SU437331A1 - Способ непрерывной разливки металла - Google Patents
Способ непрерывной разливки металлаInfo
- Publication number
- SU437331A1 SU437331A1 SU1031119A SU1031119A SU437331A1 SU 437331 A1 SU437331 A1 SU 437331A1 SU 1031119 A SU1031119 A SU 1031119A SU 1031119 A SU1031119 A SU 1031119A SU 437331 A1 SU437331 A1 SU 437331A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- ingot
- inductor
- metal
- casting
- continuous casting
- Prior art date
Description
1
Изобретение касаетс металлургии.
Известен способ непрерывной разливки металла с использованием электромагнитного Пол индуктора дл удержани расплава в заданных контурах отливки применением принудительного охлаждени и формирующих отдельные элементы внешнего контура отливки твердых поверхностей. Однако он не обеспечивает хор ошего качества боковых поверхностей и плотной;структуры формирующегос непрерывного слитка.
Предложенный способ отличаетс тем, , что над закристаллизовавшейс частью слитка сохран ют слой жидкотчз металла высотой 15-8О мм, а охлаждающую среду подают на боковую поверхность; слитка вбли-J зи жидкой зоны на рассто нии, обеспечивай шем расположение фронта кристаллизации на поверхности слитка в пределах высоты ;ин- дуктора.
Дл осуществлени способа внутрь инцуЛтора , электромагнитное поле которого при взаимодействии с помещенным в него столбом жидкого металла создает силы, направленные к центру столба, ввод т затравку.
Затем включают поле индуктора, и на затравку подают расплав, первые порции которого кристаллизуютс на затравке. Незакрвсталлизовавшийс металл поддерживаетс индуктора, выбранным с таким расчетам, чтобы. получить определенный зазор между индуктором и наружными | спо мк столба металла . Затем начинают непрерывно до получени слитка заданной длины выт гивать заготовку и заливать металл, сохран слой жидкого металла высотой 1S-80 WM над закристаллизовавшейс частью слитка. Причем на боковые поверхности слитка вблизи жидкой зоны на рассто нии, обеспечивающем расположение фронта кристаллизации в пределах высоты индуктора, подают охлаждаю щую среду.
Claims (1)
- Формула изобретениСпособ непрерывной разливки метал7;а с использоваьгаем электромагнитного пол индуктора дл удержани расплава в заданны.: контурах отливки применением принудитель3кого охлаждени и формирующих отдельныестью слитка сохран ют слой жидкого металэлементы внешнего хонтура отлнвки твер-лв вьюотой 15-60 мм, а охлвжцаюшую срйдых поверхностей, отличаюшийс ду подают на боковую поверхность слиткатем, что, с целью обеснеченн хорошего ке г-вблизи жидкой зоны на рассто нии, обеспечества боковых ш верхвостей отливок и плот+ 5чиввющем расположение фронта кристаллиной структуры формирующегос непрерывно - аааии на поверхности слитка в пределах выго I слитка, ва0 закрврталлизовавшейс ча-соты индуктора.437331