PL414306A1 - Method for reducing outer diameter of tube semi-finished products - Google Patents
Method for reducing outer diameter of tube semi-finished productsInfo
- Publication number
- PL414306A1 PL414306A1 PL414306A PL41430615A PL414306A1 PL 414306 A1 PL414306 A1 PL 414306A1 PL 414306 A PL414306 A PL 414306A PL 41430615 A PL41430615 A PL 41430615A PL 414306 A1 PL414306 A1 PL 414306A1
- Authority
- PL
- Poland
- Prior art keywords
- blank
- rollers
- outer diameter
- roller
- axis
- Prior art date
Abstract
Sposób redukcji średnicy zewnętrznej półfabrykatów rurowych, zwłaszcza skrajnych końców półfabrykatów rurowych charakteryzuje się tym, że półfabrykat (7) w kształcie odcinka tulei umieszcza się jednym końcem w otworze (5) uchwytu (4) podającego, który ma możliwość swobodnego obrotu dookoła własnej osi, następnie wprowadza się drugi koniec półfabrykatu (7) między trzy jednakowe walce (1a), (1b) i (1c), zaś położenie osiowe półfabrykatu (7) ustala się przy pomocy zderzaka (6), następnie wprawia się dwa walce (1a) i (1c) w ruch obrotowy w tym samym kierunku i ze stałą prędkością (n), która wynosi 30 obr/min, po czym wycofuje się zderzak (6) z przestrzeni roboczej walców (1a), (1b) i (1c) i wprawia się w ruch postępowy walec (1b), który przemieszcza się ze stałą prędkością, która wynosi 1 mm/s w kierunku osi półfabrykatu (7), przy czym walec (1b) ma możliwość swobodnego obrotu dookoła własnej osi, następnie oddziaływuje się na półfabrykat (7) powierzchniami (3a), (3b) i (3c) kształtującymi, które znajdują się na walcach (1a), (1b) i (1c) i wprawia się półfabrykat (7) w ruch obrotowy (n1) w kierunku przeciwnym do kierunku obrotów walców (1a) i (1c), jednocześnie wprawia się w ruch obrotowy walec (1b), który obracany jest w tym samym kierunku i z tą samą prędkością co walce (1a) i (1b).The method of reducing the outer diameter of pipe blanks, especially the extreme ends of pipe blanks is characterized by the fact that the blank (7) in the shape of a sleeve section is placed with one end in the hole (5) of the feed holder (4), which can be freely rotated around its axis, then the other end of the blank (7) is inserted between three identical rollers (1a), (1b) and (1c), and the axial position of the blank (7) is determined by means of a stop (6), then two rollers (1a) and ( 1c) in rotational motion in the same direction and with a constant speed (n), which is 30 rpm, after which the bumper (6) retracts from the working space of the rollers (1a), (1b) and (1c) and is put in in a forward motion, a roller (1b) that moves at a constant speed of 1 mm / s in the direction of the blank axis (7), whereby the roller (1b) can rotate freely around its axis, then it interacts on the blank (7) with the shaping surfaces (3a), (3b) and (3c) that are on the rollers (1a), (1b) and (1c) and the blank (7) is put into rotation (n1) in the direction opposite to the direction of rotation of the rollers (1a) and (1c), the roller (1b) is simultaneously rotated, which is rotated in the same direction and at the same speed as the rollers (1a) and (1b).
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| PL414306A PL226885B1 (en) | 2015-10-07 | 2015-10-07 | Method for reducing outer diameter of tube semi-finished products |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| PL414306A PL226885B1 (en) | 2015-10-07 | 2015-10-07 | Method for reducing outer diameter of tube semi-finished products |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| PL414306A1 true PL414306A1 (en) | 2016-12-19 |
| PL226885B1 PL226885B1 (en) | 2017-09-29 |
Family
ID=57542540
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| PL414306A PL226885B1 (en) | 2015-10-07 | 2015-10-07 | Method for reducing outer diameter of tube semi-finished products |
Country Status (1)
| Country | Link |
|---|---|
| PL (1) | PL226885B1 (en) |
-
2015
- 2015-10-07 PL PL414306A patent/PL226885B1/en unknown
Also Published As
| Publication number | Publication date |
|---|---|
| PL226885B1 (en) | 2017-09-29 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CL2014001453A1 (en) | Rock drilling machine comprises a body, a rod mounted to the body by means of a first bearing with a first end with connecting members for a drilling tool, and a lubrication system for a gear system; lubrication method of a rock drilling machine. | |
| MX376809B (en) | LIGHTWEIGHT VARIABLE WALL PROPELLER SHAFT WITH AN INTEGRAL FLANGE MEMBER AND METHOD OF MAKING THE SAME. | |
| MX360903B (en) | Continuous heating device for coil springs and heating method for coil springs using the same device. | |
| EA201891118A1 (en) | TURNING DEVICE FOR KNITTED TUBULAR PRODUCTS, IN PARTICULAR TO REVERSIBLE TUBULAR PRODUCTS WITH POCKETS, WHICH SPEECH FROM THEIR SIDE SURFACE | |
| MX2016013139A (en) | METHOD OF FORMING A LIGHT WEIGHT VARIABLE WALL DRIVE SHAFT WITH FRICTION WELDED FLANGE. | |
| PL414306A1 (en) | Method for reducing outer diameter of tube semi-finished products | |
| MX2018005723A (en) | Running tool for use with bearing assembly. | |
| PL398427A1 (en) | Method for transverse rolling of forgings with axial movement of the charge | |
| RU2013118885A (en) | METHOD FOR PRODUCING SLIDING BEARING | |
| PL404294A1 (en) | Method for the rotatry pushing with adjustable wheel base of graded axisymmetric forgings | |
| MX391022B (en) | CHUCK DEVICE. | |
| MX2016005075A (en) | CARVING TOOL. | |
| MY190259A (en) | Conveyor roll assembly, torque transmission and support means and process for making a conveyor roll assembly used in a high temperature environment | |
| PL405864A1 (en) | Method for reducing hollow forgings | |
| PL423886A1 (en) | Method for skew rolling of ball forgings | |
| PL398592A1 (en) | Method for turnover crimping with internal threads | |
| PL403064A1 (en) | Method and a device for forming hollow forging balls | |
| PL403063A1 (en) | Method and a device for forming hollow forging balls in single formation | |
| RU2015105761A (en) | INTERNAL SURFACE ADJUSTMENT TOOL, CORRECTION, BAR, HOT ROLLING, PRESS-ROLLING BROADCASTING MACHINE AND DRINKING MACHINE | |
| PL402213A1 (en) | The way of shaping hollow forgings | |
| DK3676495T3 (en) | Manufacturing method, piston blank, piston and axial piston machine with piston | |
| PL404614A1 (en) | The method of extruding the outer and inner collar | |
| WO2015044825A3 (en) | Anti-friction device of drilling elements | |
| PL398722A1 (en) | Rotary crimping method with four rolls of products with internal threads | |
| PL398724A1 (en) | Rotary crimping method with three rolls of products with internal threads |