PL422203A1 - Method for producing graphene/CoFe2O4 nanocomposite - Google Patents

Method for producing graphene/CoFe2O4 nanocomposite

Info

Publication number
PL422203A1
PL422203A1 PL422203A PL42220317A PL422203A1 PL 422203 A1 PL422203 A1 PL 422203A1 PL 422203 A PL422203 A PL 422203A PL 42220317 A PL42220317 A PL 42220317A PL 422203 A1 PL422203 A1 PL 422203A1
Authority
PL
Poland
Prior art keywords
cofe2o4
nanocomposite
producing graphene
mixture
graphene
Prior art date
Application number
PL422203A
Other languages
Polish (pl)
Other versions
PL232378B1 (en
Inventor
Anna Jędrzejewska
Daniel Sibera
Roman Jędrzejewski
Original Assignee
Zachodniopomorski Uniwersytet Technologiczny W Szczecinie
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zachodniopomorski Uniwersytet Technologiczny W Szczecinie filed Critical Zachodniopomorski Uniwersytet Technologiczny W Szczecinie
Priority to PL422203A priority Critical patent/PL232378B1/en
Publication of PL422203A1 publication Critical patent/PL422203A1/en
Publication of PL232378B1 publication Critical patent/PL232378B1/en

Abstract

Przedmiotem zgłoszenia jest sposób otrzymywania kompozytu grafen/CoFe2O4, polegający na przygotowaniu mieszaniny tlenku grafenu, azotanu żelaza III, azotanu kobaltu, wody amoniakalnej, etanolu i poddaniu jej obróbce ciśnieniowej. Sposób ten charakteryzuje się tym, że mieszaninę poddaje się obróbce ciśnieniowej w solwotermalnym reaktorze mikrofalowym, przez czas od 5 do 45 minut przy ciśnieniu od 4 do 6 MPa, następnie otrzymany materiał płucze się wodą destylowaną i suszy.The subject of the application is a method for obtaining the graphene / CoFe2O4 composite, consisting in the preparation of a mixture of graphene oxide, iron III nitrate, cobalt nitrate, ammonia water, ethanol and subjecting it to pressure treatment. This method is characterized in that the mixture is subjected to pressure treatment in a solvothermal microwave reactor for a period of 5 to 45 minutes at a pressure of 4 to 6 MPa, then the resulting material is washed with distilled water and dried.

PL422203A 2017-07-13 2017-07-13 Method for producing graphene/CoFe2O4 nanocomposite PL232378B1 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
PL422203A PL232378B1 (en) 2017-07-13 2017-07-13 Method for producing graphene/CoFe2O4 nanocomposite

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
PL422203A PL232378B1 (en) 2017-07-13 2017-07-13 Method for producing graphene/CoFe2O4 nanocomposite

Publications (2)

Publication Number Publication Date
PL422203A1 true PL422203A1 (en) 2019-01-14
PL232378B1 PL232378B1 (en) 2019-06-28

Family

ID=64958891

Family Applications (1)

Application Number Title Priority Date Filing Date
PL422203A PL232378B1 (en) 2017-07-13 2017-07-13 Method for producing graphene/CoFe2O4 nanocomposite

Country Status (1)

Country Link
PL (1) PL232378B1 (en)

Also Published As

Publication number Publication date
PL232378B1 (en) 2019-06-28

Similar Documents

Publication Publication Date Title
MX2025015455A (en) Biological methods for preparing terpenes
WO2016072622A3 (en) Cement-free accelerating admixture and cement-free composition including same
MY175115A (en) A near-infrared ray shielding film and a method thereof
IN2015DN02883A (en)
MY176581A (en) Molybdenum-silicon-boron alloy and method for producing same, and component
MX2015010429A (en) Cetuximab with modified glycosylation and uses thereof.
MX2014006802A (en) Percolated mullite and a method of forming same.
GB2567365A (en) Tampon
Schlemmer et al. The current density in quantum electrodynamics in external potentials
EA201992846A1 (en) METHOD FOR PRODUCING COMPOSITE PARTICLES AND INSULATION MATERIAL FOR THE PRODUCTION OF INSULATION PRODUCTS FOR THE INDUSTRY OF CONSTRUCTION MATERIALS, AND ALSO RELEVANT APPLICATION
MY201490A (en) Catalyst, method for producing catalyst, and method for producing acrylonitrile
PL422203A1 (en) Method for producing graphene/CoFe2O4 nanocomposite
PL423318A1 (en) Method for producing graphene/NiFe2O4 nanocomposite
PH12020550834A1 (en) Fermented soybean composition and method for producing fermented soybean composition
PL427390A1 (en) Method of producing graphene/MnFe<sub>2</sub>O<sub>4</sub> <sub> </sub> nanocomposite
FI20125414L (en) Filter bag, method of its manufacture and use
PL405829A1 (en) Concrete with enhanced strength parameters and method of its manufacturing
MD712Y (en) Process for producing MoO3 nanostructures
PL422184A1 (en) Meat product and method for producing it
MX2015009868A (en) Process of manufacturing of soft magnetic ceramic and its use.
RU2013154150A (en) METHOD FOR PRODUCING DECORATIVE PASTE
MX2015001221A (en) Process for obtaining a repellent against snakes, vermins and other animals.
RU2013115568A (en) SYNTHETIC RADIOACTIVE NANODIAMOND AND METHOD OF ITS PRODUCTION
UA75922U (en) METHOD OF OBTAINING Tincture from Livestock Roots
Gadakh Amrutvahini Sheti & Shikshan Vikas Sanstha's