TWI311086B - - Google Patents
Download PDFInfo
- Publication number
- TWI311086B TWI311086B TW95148319A TW95148319A TWI311086B TW I311086 B TWI311086 B TW I311086B TW 95148319 A TW95148319 A TW 95148319A TW 95148319 A TW95148319 A TW 95148319A TW I311086 B TWI311086 B TW I311086B
- Authority
- TW
- Taiwan
- Prior art keywords
- workpiece
- electrode
- clamp
- slide rail
- rollers
- Prior art date
Links
- 238000003466 welding Methods 0.000 claims description 34
- 238000000034 method Methods 0.000 claims description 22
- 239000011324 bead Substances 0.000 claims description 14
- 238000003825 pressing Methods 0.000 claims description 9
- 239000004020 conductor Substances 0.000 claims description 3
- 238000004519 manufacturing process Methods 0.000 description 5
- 230000007547 defect Effects 0.000 description 4
- 239000000463 material Substances 0.000 description 3
- 239000002184 metal Substances 0.000 description 3
- 238000005096 rolling process Methods 0.000 description 3
- 238000007789 sealing Methods 0.000 description 3
- 238000010586 diagram Methods 0.000 description 2
- 230000000694 effects Effects 0.000 description 2
- 230000015572 biosynthetic process Effects 0.000 description 1
- 238000006243 chemical reaction Methods 0.000 description 1
- 238000007796 conventional method Methods 0.000 description 1
- 238000005516 engineering process Methods 0.000 description 1
- 230000004927 fusion Effects 0.000 description 1
- 238000012986 modification Methods 0.000 description 1
- 230000004048 modification Effects 0.000 description 1
- 230000000750 progressive effect Effects 0.000 description 1
- 238000005476 soldering Methods 0.000 description 1
Landscapes
- Sealing Battery Cases Or Jackets (AREA)
- Resistance Welding (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| TW95148319A TW200827076A (en) | 2006-12-22 | 2006-12-22 | Method of resistance roller welding and resistance roller welding apparatus |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| TW95148319A TW200827076A (en) | 2006-12-22 | 2006-12-22 | Method of resistance roller welding and resistance roller welding apparatus |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| TW200827076A TW200827076A (en) | 2008-07-01 |
| TWI311086B true TWI311086B (2) | 2009-06-21 |
Family
ID=44817101
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| TW95148319A TW200827076A (en) | 2006-12-22 | 2006-12-22 | Method of resistance roller welding and resistance roller welding apparatus |
Country Status (1)
| Country | Link |
|---|---|
| TW (1) | TW200827076A (2) |
-
2006
- 2006-12-22 TW TW95148319A patent/TW200827076A/zh unknown
Also Published As
| Publication number | Publication date |
|---|---|
| TW200827076A (en) | 2008-07-01 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| WO2018103081A1 (zh) | 一种激光复合焊接设备 | |
| US9943928B2 (en) | Method of operating an apparatus for linear friction welding | |
| JP4332157B2 (ja) | 摩擦攪拌接合装置 | |
| KR101456410B1 (ko) | 절단 방법, 로터 제조 방법 및 절단 장치 | |
| CN207269038U (zh) | 一种电池封口侧焊定位夹具及系统 | |
| US9278479B2 (en) | Apparatus for linear friction welding | |
| CN102554451B (zh) | 双边超声波焊机 | |
| TWI311086B (2) | ||
| CN102554450A (zh) | 一种动力电池多层电极超声波机械手焊接设备 | |
| CN107000110A (zh) | 缝焊用滚轮电极的整形装置及整形方法 | |
| CN214979461U (zh) | 一种定位机构及定位设备 | |
| CN1791489A (zh) | 凸焊装置及其凸焊方法 | |
| US8230892B1 (en) | Thermoplastic welding apparatus and method | |
| CN110116262B (zh) | 一种焊接工装设备 | |
| CN216632995U (zh) | 一种圆筒形工件的外径抱紧装置 | |
| JP6868885B2 (ja) | 接合装置並びにそれを用いた接合方法及び接合体の製造方法 | |
| WO2016147999A1 (ja) | 摩擦撹拌接合装置 | |
| CN215698864U (zh) | 一种焊接设备 | |
| CN212526549U (zh) | 一种激光的焊接结构 | |
| CN118595602B (zh) | 一种高压快插连接件焊接工艺 | |
| JP2013078772A5 (2) | ||
| CN211135982U (zh) | 一种用于手机电池的检测折弯夹具 | |
| CN108941872B (zh) | 电阻焊接设备及其焊接方法 | |
| JP4594882B2 (ja) | 摩擦攪拌接合装置および摩擦攪拌接合方法 | |
| KR101379735B1 (ko) | 서브머지드 아크 용접기용 헤드 조립체 |