SU367168A1 - Магнезиальная раскислительная смесь - Google Patents

Магнезиальная раскислительная смесь

Info

Publication number
SU367168A1
SU367168A1 SU1641877A SU1641877A SU367168A1 SU 367168 A1 SU367168 A1 SU 367168A1 SU 1641877 A SU1641877 A SU 1641877A SU 1641877 A SU1641877 A SU 1641877A SU 367168 A1 SU367168 A1 SU 367168A1
Authority
SU
USSR - Soviet Union
Prior art keywords
reducing mixture
magnetic reducing
magnetic
mixture
coke
Prior art date
Application number
SU1641877A
Other languages
English (en)
Inventor
А. С. Пинчук Е. М. Иванов Ф. Г. Шаврин
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to SU1641877A priority Critical patent/SU367168A1/ru
Application granted granted Critical
Publication of SU367168A1 publication Critical patent/SU367168A1/ru

Description

1
Изобретение относитс  к области производства черных металлов.
При выплавке стали и сплавов в дуговых печах используют раскислительную смесь, состо щую из извести, плавикового шпата, молотого кокса и ферросилици , вз тых в соотношении 5:1:1:1.
Однако дл  этой смеси характерно повышенное содержание влаги, вносимой известью , и длительное шлакообразование.
Цель изобретени  - улучшение качества металла и свойств шлака.
Достигаетс  это путем использовани  в качестве компонентов магнезитового порошка, молотых ферросилици  и кокса и порошка алюмини , вз тых в следующем соотношении, вес. %:
основа
15-20
15-20
5-10
Предмет изобретени 
Магнезиальна  раскислительна  смесь дл  выплавки стали, включающа  магнезитовый порошок, молотый ферросилиций, кокс, алюминиевый порошок, отличающа с  тем, что, с целью улучшени  качества металла и свойств шлака, компоненты вз ты в следующем соотношении, вес. %: Магнезитоснова
Ферросилиций15-20
Кокс15-20
Алюминий5-10
SU1641877A 1971-04-09 1971-04-09 Магнезиальная раскислительная смесь SU367168A1 (ru)