PL421065A1 - Sposób wytwarzania belki podsuwnicowej oraz belka podsuwnicowa - Google Patents
Sposób wytwarzania belki podsuwnicowej oraz belka podsuwnicowaInfo
- Publication number
- PL421065A1 PL421065A1 PL421065A PL42106517A PL421065A1 PL 421065 A1 PL421065 A1 PL 421065A1 PL 421065 A PL421065 A PL 421065A PL 42106517 A PL42106517 A PL 42106517A PL 421065 A1 PL421065 A1 PL 421065A1
- Authority
- PL
- Poland
- Prior art keywords
- welding
- pulse
- crane beam
- flange
- trapezoidal
- Prior art date
Abstract
Sposób wytwarzania belki podsuwnicowej, obejmujący etapy, w których kolejno projektuje się belkę podsuwnicową zawierającą trapezowy środnik połączony z dolną półką i górną półką w kształcie ceownika połączonego z torowiskiem, po czym kształtuje się z arkuszy blachy środnik i ceownik, a następnie spawa się elementy ze sobą, charakteryzuje się tym, że: na stole spawalniczym unieruchamia się elementy względem siebie; skanuje się linie styku średnika (3) z półką górną (1) i półką dolną (2) na całej długości belki podsuwnicowej; spawa się metodą spawania impulsowego środnik (3) z półką górną (1) i półką dolną (2) wzdłuż odczytanych linii styku w jednym przebiegu na całej długości belki podsuwnicowej; wykonuje się metodą spawania impulsowego spoiny doczołowe łączące średniki (3) trapezowe; spawa się metodą spawania impulsowego torowisko (4) do półki górnej (1) belki w jednym przebiegu na całej długości belki podsuwnicowej; przy czym spawanie metodą spawania impulsowego prowadzi się stosując podwójne impulsy o zmiennej wartości prądu, tak że do linii łączenia elementów zbliża się materiał dodatkowy w postaci drutu i generuje się impuls zasadniczy o natężeniu od 490 A do 520 A, powodując upłynnienie metalu spawanych powierzchni i drutu, po czym po opadnięciu impulsu zasadniczego generuje się impuls pomocniczy, o natężeniu prądu mniejszym od wartości natężenia dla impulsu zasadniczego i wartości 360 A do 380 A, powodując ustabilizowanie jeziorka i powstanie spoiny, przy czym jeden cykl pracy obejmujący impuls zasadniczy i pomocniczy trwa (t1) 6 ms.
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| PL421065A PL232084B1 (pl) | 2017-03-30 | 2017-03-30 | Sposób wytwarzania belki podsuwnicowej oraz belka podsuwnicowa |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| PL421065A PL232084B1 (pl) | 2017-03-30 | 2017-03-30 | Sposób wytwarzania belki podsuwnicowej oraz belka podsuwnicowa |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| PL421065A1 true PL421065A1 (pl) | 2018-10-08 |
| PL232084B1 PL232084B1 (pl) | 2019-05-31 |
Family
ID=63688036
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| PL421065A PL232084B1 (pl) | 2017-03-30 | 2017-03-30 | Sposób wytwarzania belki podsuwnicowej oraz belka podsuwnicowa |
Country Status (1)
| Country | Link |
|---|---|
| PL (1) | PL232084B1 (pl) |
-
2017
- 2017-03-30 PL PL421065A patent/PL232084B1/pl unknown
Also Published As
| Publication number | Publication date |
|---|---|
| PL232084B1 (pl) | 2019-05-31 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| DE50100196D1 (de) | Schweissvorrichtung und Verfahren zum Längsverschweissen von aus metallischem Bandmaterial geformten Profilen | |
| MX374509B (es) | Métodos para unir dos piezas de partida y piezas de partida y productos obtenidos | |
| RU2019144109A (ru) | Способ соединения двух заготовок, заготовки и полученные продукты | |
| CN102773590B (zh) | 一种小截面方形大梁及其焊接工艺 | |
| Huilin et al. | Automatic welding technologies for long-distance pipelines by use of all-position self-shielded flux cored wires | |
| EP4090492C0 (de) | Verfahren zum stumpfschweissen von wenigstens zwei blechen | |
| PL421065A1 (pl) | Sposób wytwarzania belki podsuwnicowej oraz belka podsuwnicowa | |
| CN104607785B (zh) | 一种箱型梁焊接方法 | |
| CN102528241A (zh) | 一种高强度钢液压支架构件的焊接方法 | |
| HRP20161276T1 (hr) | Postupak i uređaj za proizvodnju podmetača s dvostrukim šipkama | |
| MX2022002006A (es) | Tecnica de modificacion previa a la soldadura para una pieza en bruto soldada a medida. | |
| CN205834537U (zh) | 一种龙门式焊接装置 | |
| US1161419A (en) | Method of welding. | |
| JP6098771B1 (ja) | 多電極サブマージアーク溶接方法および溶接継手の製造方法 | |
| Anant et al. | Advancement in narrow gap GMA weld joint of thick section of austenitic stainless steel to HSLA steel | |
| Anant et al. | Experimental investigation on transverse shrinkage stress and distortion of extra narrow and conventional gap dissimilar butt joint of austenitic stainless steel to low alloy steel | |
| US388245A (en) | Otohlas benabdos | |
| CN204545706U (zh) | 能防止焊缝下凹的激光焊焊接装置 | |
| RU2674049C1 (ru) | Способ изготовления сварных конструкций | |
| RU2442679C1 (ru) | Способ двусторонней дуговой сварки | |
| CN104227249A (zh) | 衬套自动焊接机的激光头上下位置微调机构 | |
| SU133574A1 (ru) | Трехгранна кранова стрела решетчатого типа | |
| CN102500934A (zh) | 激光自动断丝的工艺方法 | |
| CN110508926B (zh) | 一种激光-mig复合焊接的方法 | |
| KR101359234B1 (ko) | 다전극 서브머지드 아크용접장치 |