Disclosure of Invention
Aiming at the problems in the prior art, the invention provides a method for manufacturing ceramics by utilizing a three-dimensional printing technology, which specifically comprises the steps of preparing tetraethoxysilane and powder materials with preset components in advance, and mixing water, cosolvent and acid-base regulator according to a certain proportion to obtain a composite functional reagent;
the method comprises the steps that firstly, a three-dimensional model to be printed is generated through an upper computer, a plurality of layers of corresponding plane graphs are formed after the three-dimensional model is sliced, and the plane graphs are sent to a lower three-dimensional printer to be printed;
also comprises the following steps:
step S1, mixing the tetraethoxysilane, the powder material and the composite functional reagent on a molding surface to form a printing layer corresponding to the plan view;
step S2, heating the printing layer by adopting a heating device of the three-dimensional printer to complete the forming of one layer;
step S3, repeating the steps S1-S2 until all the plane views are printed and a ceramic precursor is formed, and turning to step S4;
and step S4, processing the ceramic precursor to obtain a ceramic piece, and then withdrawing.
Preferably, the powder material, the tetraethoxysilane and the composite functional reagent are respectively prepared, so that the mass ratio of the tetraethoxysilane to the powder material is 2-15%, and the mass of water in the composite functional reagent is 2-5 times of the mass of the tetraethoxysilane.
Preferably, the powder material comprises one or a mixture of several of porcelain clay, kaolin, pottery clay, bentonite and feldspar powder;
the particle size range of the powder is 100-.
Preferably, in step S2, the heating device is an infrared heating device, or a microwave heating device, or an ultrasonic accelerated reaction device.
Preferably, when the complex functional reagent is formed by mixing, the certain proportion is as follows: the content of water is not less than 50%, and the content of cosolvent is not less than 10%.
Preferably, the complex functional agent formed by mixing:
the cosolvent comprises ethanol, and/or methanol, and/or isopropanol, and/or n-butanol, and/or dioxane, and/or formamide, and/or acetone, and/or tetrahydrofuran;
the acid-base regulator comprises hydrochloric acid, and/or hydrofluoric acid, and/or sulfuric acid, and/or nitric acid, and/or ammonia water, and/or organic ammonia.
Preferably, the tetraethoxysilane and the powder material are mixed in advance to form a first premixed powder material;
the step S1 specifically includes:
step S11a, laying the first premixed powder on the molding surface;
and step S12a, adopting the array piezoelectric spray heads of the three-dimensional printer to spray the composite functional reagent on the molding surface to form the printing layer.
Preferably, the powder material and the composite functional reagent are mixed in advance to form a second premixed powder material;
the step S1 specifically includes:
step S11b, laying the second premixed powder on the molding surface;
and step S12b, jetting the tetraethoxysilane on the molding surface by using an array type piezoelectric nozzle of the three-dimensional printer to form the printing layer.
Preferably, the step S1 specifically includes:
step S11c, paving the powder material on the molding surface;
and S12c, spraying the ethyl orthosilicate on the molding surface by using a first array type piezoelectric sprayer on the three-dimensional printer, and spraying the composite functional reagent on the molding surface by using a second array type piezoelectric sprayer on the three-dimensional printer to form the printing layer.
Preferably, the ceramic part is formed by processing the ceramic precursor in a sintering manner, and specifically includes:
step A1, soaking the ceramic precursor in tetraethoxysilane;
step A2, placing the ceramic precursor into the composite functional reagent for soaking;
and A3, taking out the ceramic precursor, drying and sintering to form the ceramic piece.
Preferably, the ceramic precursor is processed in a sintering-free manner to form the ceramic part, and the method specifically includes:
step B1, soaking the ceramic precursor in tetraethoxysilane;
step B2, placing the ceramic precursor into the composite functional reagent for soaking;
step B3, taking out the ceramic precursor and drying;
repeating the steps B1-B3 until the ceramic piece is formed after the liquid cannot penetrate into the ceramic precursor.
The invention has the beneficial effects that:
1) the raw materials with lower price are adopted, so that the cost of the three-dimensional printing ceramic part is reduced;
2) the manufactured ceramic piece has few defects and high density;
3) the printing size of the ceramic piece is not limited, the printing efficiency is high, and the production efficiency is effectively improved;
4) the forming binder in the printing and forming process is inorganic silicon dioxide, is one of effective components of the ceramic, does not need to be degreased, does not generate a large amount of organic matters in the sintering process, and is more environment-friendly in the production process.
Detailed Description
The invention is described in detail below with reference to the figures and specific embodiments. The present invention is not limited to the embodiment, and other embodiments may be included in the scope of the present invention as long as the gist of the present invention is satisfied.
