PL4807B1 - A method of producing artificial fuel from a mixture of coal. - Google Patents

A method of producing artificial fuel from a mixture of coal. Download PDF

Info

Publication number
PL4807B1
PL4807B1 PL4807A PL480724A PL4807B1 PL 4807 B1 PL4807 B1 PL 4807B1 PL 4807 A PL4807 A PL 4807A PL 480724 A PL480724 A PL 480724A PL 4807 B1 PL4807 B1 PL 4807B1
Authority
PL
Poland
Prior art keywords
coal
mixture
sintering
producing artificial
artificial fuel
Prior art date
Application number
PL4807A
Other languages
Polish (pl)
Filing date
Publication date
Application filed filed Critical
Publication of PL4807B1 publication Critical patent/PL4807B1/en

Description

Przedmiot wynalazku niniejszego sta¬ nowi wyrób zwartego {twardego paliwa) z mieszaniny koksujacych sie i niekoksuija- cych sie wegli tak dobranych, ze nadmiar materjalu wiazacego zawartego w weglu spiekajacym sie moze byc pochloniety przez wegiel niespiekajacy sie. Zadaniem wynalazku jest wytworzyc z tych materja- lów paliwo dogodne do uzycia w wielkich piecach, odlewniach oraz do celów domo¬ wych.Aby otrzymac paliwo zdatne do wspo¬ mnianego uzytku z materjalu natury powy¬ zej wsipomniianej jest niezbednem nietyliko miec baczenie na naturalne wlasciwosci u- zytego wegla, stosunek róznych weg|li w kazdej danej mieszaninie oraz temperatu¬ re zweglania, lecz jest tez bardzo waznem, aby wiegiel sipiekajacy sie, zawierajacy nadmiar materjalu wiazacego, zostal roz¬ mieszczony zupelnie równomiernie w masie mieszaniny.Wedlug wynalazku niniejszego, ze spie¬ kajacego sie wegla w rozdrobnionym luib rozpylonym stanie tworzy sie emulsja z woda, miekkiem mydlem z woda, kreozo¬ tem lub innym plynem, i w takim stanie wegiel spiekajacy sie zostaje zmieszany z weglem niespiekajacym sie, rozdrobnionym w jakibadz sposób do nalezytego wymiaru drobin. Mieszanina ta podlega stwardnieniu zapomoca stlaczania w formie przewazniemajacej ksztalt poprzecznego przekroju pieca czyli retorty. Plyn, z którym jest zmieszany rozdrobniony niespiekajacy sie wegiel, sluzacy czasowo lacznikiem wiaza¬ cym mase, dopomaga tez do równomierne¬ go rozdzialu rozdrobnionego wegla spieka¬ jacego sie w masie, przy otstatecznem mie¬ szaniu.Dogodny stosunek skladników miesza¬ niny wegla, który moze byc wziety jako przyklad, stanowi 10 do 20 procentów wa¬ gowych wieigla spiekajacego sie i 80 do 90 procentów wagowych wegla niespiekaijace- go sie, który tworzy jadra mieszaniny, W niektórych wypadkach ilosc procen¬ towa wegla spiekajacego sie moze byc po¬ wiekszona do 50%, zaleznie od zawartosci czesci wiazacych, zawartych w weglu.Wegiel spiekajacy sie powinien byc zmielony luib rozpylony do tego stopnia, by czafctki jego mogily przejsc przez sito z oczkami (otworami) nie wiekszemi jak 4 mm. Wegiel miesjpiekajacy sie powinien byc tak rozmielony aby kawalki jego prze¬ szly przez sito z otworami nie wiekszemi od 3 num w celu bardziej jednolitego rozdzia¬ lu spiekajacego sie wegla w masie miesza¬ niny; wegiel ten po nalezytern rozmieleniu pozostaje zmieszany z woda lub innym ply¬ nem, przez co stwarza sie emulsja cemen¬ tujaca rozpylony wegiel spiekajacy sie.Stosunek ilosci! dodanej wody Mb innego plynu zmienia sie w zaleznosci od stanu wegla przed operacja. Wynalazca znalazl, ze aby otrzymac dobre wyniki, nalezy do¬ dawac wody lub innego plynu w takim sto¬ sunku, aby ostateczna mieszanina wegli dwóch wspomnianych gatunków zawierala 10 do 15% wagowych wody lujb innego plynu.Otrzymana w ten sposób przedwstepna mieszanina weigla spiekajacego sie z ply¬ nem, dodaje sie do rozmielonejgo lub po- krufczoneigo przedtem wegla nie spiekaja¬ cego sie w naleznym stosunku, jak wspo¬ mniano wyzej, oraz rozdzielona równomier¬ nie wsród masy zapomoca dalszego