PL445497A1 - Sposób wytwarzania siarczanu(VI) magnezu - Google Patents
Sposób wytwarzania siarczanu(VI) magnezuInfo
- Publication number
- PL445497A1 PL445497A1 PL445497A PL44549723A PL445497A1 PL 445497 A1 PL445497 A1 PL 445497A1 PL 445497 A PL445497 A PL 445497A PL 44549723 A PL44549723 A PL 44549723A PL 445497 A1 PL445497 A1 PL 445497A1
- Authority
- PL
- Poland
- Prior art keywords
- aqueous solution
- magnesium sulphate
- concentration
- weight
- producing magnesium
- Prior art date
Abstract
Zgłoszenie dotyczy sposobu wytwarzaniu siarczan(VI) magnezu, który polega na tym, że w pierwszym etapie wodny roztwór chlorku magnezu o stężeniu 9,7% - 25% mas. i temperaturze 25° - 40°C wprowadza się do kolumny wypełnionej żywicą jonowymienną z objętościowym natężeniem przepływu wynoszącym 10 - 30 cm3 • min-1 otrzymując odciek, będący wodnym roztworem kwasu chlorowodorowego, następnie do kolumny wypełnionej żywicą jonowymienną wprowadza się wodny roztwór kwasu siarkowego(VI) o stężeniu 10% - 20% mas. i temperaturze 20°C - 30°C z objętościowym natężeniem przepływu wynoszącym 15 - 20 cm3 • min-1, otrzymując odciek, stanowiący wodny roztwór siarczanu(VI) magnezu o stężeniu 9% - 20% mas.
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| PL445497A PL248273B1 (pl) | 2023-07-06 | 2023-07-06 | Sposób wytwarzania siarczanu(VI) magnezu |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| PL445497A PL248273B1 (pl) | 2023-07-06 | 2023-07-06 | Sposób wytwarzania siarczanu(VI) magnezu |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| PL445497A1 true PL445497A1 (pl) | 2025-01-07 |
| PL248273B1 PL248273B1 (pl) | 2025-11-17 |
Family
ID=94174490
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| PL445497A PL248273B1 (pl) | 2023-07-06 | 2023-07-06 | Sposób wytwarzania siarczanu(VI) magnezu |
Country Status (1)
| Country | Link |
|---|---|
| PL (1) | PL248273B1 (pl) |
Citations (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CA1177467A (en) * | 1981-06-22 | 1984-11-06 | Solon G. Whitney | Method of selectively removing adsorbed calcium and magnesium from cation exchange resins |
| CN102320636A (zh) * | 2011-08-31 | 2012-01-18 | 四川宜宾县天源离子交换树脂厂 | 利用阳离子交换树脂生产中废硫酸生产7水硫酸镁的方法 |
| PL219041B1 (pl) * | 2012-02-06 | 2015-03-31 | Zakłady Chemiczne Alwernia Spółka Akcyjna | Sposób wytwarzania granulowanego nawozowego siarczanu magnezowego |
| CN105819474A (zh) * | 2016-03-30 | 2016-08-03 | 安徽三星树脂科技有限公司 | 利用阳树脂生产过程中产生的废酸生产硫酸镁的方法 |
-
2023
- 2023-07-06 PL PL445497A patent/PL248273B1/pl unknown
Patent Citations (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CA1177467A (en) * | 1981-06-22 | 1984-11-06 | Solon G. Whitney | Method of selectively removing adsorbed calcium and magnesium from cation exchange resins |
| CN102320636A (zh) * | 2011-08-31 | 2012-01-18 | 四川宜宾县天源离子交换树脂厂 | 利用阳离子交换树脂生产中废硫酸生产7水硫酸镁的方法 |
| PL219041B1 (pl) * | 2012-02-06 | 2015-03-31 | Zakłady Chemiczne Alwernia Spółka Akcyjna | Sposób wytwarzania granulowanego nawozowego siarczanu magnezowego |
| CN105819474A (zh) * | 2016-03-30 | 2016-08-03 | 安徽三星树脂科技有限公司 | 利用阳树脂生产过程中产生的废酸生产硫酸镁的方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| PL248273B1 (pl) | 2025-11-17 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| BR0302812A (pt) | Método para produção de ácido acrìlico | |
| CN106745822B (zh) | 一种基于呼吸图谱判别活性污泥微生物休眠与流失的方法 | |
| RU2008102657A (ru) | Искусственный физиологический солевой раствор и производственный способ его получения | |
| WO2002057185A3 (en) | Process for producing potassium sulfate from sodium sulfate | |
| CN105152327B (zh) | 具有羟基磷灰石内核的厌氧氨氧化颗粒污泥的培养方法 | |
| CN102556972A (zh) | 利用富含Br-的工业废水提取溴素的方法 | |
| CN106348427B (zh) | 一种基于呼吸图谱评估活性污泥是否适应新环境的方法 | |
| PL445497A1 (pl) | Sposób wytwarzania siarczanu(VI) magnezu | |
| CN107254315A (zh) | 六价铬污染土壤的多级还原稳定化药剂及其使用方法 | |
| CN103114281B (zh) | 一种不含铬的钝化液 | |
| WO2005060523A8 (en) | Process for making nickel hydroxide | |
| BRPI0705682A (pt) | método para produzir ácido metacrìlico | |
| CN107236057A (zh) | 一种获得达肝素钠的降解方法 | |
| PL445498A1 (pl) | Sposób wytwarzania siarczanu(VI) potasu i chlorku magnezu z wykorzystaniem procesu podwójnej wymiany jonowej | |
| CN112142202A (zh) | 一体式半硝化-厌氧氨氧化反应器脱氮处理污水方法 | |
| CN108360014A (zh) | 一种次氯酸盐的现场制备方法 | |
| CN103130671B (zh) | 一种清洁的甲基丙烯酰胺的制备和提纯方法 | |
| CN103543239A (zh) | 废水中硫化物检测方法 | |
| CN106966486A (zh) | 一种过硫氢钾高效水体改良剂 | |
| CN107502651B (zh) | 一种基于钙的强化作用评估活性污泥系统稳健性的方法 | |
| RU2009109350A (ru) | Усовершенствованный окислительно-восстановительный раствор для обессеривания газа | |
| CN106011824A (zh) | 一种机械电镀用环保型钝化液 | |
| JP5530190B2 (ja) | 鉄・ニッケル・クロム合金めっき液及びめっき方法 | |
| CN110200011A (zh) | 一种复合二氧化氯的制备方法 | |
| BRPI0519998B8 (pt) | soluções biocídicas aquosas concentradas formadas de cloreto de bromo, hidróxido de sódio e ácido sulfâmico e seu processo de formação |