SU616252A1 - Бетонна смесь - Google Patents

Бетонна смесь

Info

Publication number
SU616252A1
SU616252A1 SU752118145A SU2118145A SU616252A1 SU 616252 A1 SU616252 A1 SU 616252A1 SU 752118145 A SU752118145 A SU 752118145A SU 2118145 A SU2118145 A SU 2118145A SU 616252 A1 SU616252 A1 SU 616252A1
Authority
SU
USSR - Soviet Union
Prior art keywords
sodium nitrite
corrosion
concrete
strength
concrete mix
Prior art date
Application number
SU752118145A
Other languages
English (en)
Inventor
Михаил Моисеевич Чернин-Яхнюк
Лео Николевич Шарыгин
Владимир Михайлович Кравцов
Георгий Нисович Гельфман
Алексей Филиппович Полак
Владимир Донович Фаерштейн
Original Assignee
Научно-Исследовательский Институт Промышленного Строительства
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Научно-Исследовательский Институт Промышленного Строительства filed Critical Научно-Исследовательский Институт Промышленного Строительства
Priority to SU752118145A priority Critical patent/SU616252A1/ru
Application granted granted Critical
Publication of SU616252A1 publication Critical patent/SU616252A1/ru

Links

Landscapes

  • Curing Cements, Concrete, And Artificial Stone (AREA)
  • Lubricants (AREA)

Claims (2)

  1. (545; БЕТОННАЯ СМЕСЬ Заполнитель47 Нитрит натри 0,22 АМИД жирных.кислот 0,11 CHjCCHi i -C -Catt OHРезультаты исгштамий); Прочность на сжатие, 33,6 0,15 Стационарный потен , UHajD, В Коэф цйент подавлени  Более 9 коррозии 10,9 рН поровой жидкости Порова  жидкость бетона  вл ет с  хорошим пассиватором, что обеспе чивает коррозионную стойкость и про ность железобетонных изделий. Формула изобретени  Бетонна  смесь, включающа  в жу щее, заполнитель, нитрит натри  и. воду, отличающа  с   тем, что, с целью повышени  прочности и коррозионной стойкости, она содержит дополнительно амм.жирны} к 1слот общёТ формулы Ф Т гй-Сьйчб /; где B-CHjCdHj) vtpM n 21 при следующем соотношении компонентов, вес.% В жущее15-40 Заполнитель 47-80 Нитрит натри  0,22-0,27 Амид жирных кислот0, ВодаОстальное, причем в жущее содержит 30-40 вес.% продукта обжига твердог;#1 .остатка дистиллерных стоков и )66-70 вес.% молотого кварцевого песка. Источники информацииг прин тые во внимание при экспертизе: 1. Ратинов В.Б. и др. Хими  в строительстве . Издательство литературы по строительству, М., 19€9, с. 132-150.
  2. 2. Енишерлов С.Г. и др. Защита арматуры железобетонных изделий от коррозии с помощью добавок нитро , вып. XI, Стройиздат, 1973, с. 303-314.
SU752118145A 1975-04-10 1975-04-10 Бетонна смесь SU616252A1 (ru)