mie¬ szania, przez co twarde czastki zostaj a rów¬ nomiernie oblepione i zlaczone wzajemnie.Naistepnie otrzymany material zostaje ksztaltowany i po stwardnieniu w formie umieszczony w retorcie jgdzie podlega zwe¬ gleniu (karbonizacji) przy temperaturze od 600 do 1200°C.Otrzymane w ten sposób paliwo moze byc uzyte w domowych kominkach lub pie¬ cach lufo tez dla celów metalurgji. PL PLThe subject of the present invention is the production of a compact (hard fuel) from a mixture of coking and non-coking coals so selected that the excess binding material contained in the caking coal can be absorbed by the non-caking coal. The object of the invention is to produce from these materials a fuel suitable for use in blast furnaces, foundries and for domestic purposes. In order to obtain a fuel suitable for the above-mentioned use from a material of the nature mentioned, it is not only necessary to take into account the natural properties of the coal used, the ratio of the various coals in each given mixture and the charring temperature, but it is also very important that the sintering coal, containing an excess of binding material, is distributed quite evenly throughout the mass of the mixture. According to the present invention, the sintering coal in a crushed or atomized state is emulsified with water, soft soap with water, creosote or other liquid, and in In this state, sintering coal is mixed with non-sintering coal, crushed in some way to the appropriate particle size. This mixture is hardened by pressing in a form usually shaped like the cross-section of a furnace, i.e., a retort. The liquid with which the crushed non-caking coal is mixed, which serves as a temporary binder for the mass, also helps to evenly distribute the crushed sintering coal throughout the mass during the final mixing. A convenient ratio of the coal mixture components, which may be taken as an example, is 10 to 20 percent by weight of the sintering coal and 80 to 90 percent by weight of the non-caking coal, which forms the nuclei of the mixture. In some cases the percentage of sintering coal may be increased to 50 percent, depending on the content of binding components contained in the coal. The sintering coal should be ground or sprayed for this purpose. degree that its particles can pass through a sieve with openings no larger than 4 mm. The sintering coal should be ground so that its pieces pass through a sieve with openings no larger than 3 mm in order to more uniformly distribute the sintering coal in the mass of the mixture; after proper grinding, this coal remains mixed with water or another liquid, thereby creating an emulsion that cements the atomized sintering coal. The ratio of the amount of added water to the other liquid varies depending on the condition of the coal before the operation. The inventor has found that in order to obtain good results, water or another liquid should be added in such a proportion that the final mixture of the two types of coal mentioned contains 10 to 15% by weight of water or another liquid. The preliminary mixture of sintering coal and liquid obtained in this way is added to the previously ground or crushed non-sintering coal in the proper ratio, as mentioned above, and distributed evenly throughout the mass by further mixing, whereby the hard particles are evenly coated and bonded together. Then the obtained material is shaped and, after hardening in a mold, placed in a retort where it undergoes carbonization at a temperature of 600 to 1200°C. The fuel obtained in this way can be used in home fireplaces or stoves, or for metallurgical purposes.

PL4807A 1924-09-04 A method of producing artificial fuel from a mixture of coal. PL4807B1 (en)