SU700472A1 - Способ обогрева ванной стекловаренной печи - Google Patents
Способ обогрева ванной стекловаренной печиInfo
- Publication number
- SU700472A1 SU700472A1 SU782620622A SU2620622A SU700472A1 SU 700472 A1 SU700472 A1 SU 700472A1 SU 782620622 A SU782620622 A SU 782620622A SU 2620622 A SU2620622 A SU 2620622A SU 700472 A1 SU700472 A1 SU 700472A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- heating bath
- bath glass
- moulding oven
- glass
- moulding
- Prior art date
Description
на ванной стекловаренной печи системы БВВС Токмакского стекольного заводаМаксимум тепловых нагрузок в зоне шихты устанавливают на рассто нии 7 м от торцовой загрузочной стевки печи лри длине максимума 3,7 м (длина отапливаемой части печи составл ет 26,5 м). При этом минимум тепловых нагрузок в зопе варочной пены (четверта пара горелок) составл ет 0,54 от величины .макси мума в зоне шихты.
Распределение газа по горелкам семигорелочной ванной стекловаренной печи, а также абсолютные и относительные тепловые нагрузки в соответствуюи1,их зонах представлены в таблице.
Испытани предложенного способа обогрева ванной стекловаренной печи показали , что оптимальное расположение максимума тепловых нагрузок в зоне шихты на рассто нии 0,2-0,3 длины отапливаемой части от ее торцовой загрузочной стенки при длине максимума 0,15-0,3.
Три такой тепловой нагрузке в зоне ШИХТЫ оптимальна величина минимума в зоне варочной пены составл ет 0,5-0,6 от величины максимума в зоне шихты.
Использование предложенного способа обогрева позвол ет снизить удельный расход топлива на 10%.
Claims (2)
1.Авторское свидетельство СССР № 400529, кл. СОЗ В 5/24, 1972.
2.Авторское свидетельство СССР № 591415, кл. СОЗ В 5/24, 1976.