A method for manufacturing ceramics by utilizing a three-dimensional printing technology comprises the steps of preparing tetraethoxysilane, powder materials with preset components and a composite functional reagent obtained by mixing water, a cosolvent and an acid-base regulator according to a certain proportion in advance;
the method comprises the steps that firstly, a three-dimensional model to be printed is generated through an upper computer, a plurality of layers of corresponding plane graphs are formed after the three-dimensional model is sliced, and the plane graphs are sent to a lower three-dimensional printer to be printed;
as shown in fig. 1, the method further comprises the following steps:
step S1, mixing tetraethoxysilane, powder material and composite functional reagent on a molding surface to form a printing layer corresponding to a plan view;
step S2, heating the printing layer by adopting a heating device of the three-dimensional printer to complete the forming of one layer;
step S3, repeating the steps S1-S2 until all the plane views are printed and the ceramic precursor is formed, and turning to step S4;
and step S4, processing the ceramic precursor to obtain a ceramic piece, and then withdrawing.
Specifically, in this embodiment, the layer thickness of the printing layer may be set on the upper computer software as required, and the set value of the layer thickness may be between 0.05 mm and 1 mm.
In a preferred embodiment of the invention, the powder material, the tetraethoxysilane and the composite functional reagent are respectively prepared, so that the mass ratio of the tetraethoxysilane to the powder material is 2-15%, and the mass of water in the composite functional reagent is 2-5 times of that of the tetraethoxysilane.
Specifically, in this embodiment, the amount of tetraethoxysilane is less, the amount of the powder material is more, and the mass ratio of tetraethoxysilane to the powder material includes, but is not limited to, 2% to 15%, wherein tetraethoxysilane may also be replaced by a liquid containing tetraethoxysilane as a main component.
In a preferred embodiment of the invention, the powder material comprises one or a mixture of several of porcelain clay, kaolin, pottery clay, bentonite and feldspar powder; and the particle size range of the powder is 100-8000 meshes.
Specifically, in this embodiment, the powder material is one or a mixture of several kinds of powders of ceramic main raw materials, and the invention is not particularly limited.
In a preferred embodiment of the present invention, in step S2, the heating device is an infrared heating device, or a microwave heating device, or an ultrasonic accelerated reaction device.
In a preferred embodiment of the present invention, when the complex functional reagent is formed by mixing, the ratio is: the content of water is not less than 50%, and the content of cosolvent is not less than 10%.
In a preferred embodiment of the present invention, the complex functional reagent formed by mixing:
the cosolvent comprises ethanol, and/or methanol, and/or isopropanol, and/or n-butanol, and/or dioxane, and/or formamide, and/or acetone, and/or tetrahydrofuran;
the pH regulator comprises hydrochloric acid, and/or hydrofluoric acid, and/or sulfuric acid, and/or nitric acid, and/or ammonia water, and/or organic ammonia.
Specifically, in this embodiment, the co-solvent in the multifunctional agent includes, but is not limited to, ethanol, and/or methanol, and/or isopropanol, and/or n-butanol, and/or dioxane, and/or formamide, and/or acetone, and/or tetrahydrofuran; the pH regulator in the composite functional reagent comprises but is not limited to hydrochloric acid, and/or hydrofluoric acid, and/or sulfuric acid, and/or nitric acid, and/or ammonia water, and/or organic ammonia.
In a preferred embodiment of the invention, the tetraethoxysilane and the powder material are mixed in advance to form a first premixed powder material;
in this embodiment, as shown in fig. 2, step S1 specifically includes:
step S11a, laying the first premixed powder on a molding surface;
and step S12a, spraying the composite functional reagent on the molding surface by using the array piezoelectric spray head of the three-dimensional printer to form a printing layer.
Specifically, in this embodiment, the array type piezojet of the three-dimensional printer moves above the molding surface, and sprays the composite functional reagent on the specific area according to the plan view, and the spraying amount of the composite functional reagent is controlled so that the mass of water in the composite functional reagent per unit volume of the powder material is 2 to 5 times the mass of tetraethoxysilane in the first premixed powder.
In another preferred embodiment of the invention, the powder material is mixed with the composite functional reagent in advance to form a second premixed powder material;
in this embodiment, as shown in fig. 3, step S1 specifically includes:
step S11b, laying the second premixed powder on a molding surface;
and step S12b, adopting an array type piezoelectric spray head of the three-dimensional printer to spray ethyl orthosilicate on the molding surface to form a printing layer.
In another preferred embodiment of the present invention, as shown in fig. 4, step S1 specifically includes:
step S11c, laying powder material on a molding surface;
and step S12c, jetting ethyl orthosilicate on the molding surface by using a first array type piezoelectric jet head on the three-dimensional printer, and simultaneously jetting a composite functional reagent on the molding surface by using a second array type piezoelectric jet head on the three-dimensional printer to form a printing layer.
In other words, in the technical scheme of the invention, the powder material, the tetraethoxysilane and the composite functional reagent are mixed on the molding surface of each layer, and the adding mode and the adding sequence of the powder material, the tetraethoxysilane and the composite functional reagent are not limited.
In the present invention, in step S1, after the powder material (or the first premixed powder or the second premixed powder) is applied, the region where the tetraethoxysilane and/or the composite functional agent is sprayed is a specific region on the molding surface, that is, a region where a pattern to be three-dimensionally printed is provided on the molding surface, and the spraying operation is not required in a blank region on the molding surface.
