WO2016021009A1 - Récipient en matière plastique - Google Patents
Récipient en matière plastique Download PDFInfo
- Publication number
- WO2016021009A1 WO2016021009A1 PCT/JP2014/070760 JP2014070760W WO2016021009A1 WO 2016021009 A1 WO2016021009 A1 WO 2016021009A1 JP 2014070760 W JP2014070760 W JP 2014070760W WO 2016021009 A1 WO2016021009 A1 WO 2016021009A1
- Authority
- WO
- WIPO (PCT)
- Prior art keywords
- reduced pressure
- bottom wall
- resin container
- pressure absorbing
- container
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Ceased
Abstract
Priority Applications (5)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| PCT/JP2014/070760 WO2016021009A1 (fr) | 2014-08-06 | 2014-08-06 | Récipient en matière plastique |
| SG11201700853PA SG11201700853PA (en) | 2014-08-06 | 2014-08-06 | Resin container |
| MYPI2017700341A MY183596A (en) | 2014-08-06 | 2014-08-06 | Resin container |
| JP2016539743A JP6678106B2 (ja) | 2014-08-06 | 2014-08-06 | 樹脂製容器 |
| TW104117165A TWI566990B (zh) | 2014-08-06 | 2015-05-28 | 樹脂製容器 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| PCT/JP2014/070760 WO2016021009A1 (fr) | 2014-08-06 | 2014-08-06 | Récipient en matière plastique |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| WO2016021009A1 true WO2016021009A1 (fr) | 2016-02-11 |
Family
ID=55263315
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| PCT/JP2014/070760 Ceased WO2016021009A1 (fr) | 2014-08-06 | 2014-08-06 | Récipient en matière plastique |
Country Status (5)
| Country | Link |
|---|---|
| JP (1) | JP6678106B2 (fr) |
| MY (1) | MY183596A (fr) |
| SG (1) | SG11201700853PA (fr) |
| TW (1) | TWI566990B (fr) |
| WO (1) | WO2016021009A1 (fr) |
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2017154804A (ja) * | 2016-03-03 | 2017-09-07 | 大日本印刷株式会社 | プラスチックボトル、充填体、及び充填体の製造方法 |
| JP2017165453A (ja) * | 2016-03-16 | 2017-09-21 | 大日本印刷株式会社 | プラスチックボトル、及び充填体 |
| JP2018162095A (ja) * | 2017-03-27 | 2018-10-18 | サントリーホールディングス株式会社 | 樹脂製容器 |
| JP2020196546A (ja) * | 2020-09-09 | 2020-12-10 | 大日本印刷株式会社 | プラスチックボトル、及び充填体 |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| USD1126002S1 (en) | 2024-10-08 | 2026-05-12 | Co2Pac Limited | Container |
Citations (12)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH043910U (fr) * | 1990-04-23 | 1992-01-14 | ||
| US5407086A (en) * | 1992-08-21 | 1995-04-18 | Yoshino Kogyosho Co., Ltd. | Bottle |
| WO2003029087A1 (fr) * | 2001-09-27 | 2003-04-10 | Yoshino Kogyosho Co., Ltd. | Contenant en resine synthetique a memoire de forme |
| JP2005008153A (ja) * | 2003-06-16 | 2005-01-13 | Dainippon Printing Co Ltd | 合成樹脂製壜体 |
| WO2005120991A1 (fr) * | 2004-06-04 | 2005-12-22 | Plastipak Packaging, Inc. | Conteneur plastique |
| JP2007091338A (ja) * | 2005-08-31 | 2007-04-12 | Yoshino Kogyosho Co Ltd | 合成樹脂製角型壜体 |
