WO2020119002A1 - Procédé d'étirage avec positionnement bidirectionnel axial et de moulage d'article creux par soufflage - Google Patents

Procédé d'étirage avec positionnement bidirectionnel axial et de moulage d'article creux par soufflage Download PDF

Info

Publication number
WO2020119002A1
WO2020119002A1 PCT/CN2019/083557 CN2019083557W WO2020119002A1 WO 2020119002 A1 WO2020119002 A1 WO 2020119002A1 CN 2019083557 W CN2019083557 W CN 2019083557W WO 2020119002 A1 WO2020119002 A1 WO 2020119002A1
Authority
WO
WIPO (PCT)
Prior art keywords
stretching
preform
blow molding
supporting device
rod
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Ceased
Application number
PCT/CN2019/083557
Other languages
English (en)
Chinese (zh)
Inventor
谢国基
姜晓平
胡青春
卢佳
梁炎均
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
GDXL Precise Machinery Co Ltd
Original Assignee
GDXL Precise Machinery Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by GDXL Precise Machinery Co Ltd filed Critical GDXL Precise Machinery Co Ltd
Publication of WO2020119002A1 publication Critical patent/WO2020119002A1/fr
Anticipated expiration legal-status Critical
Ceased legal-status Critical Current

Abstract

L'invention concerne un procédé d'étirage avec positionnement bidirectionnel axial et de moulage d'article creux par soufflage. Selon l'invention, un dispositif de support pour le support temporaire du fond d'une préforme de bouteille est disposé dans une cavité de moule. Le procédé de moulage de récipient par soufflage comprend les étapes suivantes : étape 1 : le chauffage d'une préforme de bouteille à une température d'étirage et la mise en œuvre d'un pré-moulage par soufflage avec étirage simultané ; étape 2 : lorsque la préforme de bouteille est étirée jusqu'à la position du dispositif de support, le support par le dispositif de support du centre du fond de la préforme de bouteille qui a été progressivement étirée et expansée, la vitesse d'étirage étant ralentie ou l'étirage étant interrompu à la position du point de support au fond de la préforme de bouteille et la périphérie du point de support étant étirée en continu sous l'effet de la pression d'air et de l'inertie de son propre matériau ; et étape 3 : après qu'un fond conique est préformé, le retrait ou le déplacement du dispositif de support avec une tige d'étirage, la poursuite de l'étirage par la tige d'étirage, l'injection d'air sous pression, puis la mise en œuvre d'un refroidissement pour former un récipient moulé par soufflage. Au moyen du support à l'étape 2, le matériau au fond de la préforme de bouteille est complètement étiré et est réparti plus uniformément au fond de la bouteille, de sorte qu'un meilleur refroidissement et un meilleur moulage peuvent être réalisés.
PCT/CN2019/083557 2018-12-13 2019-04-20 Procédé d'étirage avec positionnement bidirectionnel axial et de moulage d'article creux par soufflage Ceased WO2020119002A1 (fr)

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
CN201811527312.2A CN109454851B (zh) 2018-12-13 2018-12-13 一种轴向双方向定位拉伸中空吹塑成型方法
CN201811527312.2 2018-12-13

Publications (1)

Publication Number Publication Date
WO2020119002A1 true WO2020119002A1 (fr) 2020-06-18

Family

ID=65613219

Family Applications (1)

Application Number Title Priority Date Filing Date
PCT/CN2019/083557 Ceased WO2020119002A1 (fr) 2018-12-13 2019-04-20 Procédé d'étirage avec positionnement bidirectionnel axial et de moulage d'article creux par soufflage

Country Status (2)

Country Link
CN (1) CN109454851B (fr)
WO (1) WO2020119002A1 (fr)

Families Citing this family (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN109454851B (zh) * 2018-12-13 2021-06-01 广东星联精密机械有限公司 一种轴向双方向定位拉伸中空吹塑成型方法
CN110303664A (zh) * 2019-07-24 2019-10-08 广东星联精密机械有限公司 一种配备加热拉伸系统的吹塑成型模具及方法

Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2002067131A (ja) * 2000-08-30 2002-03-05 Aoki Technical Laboratory Inc 延伸ブロー成形方法及びブロー金型
CN101130274A (zh) * 2006-08-22 2008-02-27 东莞佳鸿机械制造有限公司 吹塑机的瓶胚拉伸吹气装置
CN109454851A (zh) * 2018-12-13 2019-03-12 广东星联精密机械有限公司 一种轴向双方向定位拉伸中空吹塑成型方法

Family Cites Families (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
DE102012111348A1 (de) * 2012-11-23 2014-05-28 Krones Ag Streckblasverfahren sowie Streckblasmaschine
JP6437379B2 (ja) * 2015-04-30 2018-12-12 株式会社吉野工業所 液体ブロー成形装置および液体ブロー成形方法

Patent Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2002067131A (ja) * 2000-08-30 2002-03-05 Aoki Technical Laboratory Inc 延伸ブロー成形方法及びブロー金型
CN101130274A (zh) * 2006-08-22 2008-02-27 东莞佳鸿机械制造有限公司 吹塑机的瓶胚拉伸吹气装置
CN109454851A (zh) * 2018-12-13 2019-03-12 广东星联精密机械有限公司 一种轴向双方向定位拉伸中空吹塑成型方法

Also Published As

Publication number Publication date
CN109454851A (zh) 2019-03-12
CN109454851B (zh) 2021-06-01

Similar Documents

Publication Publication Date Title
US2890483A (en) Machine for forming plastic containers
US2973558A (en) Method for deep-draw vacuum forming
CN111037866A (zh) 一种具有快速冷却功能的汽车外围侧板注塑模具
WO2021012839A1 (fr) Moule de moulage par soufflage et procédé équipé d'un système chauffant et d'étirage
WO2020119002A1 (fr) Procédé d'étirage avec positionnement bidirectionnel axial et de moulage d'article creux par soufflage
CN102107523B (zh) 汽车油管的卧式吹塑成型模具及其吹塑成型方法
US4085177A (en) Process for thermoforming a hollow plastic article using an extendible porous male mold assembly
WO2018074315A1 (fr) Dispositif de moulage par soufflage et procédé de fabrication d'un récipient de résine synthétique l'utilisant
CN202213104U (zh) 一种用于轮胎硫化机的卸胎机械手及升降式卸胎装置
CN210085265U (zh) 一种管制西林瓶口部成型模具
CN119285207A (zh) 一种轻量化玻璃瓶小口压吹装置及工艺方法
CN219360204U (zh) 一种包装盒注塑脱模机构
CN211334293U (zh) 隐形眼镜脱模取镜装置
CN209971501U (zh) 一种推瓶装置
CN109454855B (zh) 一种轴向双方向定位拉伸中空吹塑成型模具
CN212124140U (zh) 一种高效自动真空吹塑机
CN213830305U (zh) 一种吸塑机成型模具
CN222451437U (zh) 一种实心轮胎成型机
CN211763408U (zh) 一种吹瓶机的瓶胚入座装置
CN214645802U (zh) 应用于双向拉伸中空吹塑成型模具上的模腔结构
CN112976549B (zh) 制冷设备的内胆吸塑成型模具及内胆吸塑成型方法
CN222571556U (zh) 一种吹塑机中空料胚口型装置
JPH0257317A (ja) ブロー成形装置
CN106493886A (zh) 轮胎下调模加力装置
CN222004402U (zh) 一种储氢瓶吹塑机吹针机构

Legal Events

Date Code Title Description
121 Ep: the epo has been informed by wipo that ep was designated in this application

Ref document number: 19896070

Country of ref document: EP

Kind code of ref document: A1

NENP Non-entry into the national phase

Ref country code: DE

122 Ep: pct application non-entry in european phase

Ref document number: 19896070

Country of ref document: EP

Kind code of ref document: A1

122 Ep: pct application non-entry in european phase

Ref document number: 19896070

Country of ref document: EP

Kind code of ref document: A1

32PN Ep: public notification in the ep bulletin as address of the adressee cannot be established

Free format text: NOTING OF LOSS OF RIGHTS PURSUANT TO RULE 112(1) EPC (EPO FORM 1205A DATED 03/05/2022)

122 Ep: pct application non-entry in european phase

Ref document number: 19896070

Country of ref document: EP

Kind code of ref document: A1