory kataliza- cyjnej, gazy bogate w SOs przeprowadza sie zasadniczo przez chlodnice w celu ochlodzenia ich do okolo 60° C. Jezeli jednak gazy te przeplywaja przez urzadze- ^ nie odbarwiajace wspomniane wyzej, mozna uniknac calkowicie lub co najmniej w cze¬ sci stosowania chlodnicy, poniewaz chlo- PWZG Warszawa, Tamka dzenie odbywa sie w czasie procesu od¬ barwiania.Mozna zastosowac rozmaite srodki w ce¬ lu zapewnienia najkorzystniejszej tempe¬ ratury w czasie odbarwiania.Gazy albo kwas lub gazy i kwas moga byc podgrzewane do pozadanej tempera¬ tury w dowolny znany sposób przed do¬ prowadzeniem ich do urzadzenia, odbarwia¬ jacego, a to badz za pomoca ciepla wywia¬ zywanego na drodze chemicznej w dowol¬ nej chwili procesu, badz przez doprowa¬ dzenie ciepla z zewnatrz.Gazy, kwas surowy i kwas odbarwiony moga byc prowadzone w dowolnych odpo¬ wiednich obiegach.Wynalazek moze byc zastosowany rów¬ niez do odbarwiania za pomoca ciepla, czarnego lub ciemnego kwasu-siarkowego, otrzymanego juz uprzednio. PLThe invention relates to a method of decolorizing black or dark sulfuric acid. It is not uncommon for some methods, especially catalytic ones, to produce sulfuric acid with a very dark color, sometimes even black, e.g. when produced from certain gases, washed by roasting ores or concentrates containing organic substances in a Dwight Lloyd apparatus or the like. This coloration is undesirable since the greatest demand is for light or transparent acid. It has already been attempted to discolor the colored acid by the use of oxidizing agents, for example hydrogen peroxide, persulfuric acid or persulfates, or PbO2, but these methods are expensive. According to the invention, black or dark sulfuric acid is discolored by the action of heat. According to one embodiment of the invention, a high temperature is used for this purpose, and at the same time SO3 is used in the form of fuming or gaseous H2SO4. When black or dark sulfuric acid is heated, the discoloration begins at about 260 ° C. C and ends at a temperature of about 300 ° C. At this temperature, the decolorization process takes approximately 90 minutes. The decolorization process is performed in any suitable equipment where the acid can be subjected to heat or heat and SO2. Such a device may be, for example, a tower with baffles or a charge of acid-resistant material, for example, quartzite. Such a device is simple and economical, with the need to use special reagents. In the event of decolorization of the acid obtained from the gases generated in the calcination of ores or concentrates in the Dwight Lloyd apparatus, it has proven advantageous to use temperatures of about 300 ° C when producing According to the invention, sulfuric acid catalytic decolorization is particularly suitable for gases rich in SO3, obtained from catalysis at a temperature of about 400 ° C. These gases are directed to a heat exchanger in order to lower their temperature to about 300 ° C, and then are led to a device in which the decolorization is carried out (decolorizing device). -. These gases can also partially bypass the heat exchanger, so that some of the hot gases go straight from the catalytic converter to the decolorizing device. In known devices - used for the catalytic production of sulfuric acid, the gases must be cooled to about 60 ° C before feeding them to the absorption apparatus. After a certain amount of heat is transferred to the gases fed to the catalytic chamber, the SO2-rich gases are essentially passed through coolers to cool them down to about 60 ° C. However, if these gases pass through the equipment, Decolorizing mentioned above, can be avoided completely or at least in part of the use of the cooler, because the cooling of PWZG Warszawa, Tamka is done during the dyeing process. Various measures can be used to ensure the most favorable temperature during decolorization The gases or acid or gases and acid may be heated to the desired temperature in any known manner before being fed to the apparatus to discolor, or by means of chemically induced heat at any point in the process. or by applying heat from the outside. The gases, crude acid and decolorized acid may be carried out in any suitable circuits. The invention may also be applied to discoloration. binding with heat, black or dark sulfuric acid obtained previously. PL

Claims (4)

Zastrzezenia patentowe. 1. Sposób _odbarwiania czarnego lub ciemnego kwasu siarkowego, zwlaszcza kwasu siarkowego, otrzymanego sposobem katalitycznym, znamienny tym, ze kwas poddaje sie w wyzszej temperaturze dzia¬ laniu SO3 . Patent claims. A method of decolorizing black or dark sulfuric acid, in particular sulfuric acid, obtained by a catalytic process, characterized in that the acid is subjected to SO3 at a higher temperature. 2. Sposób wedlug zastrz. 1, znamienny tym, ze na kwas dziala sie SO3 w postaci H2SO4 dymiacego. 2. The method according to claim The process of claim 1, characterized in that the acid is treated with SO3 in the form of fuming H2SO4. 3. Sposób wedlug zastrz. 1, znamienny tym, ze na kwas dziala sie SO* w postaci gazowej. 3. The method according to p. A process as claimed in claim 1, characterized in that the acid is treated with SO * in gaseous form. 4. Odmiana sposobu wedlug zastrz. 1, znamienna tym, ze odbarwienie kwasu przeprowadza sie jedynie wskutek dziala¬ nia ciepla, przy czym stosuje sie tempera¬ ture lezaca pomiedzy 260° — 300° C. Societó Generale Metali u rgi- que de Hoboken So ciete Anonym*e Zastepca: inz. F. Winnicki rzecznik patentowy foiRLlOTEKAl J. ISO Zim. 213. B-47896 IBIBL-I^ I lllr»i»du Patentowego! IjoArttief'.^*^ ¦•¦.¦.-¦¦ ¦--¦ PL4. A variant of the method according to claim The method of claim 1, characterized in that the decolorization of the acid is carried out solely by the action of heat, with a temperature between 260 ° - 300 ° C being used. Societó Generale Metali at rgique de Hoboken Societe Anonym * e Deputy: inz F. Winnicki, patent attorney foiRLLOTEKAl J. ISO Zim. 213. B-47896 IBIBL-I ^ IIIr »and» du Patent! IjoArttief '. ^ * ^ ¦ • ¦.¦.-¦¦ ¦ - ¦ PL
PL32874A 1938-11-22 A method of decolorizing black or dark sulfuric acid PL32874B1 (en)