| JP2008143594A (ja) * | 2006-12-13 | 2008-06-26 | Dainippon Printing Co Ltd | 内容物容器およびそれを構成する容器本体 |
| JP2009007026A (ja) * | 2007-06-27 | 2009-01-15 | Yoshino Kogyosho Co Ltd | ボトル |
| JP4217890B2 (ja) * | 2003-09-26 | 2009-02-04 | 東洋製罐株式会社 | 合成樹脂製容器 |
| WO2011112278A2 (fr) * | 2010-03-10 | 2011-09-15 | Amcor Limited | Récipient thermofixé |
| JP4912784B2 (ja) * | 2006-07-31 | 2012-04-11 | 株式会社吉野工業所 | 合成樹脂製ボトル |
| US8602237B2 (en) * | 2009-10-06 | 2013-12-10 | Graham Packaging Company, L.P. | Pasteurizable and hot-fillable blow molded plastic container |
Family Cites Families (10)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP3412494B2 (ja) * | 1998-02-09 | 2003-06-03 | 東洋製罐株式会社 | 合成樹脂製ボトル |
| JP4192303B2 (ja) * | 1998-08-11 | 2008-12-10 | 東洋製罐株式会社 | 丸型プラスチックボトル |
| JP4395696B2 (ja) * | 2001-08-21 | 2010-01-13 | 東洋製罐株式会社 | 合成樹脂製容器 |
| JP4675013B2 (ja) * | 2001-09-26 | 2011-04-20 | 株式会社吉野工業所 | ピンチグリップ式ボトル型容器 |
| JP4596115B2 (ja) * | 2003-03-31 | 2010-12-08 | 株式会社吉野工業所 | 合成樹脂製壜体 |
| JP4219771B2 (ja) * | 2003-08-29 | 2009-02-04 | 株式会社吉野工業所 | 合成樹脂製ボトル型容器 |
| AR051580A1 (es) * | 2004-09-30 | 2007-01-24 | Melrose David Murray | Recipiente de presion con paneles de vacio diferenciales |
| JP2012254819A (ja) * | 2011-06-10 | 2012-12-27 | Kirin Brewery Co Ltd | プラスチック成形体 |
| MX351554B (es) * | 2011-06-28 | 2017-10-19 | Abc Group Inc | Perfil de superficie de expansión por congelación. |
| JP6040013B2 (ja) * | 2012-11-30 | 2016-12-07 | 株式会社吉野工業所 | ボトル |
-
2014
- 2014-08-06 WO PCT/JP2014/070760 patent/WO2016021009A1/fr not_active Ceased
- 2014-08-06 SG SG11201700853PA patent/SG11201700853PA/en unknown
- 2014-08-06 MY MYPI2017700341A patent/MY183596A/en unknown
- 2014-08-06 JP JP2016539743A patent/JP6678106B2/ja active Active
-
2015
- 2015-05-28 TW TW104117165A patent/TWI566990B/zh active
Patent Citations (12)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH043910U (fr) * | 1990-04-23 | 1992-01-14 | ||
| US5407086A (en) * | 1992-08-21 | 1995-04-18 | Yoshino Kogyosho Co., Ltd. | Bottle |
| WO2003029087A1 (fr) * | 2001-09-27 | 2003-04-10 | Yoshino Kogyosho Co., Ltd. | Contenant en resine synthetique a memoire de forme |
| JP2005008153A (ja) * | 2003-06-16 | 2005-01-13 | Dainippon Printing Co Ltd | 合成樹脂製壜体 |
| JP4217890B2 (ja) * | 2003-09-26 | 2009-02-04 | 東洋製罐株式会社 | 合成樹脂製容器 |
| WO2005120991A1 (fr) * | 2004-06-04 | 2005-12-22 | Plastipak Packaging, Inc. | Conteneur plastique |
| JP2007091338A (ja) * | 2005-08-31 | 2007-04-12 | Yoshino Kogyosho Co Ltd | 合成樹脂製角型壜体 |
| JP4912784B2 (ja) * | 2006-07-31 | 2012-04-11 | 株式会社吉野工業所 | 合成樹脂製ボトル |
| JP2008143594A (ja) * | 2006-12-13 | 2008-06-26 | Dainippon Printing Co Ltd | 内容物容器およびそれを構成する容器本体 |
| JP2009007026A (ja) * | 2007-06-27 | 2009-01-15 | Yoshino Kogyosho Co Ltd | ボトル |
