PL398955A1 - Modification of asphalt, a mixture of dicyclopentadiene, styrene, polybutadiene rubber and sulfur - Google Patents

Modification of asphalt, a mixture of dicyclopentadiene, styrene, polybutadiene rubber and sulfur

Info

Publication number
PL398955A1
PL398955A1 PL398955A PL39895512A PL398955A1 PL 398955 A1 PL398955 A1 PL 398955A1 PL 398955 A PL398955 A PL 398955A PL 39895512 A PL39895512 A PL 39895512A PL 398955 A1 PL398955 A1 PL 398955A1
Authority
PL
Poland
Prior art keywords
mixture
asphalt
dicyclopentadiene
styrene
sulfur
Prior art date
Application number
PL398955A
Other languages
Polish (pl)
Other versions
PL221759B1 (en
Inventor
Lucjan Pawlowski
Tadeusz Matynia
Original Assignee
Politechnika Lubelska
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Politechnika Lubelska filed Critical Politechnika Lubelska
Priority to PL398955A priority Critical patent/PL221759B1/en
Publication of PL398955A1 publication Critical patent/PL398955A1/en
Publication of PL221759B1 publication Critical patent/PL221759B1/en

Abstract

Sposób modyfikacji asfaltu mieszanina dicyklopentadienu, styrenu, kauczuku polibutadienowego i siarki charakteryzuje sie tym, ze mieszanine zawierajaca 1.37% dicyklopentadienu, 75,74% styrenu, 18,43% kauczuku polibutadienowego i 2,57% siarki wygrzewa sie przez okres 5 godzin w temperaturze 40°C, po czym dozuje sie porcjami intensywnie mieszajac do asfaltu 50/70 rozgrzanego do temperatury 140°C w ilosci 3% mieszaniny w stosunku do asfaltu 50/70. Nastepnie mieszanine wygrzewa sie przez 20 godzin w temperaturze 140°C.The asphalt modification method, a mixture of dicyclopentadiene, styrene, polybutadiene rubber and sulfur, is characterized by the fact that the mixture containing 1.37% dicyclopentadiene, 75.74% styrene, 18.43% polybutadiene rubber and 2.57% sulfur is heated for 5 hours at 40 ° C, after which it is dosed in portions, intensively mixing into asphalt 50/70 heated to 140 ° C in an amount of 3% of the mixture in relation to asphalt 50/70. The mixture is then heated for 20 hours at 140 ° C.

PL398955A 2012-04-24 2012-04-24 Method for modifying bitumen mixture of dicyclopentadiene and styrene, polybutadiene rubber and sulfur PL221759B1 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
PL398955A PL221759B1 (en) 2012-04-24 2012-04-24 Method for modifying bitumen mixture of dicyclopentadiene and styrene, polybutadiene rubber and sulfur

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
PL398955A PL221759B1 (en) 2012-04-24 2012-04-24 Method for modifying bitumen mixture of dicyclopentadiene and styrene, polybutadiene rubber and sulfur

Publications (2)

Publication Number Publication Date
PL398955A1 true PL398955A1 (en) 2013-10-28
PL221759B1 PL221759B1 (en) 2016-05-31

Family

ID=49449307

Family Applications (1)

Application Number Title Priority Date Filing Date
PL398955A PL221759B1 (en) 2012-04-24 2012-04-24 Method for modifying bitumen mixture of dicyclopentadiene and styrene, polybutadiene rubber and sulfur

Country Status (1)

Country Link
PL (1) PL221759B1 (en)

Also Published As

Publication number Publication date
PL221759B1 (en) 2016-05-31

Similar Documents

Publication Publication Date Title
EP2960294A4 (en) Novel highly viscoelastic warm mix modifier composition and preparation method therefor, and new and regenerated warm mix modified asphalt concrete mixture composition and preparation method therefor
IL257164A (en) Glucocorticoid compositions for use in treating adverse effects caused by cd3 specific binding domains
BR112014008233A2 (en) crosslinkable composition, part kit, one-component uses, a coating additive mixture, and a cross-linking composition, rma coating additive mixture, and, coating composition
PH12016500611A1 (en) Compositions useful for treating disorders related to kit
IL229090A0 (en) Rubber mixtures containing silicic acid and sulfur containing additives
IL243645A0 (en) Compositions, methods and kits for diagnosing and treating cd206 expressing cell-related disorders
BR112016016400A2 (en) COMPOSITIONS OF CHIRALLY CONTROLLED OLIGONUCLEOTIDES, THEIR USE, THEIR PHARMACEUTICAL COMPOSITION, AND METHODS
SMT201900362T1 (en) Method for repair of ligament or tendon
MX366318B (en) Heterocycle amines and uses thereof.
PH12015500210A1 (en) Demulsifying compositions and methods of use
BR112013007418A2 (en) hydrated cement products for pulverized concrete
FR2993889B1 (en) THERMO-EXPANSIBLE RUBBER COMPOSITION FOR PNEUMATIC
EP2772513A4 (en) MODIFIED MASKING RUBBER MIXTURE, RUBBER COMPOSITION PREPARED THEREWITH, AND VULCANIZED RUBBER AND METHOD FOR PREPARING THE SAME
BR112013030113A2 (en) asphalt composition, processes for making an asphalt composition and for preparing an asphalt pavement, and sulfur globule
MX2018005343A (en) Improved method of making a mercury sorbent.
IN2014KN01158A (en)
SG11202012660QA (en) Asphalt mixture composition comprising digestate additive
EP2832823A4 (en) PROCESS FOR MIXING COAL, MIXED COAL AND PROCESS FOR PRODUCING COKE
HUE038423T2 (en) Compounds, compositions and methods using e-selectin antagonists for mobilization of hematopoietic cells
SG11201402730TA (en) Amine based additive composition for control and inhibition of polymerization of styrene, and method of use thereof
EP3029148A4 (en) Method for determining nucleic acid composition of nucleic acid mixture
BR112014012561A2 (en) amine mixture, process for preparing an amine mixture, fuel composition, and use of an amine mixture
EA201201633A1 (en) METHOD FOR PROVIDING LOW HS ALLOCATION DURING SEROASPHALT RECEIVING
BR112015027990A2 (en) method for producing component with a predetermined level of brightness
IN2015DN01221A (en)