In a preferred embodiment of the present invention, the ceramic precursor is processed by sintering to form a ceramic part, as shown in fig. 5, which specifically includes:
step A1, soaking the ceramic precursor in tetraethoxysilane;
step A2, placing the ceramic precursor into a composite functional reagent for soaking;
and step A3, taking out the ceramic precursor, drying and sintering to form the ceramic piece.
In a preferred embodiment of the present invention, the ceramic precursor is processed in a sintering-free manner to form a ceramic part, as shown in fig. 6, which specifically includes:
step B1, soaking the ceramic precursor in tetraethoxysilane;
step B2, placing the ceramic precursor into the composite functional reagent for soaking;
step B3, taking out the ceramic precursor and drying;
and repeating the steps B1-B3 until the ceramic piece is formed after the liquid cannot permeate into the ceramic precursor.
In a preferred embodiment of the present invention, the ceramic part is fabricated according to the steps shown in fig. 1 and 2:
fully mixing ethyl orthosilicate with silicon content of 40% and porcelain clay with the granularity of 600 meshes by using a roller mixer or other equipment according to the mass ratio of 2:100 to obtain first premixed powder; pouring water, ethanol and 35% hydrochloric acid into a container according to the mass ratio of 78:21.5:0.5, and fully stirring and mixing to obtain the composite functional reagent.
Establishing a three-dimensional model to be printed in an upper computer, slicing the model according to a set layer thickness by using software to generate a plurality of corresponding plane graphs, reading the plane graphs by the upper computer, generating dot matrix data of the plane graphs and transmitting the dot matrix data to a lower three-dimensional printer.
As shown in figure 7, the working table top 4 is cleaned, the transmission mechanism is controlled by the control circuit to drive the piston rod 2 to move downwards by 0.3mm, and the powder bed 3 connected with the piston rod through threads is driven to move downwards by the control circuit.
As shown in FIG. 8, the dusting roller 51 is controlled to lay a layer of the premixed charge 6 on the powder bed 3 in a direction parallel to the work surface 4, the laid premixed charge 6 being flush with the work surface 4.
As shown in fig. 9 and 10, after acquiring dot matrix data of a plan view, the three-dimensional printer controls the array type piezojet 8 to move, and jets the composite functional reagent in the molding area 7, and controls the jetting amount so that the mass ratio of the powder material in the jetted area to the composite functional reagent is 100: 6.
As shown in fig. 11, the infrared heating device 9 located above the molding region 7 was turned on, the temperature of the molding region 7 was raised to about 60 ℃ by irradiation, and the irradiation was continued for 3 to 5 seconds to accelerate hydrolysis and polycondensation of tetraethoxysilane and form a silica molecule crosslinked network, thereby achieving powder adhesion, and the layer thickness was 0.3mm since the powder bed 3 was moved down by 0.3 mm.
The steps of moving the powder bed 3 downwards, spreading the powder, spraying the composite functional reagent and heating the molding area are repeated, all the remaining printing layers are printed layer by layer, and as shown in fig. 12, the ceramic precursor 10 is formed by stacking and bonding layer by layer in the molding area 7.
Standing for 12 hours, taking out the ceramic precursor 10 from the powder bed, and removing and recycling the powder which is not bonded and molded; soaking the ceramic precursor 10 in ethyl orthosilicate for 2 hours, then soaking in a composite functional reagent for 2 hours, then placing in an oven 11 with a constant temperature of 60 ℃ for heat preservation for 12 hours as shown in figure 13, taking out and placing to naturally dry, placing in a muffle furnace after drying, and sintering at 1300 ℃ to obtain a high-strength and high-density ceramic part;
in this embodiment, after the ceramic precursor 10 is taken out from the powder bed, a sintering-free treatment method may be adopted: soaking the ceramic precursor 10 in ethyl orthosilicate, then soaking in a composite functional reagent, taking out and naturally drying, and repeating the soaking and drying processes for multiple times until liquid cannot permeate to obtain a high-strength and high-density ceramic part;
in the present embodiment, the powder spreading device is of a roller type, and may be changed to a scraper type as shown in fig. 14 according to circumstances.
In another preferred embodiment of the present invention, the ceramic part is fabricated according to the steps shown in fig. 1 and 3, wherein,
fully mixing a powder material and a composite functional reagent to form second premixed powder, and then spraying tetraethoxysilane by using an array type spray head;
the remaining steps are the same as those in the previous embodiment, and are not described again here.
In another preferred embodiment of the present invention, the ceramic part is fabricated according to the steps shown in fig. 1 and 4, wherein,
directly laying the powder material on a powder bed, and then respectively spraying ethyl orthosilicate and a composite functional reagent by adopting two groups of independent array piezoelectric spray heads;
the remaining steps are the same as those in the previous embodiment, and are not described again here.
While the invention has been described with reference to a preferred embodiment, it will be understood by those skilled in the art that various changes in form and detail may be made therein without departing from the spirit and scope of the invention.