| US8602237B2 (en) * | 2009-10-06 | 2013-12-10 | Graham Packaging Company, L.P. | Pasteurizable and hot-fillable blow molded plastic container |
| WO2011112278A2 (fr) * | 2010-03-10 | 2011-09-15 | Amcor Limited | Récipient thermofixé |
Cited By (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2017154804A (ja) * | 2016-03-03 | 2017-09-07 | 大日本印刷株式会社 | プラスチックボトル、充填体、及び充填体の製造方法 |
| JP2017165453A (ja) * | 2016-03-16 | 2017-09-21 | 大日本印刷株式会社 | プラスチックボトル、及び充填体 |
| JP7003391B2 (ja) | 2016-03-16 | 2022-01-20 | 大日本印刷株式会社 | プラスチックボトル、及び充填体 |
| JP2018162095A (ja) * | 2017-03-27 | 2018-10-18 | サントリーホールディングス株式会社 | 樹脂製容器 |
| JP2020196546A (ja) * | 2020-09-09 | 2020-12-10 | 大日本印刷株式会社 | プラスチックボトル、及び充填体 |
| JP7006743B2 (ja) | 2020-09-09 | 2022-01-24 | 大日本印刷株式会社 | プラスチックボトル、及び充填体 |
Also Published As
| Publication number | Publication date |
|---|---|
| SG11201700853PA (en) | 2017-03-30 |
| JP6678106B2 (ja) | 2020-04-08 |
| TW201605693A (zh) | 2016-02-16 |
| MY183596A (en) | 2021-03-02 |
| JPWO2016021009A1 (ja) | 2017-06-22 |
| TWI566990B (zh) | 2017-01-21 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP6732410B2 (ja) | 合成樹脂製容器 | |
| AU2009208458B2 (en) | Synthetic resin bottle | |
| BR112017003390B1 (pt) | Base de recipiente de dois estágios | |
| JP6678106B2 (ja) | 樹脂製容器 | |
| US11352184B2 (en) | Container | |
| WO2018159630A1 (fr) | Contenant en résine | |
| WO2017037993A1 (fr) | Récipient en résine synthétique et procédé de fabrication de celui-ci | |
| CN111801277B (zh) | 容器 | |
| JP6685842B2 (ja) | ブロー成形容器 | |
| JP6671104B2 (ja) | 合成樹脂製容器 | |
| WO2018123944A1 (fr) | Récipient en résine | |
| JP6602528B2 (ja) | プラスチックボトル | |
| CN110461719B (zh) | 无菌填充用瓶 | |
| JP6403392B2 (ja) | 合成樹脂製ボトル | |
| CN105793161A (zh) | 具有偏置型水平肋和面板的耐真空容器 | |
| JP2015160650A (ja) | プラスチックボトル | |
| JP2018162095A (ja) | 樹脂製容器 | |
| JP6566604B2 (ja) | 合成樹脂製扁平ボトルの底部形状 | |
| JP6759050B2 (ja) | 合成樹脂製容器 | |
| JP7388807B2 (ja) | プラスチックボトル | |
| JP2018104025A (ja) | 樹脂製容器 | |
| JP2017047953A (ja) | 合成樹脂製ボトル | |
| JP2018104026A (ja) | 樹脂製容器 | |
| JP2018144879A (ja) | 加温用樹脂製容器 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| 121 | Ep: the epo has been informed by wipo that ep was designated in this application |
Ref document number: 14899179 Country of ref document: EP Kind code of ref document: A1 |
|
| WWE | Wipo information: entry into national phase |
Ref document number: IDP00201603414 Country of ref document: ID |
|
| ENP | Entry into the national phase |
Ref document number: 2016539743 Country of ref document: JP Kind code of ref document: A |
|
| NENP | Non-entry into the national phase |
Ref country code: DE |
|
| 122 | Ep: pct application non-entry in european phase |
Ref document number: 14899179 Country of ref document: EP Kind code of ref document: A1 |