PL417135A1 - Method for producing porous carbon matrix with increased oxygen and nitrogen content - Google Patents
Method for producing porous carbon matrix with increased oxygen and nitrogen contentInfo
- Publication number
- PL417135A1 PL417135A1 PL417135A PL41713516A PL417135A1 PL 417135 A1 PL417135 A1 PL 417135A1 PL 417135 A PL417135 A PL 417135A PL 41713516 A PL41713516 A PL 41713516A PL 417135 A1 PL417135 A1 PL 417135A1
- Authority
- PL
- Poland
- Prior art keywords
- porous carbon
- inorganic
- range
- temperature
- carbon matrix
- Prior art date
Abstract
Przedmiotem zgłoszenia jest sposób wytwarzania porowatych matryc węglowych, który charakteryzuje się tym, że surowiec organiczny stanowią suche lub mokre zielenice albo ich wytłoczyny, a surowcem nieorganicznym są węglany nieorganiczne rozdrobnione do ziaren o rozmiarach nanometrycznych, które mieszane są w przeliczeniu na suchą masę w stosunku wagowym w zakresie od 1 : 4 do 4 : 1, homogenizuje mechanicznie, podgrzewa z szybkością od 5°C/min do 15°C/min w atmosferze gazu obojętnego, a termolizę w warunkach beztlenowych prowadzi się w zakresie temperatur od 600°C do 900°C przez okres od 30 minut do 120 minut, po czym schładza do temperatury około 50°C, utrzymując atmosferę beztlenową, a następnie uzyskany produkt w postaci nieporowatej matrycy węglowej, zawierającej azot i tlen, poddaje się działaniu kwasów nieorganicznych lub organicznych, w celu usunięcia składnika nieorganicznego, po czym płucze wodą demineralizowaną do uzyskania wartości pH odcieku w zakresie od 6 do 7, a następnie suszy przez okres od 12 godzin do 24 godzin w temperaturze od 70°C do 100°C.The subject of the application is a method of producing porous carbon matrices, which is characterized by the fact that the organic raw material is dry or wet green algae or their pomace, and the inorganic raw material is inorganic carbonates comminuted to grains of nanometric size, which are mixed on a dry weight basis. in the range of 1: 4 to 4: 1, mechanically homogenizes, heats at a rate of 5 ° C / min to 15 ° C / min in an inert gas atmosphere, and thermolysis under anaerobic conditions is carried out in the temperature range from 600 ° C to 900 ° C for a period of 30 minutes to 120 minutes, after which it is cooled to a temperature of about 50 ° C, maintaining an anaerobic atmosphere, and then the resulting product in the form of a non-porous carbon matrix containing nitrogen and oxygen is subjected to inorganic or organic acids in order to remove the inorganic component, then rinse with demineralized water to obtain a pH value of about drip in the range of 6 to 7, and then dried for a period of 12 hours to 24 hours at a temperature of 70 ° C to 100 ° C.
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| PL417135A PL417135A1 (en) | 2016-05-09 | 2016-05-09 | Method for producing porous carbon matrix with increased oxygen and nitrogen content |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| PL417135A PL417135A1 (en) | 2016-05-09 | 2016-05-09 | Method for producing porous carbon matrix with increased oxygen and nitrogen content |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| PL417135A1 true PL417135A1 (en) | 2017-11-20 |
Family
ID=60324379
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| PL417135A PL417135A1 (en) | 2016-05-09 | 2016-05-09 | Method for producing porous carbon matrix with increased oxygen and nitrogen content |
Country Status (1)
| Country | Link |
|---|---|
| PL (1) | PL417135A1 (en) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| PL427144A1 (en) * | 2018-09-20 | 2019-03-25 | Uniwersytet Mikołaja Kopernika W Toruniu | Method for obtaining hybrid carbon materials containing oligoheterocyclic compounds |
-
2016
- 2016-05-09 PL PL417135A patent/PL417135A1/en unknown
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| PL427144A1 (en) * | 2018-09-20 | 2019-03-25 | Uniwersytet Mikołaja Kopernika W Toruniu | Method for obtaining hybrid carbon materials containing oligoheterocyclic compounds |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| AR084267A1 (en) | PROCEDURE FOR THE MANUFACTURE OF SYNTHETIC POZZOLANO | |
| JP2016505481A5 (en) | ||
| JP2016165283A5 (en) | ||
| AR078966A1 (en) | METHOD OF ELABORATION OF LITHIUM ADSORBENT AND LITHIUM ADSORBENT, RAW MATERIAL FOR LITHIUM ADSORBENT, LITHIUM CONCENTRATION METHOD AND LITHIUM CONCENTRATOR EQUIPMENT | |
| MX2016000660A (en) | Process for preparing torrefied biomass material using a combustible liquid. | |
| CN104085023A (en) | Mould-proof moth-proof process of bamboo chip | |
| PL1890709T3 (en) | Production of glucosamine from plant species | |
| SG11201809367YA (en) | Method for preserving raw meat | |
| PL417135A1 (en) | Method for producing porous carbon matrix with increased oxygen and nitrogen content | |
| LT2014110A (en) | Fermented feed of plant origin | |
| MX2015014207A (en) | Method of processing a grain product. | |
| PL417441A1 (en) | Method for obtaining hybrid carbon-nitrogen materials with developed porous structure | |
| RU2010143994A (en) | METHOD FOR PRODUCING ACTIVATED COAL | |
| IL186648A (en) | Production of glucosamine from plant species | |
| MX2021009643A (en) | Method for obtaining a modified collagen absorbent product from leather. | |
| PH12019500087A1 (en) | Absorbent products and methods for producing the same | |
| Weischedel et al. | Formation of substituted 2-iminooxazolidines via intermolecular 1, 2-addition/intramolecular N-vinylation using 3-substituted-2-bromo-2-propen-1-ols as substrates | |
| RU2013105295A (en) | METHOD FOR PRODUCING MALT | |
| LV14647A (en) | Method for producing biologically active humic product | |
| CN103637227A (en) | Method for processing preserved meat by utilizing solar energy and roast smoking | |
| CN102786291A (en) | Diatomite breathing brick and production method thereof | |
| CN103803982A (en) | Preparation method of rice hull stacked porous silicon carbide | |
| PL428296A1 (en) | Method for obtaining bio-coal with high nitrogen content and the bio-coal obtained with this method | |
| EA201400947A1 (en) | METHOD OF MANUFACTURE OF DRIED YEAST | |
| JP2019519230A5 (en) |