Refinement Of Pig-Iron, Manufacture Of Cast Iron, And Steel Manufacture Other Than In Revolving Furnaces
(AREA)
Abstract
The cast iron contains coal and bituminous shist C 2.6-2.8, Cr 22-24, Si maximum 0.6, Mn0.6-0.8, V 0.2-0.4, 5 maximum 0.025, P maximum 0.024, Al 0.05-003, Ti+Mg+Ce+Zr = 0.095-0.140 per cent by weight respectively. The ratio (Ti + Zr)/Mg = 5, and the ratio Cr/C = 8.5.