CN118564762A - Repair method of underwater damaged pipeline in underground excavation and pipe jacking operation - Google Patents

Repair method of underwater damaged pipeline in underground excavation and pipe jacking operation Download PDF

Info

Publication number
CN118564762A
CN118564762A CN202410806673.XA CN202410806673A CN118564762A CN 118564762 A CN118564762 A CN 118564762A CN 202410806673 A CN202410806673 A CN 202410806673A CN 118564762 A CN118564762 A CN 118564762A
Authority
CN
China
Prior art keywords
pipeline
damaged
pipe
jacking
underwater
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN202410806673.XA
Other languages
Chinese (zh)
Other versions
CN118564762B (en
Inventor
程伟峰
邹超
周琪
赵兴达
陈雷
杨虹
胡文迪
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
PowerChina Kunming Engineering Corp Ltd
PowerChina Urban Planning and Design Institute Co Ltd
Original Assignee
PowerChina Kunming Engineering Corp Ltd
PowerChina Urban Planning and Design Institute Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by PowerChina Kunming Engineering Corp Ltd, PowerChina Urban Planning and Design Institute Co Ltd filed Critical PowerChina Kunming Engineering Corp Ltd
Priority to CN202410806673.XA priority Critical patent/CN118564762B/en
Priority claimed from CN202410806673.XA external-priority patent/CN118564762B/en
Publication of CN118564762A publication Critical patent/CN118564762A/en
Application granted granted Critical
Publication of CN118564762B publication Critical patent/CN118564762B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种暗挖顶管作业中水下破损管道的修补方法,属于管道修复技术领域,本暗挖顶管作业中水下破损管道的修补方法包括:调配用于封闭管道破损点的水硬性凝胶材料;根据破损管道的内径制备可调支撑架,由潜水员使用水硬性凝胶材料和模具在水下对管道破损点进行修补封堵;修补完成后将弧面板与修补处贴合并伸长顶杆,顶杆与管道内壁相抵,使可调支撑架对修补处形成对抗外部水压的支撑;制备直径略小于管道内径的加固环,加固环两侧预留有注浆孔;将竖井及管道积水抽干,拆卸可调支撑架,将加固环安装到管道破损点,通过注浆孔向加固环与管道的间隙注浆。

The invention discloses a method for repairing an underwater damaged pipeline in a dark excavation pipe jacking operation, and belongs to the technical field of pipeline repair. The method for repairing an underwater damaged pipeline in a dark excavation pipe jacking operation comprises: preparing a hydraulic gel material for sealing a damaged point of the pipeline; preparing an adjustable support frame according to the inner diameter of the damaged pipeline, and having a diver repair and seal the damaged point of the pipeline underwater using the hydraulic gel material and a mold; after the repair is completed, a curved panel is attached to the repaired part and a push rod is extended, and the push rod is abutted against the inner wall of the pipeline, so that the adjustable support frame forms a support for the repaired part to resist external water pressure; preparing a reinforcement ring with a diameter slightly smaller than the inner diameter of the pipeline, and grouting holes are reserved on both sides of the reinforcement ring; draining the accumulated water in the shaft and the pipeline, disassembling the adjustable support frame, installing the reinforcement ring to the damaged point of the pipeline, and grouting the gap between the reinforcement ring and the pipeline through the grouting holes.

Description

Repair method for underwater damaged pipeline in underground excavation pipe jacking operation
Technical Field
The invention relates to the technical field of pipeline repair, in particular to a repair method for a damaged pipeline under water in underground excavation pipe jacking operation.
Background
The pipe-jacking construction is an underground pipeline paving technology, the ground is not required to be excavated, and a jack pushing and machine head traction technology is adopted to pave a pipe section to a design position. The ground barrier is not needed to be considered in design, the road barrier can be cut off and straightened between two points, the construction operation surface is small, excavation and backfill are not needed, and the comprehensive cost is low. Has the advantages of no traffic blockage, road and vegetation damage, small influence on surrounding environment, and the like.
At present, the construction process for underground excavation pipe jacking operation is largely applied to urban pipe network transformation, and due to different regional differences, geological conditions are complex, and factors such as sharp stones on the pipe jacking travelling path possibly cause pipeline rupture in the pipe jacking construction process. And finally, the jacking construction of the jacking pipe is broken and water seepage is caused, so that the construction period progress is seriously influenced. A large amount of groundwater is flushed into the pipe and thus into the working well, the pipe jacking equipment, etc. are submerged.
Disclosure of Invention
The invention aims to at least solve one of the technical problems in the prior art, and therefore, the invention provides a repair method for a damaged pipeline under water in the underground pipe jacking operation, which can repair a damaged section efficiently and at low cost.
The repair method for the underwater damaged pipeline in the underground excavation jacking pipe operation comprises the following steps:
Step 1: the pressure in the pipeline is increased by injecting water into the vertical shaft, so that the water level in the vertical shaft is higher than the water level of a water source communicated with the broken point of the pipeline;
step 2: preparing a hydraulic gel material for closing a pipeline breakage point;
Step 3: preparing an adjustable support according to the inner diameter of a damaged pipeline, wherein the adjustable support comprises an arc panel, the arc panel is matched with the inner wall of the pipeline, and one side of the arc panel, which is far away from the inner wall of the pipeline, is provided with a push rod with an adjustable length;
step 4: repairing and plugging the damaged point of the pipeline underwater by using a hydraulic gel material and a mould by a diver;
Step 5: after the repair is finished, the arc panel is attached to the repair part, and the ejector rod is extended, and the ejector rod is propped against the inner wall of the pipeline, so that the adjustable support frame forms a support for the repair part against external water pressure;
step 6: preparing a reinforcing ring with the diameter slightly smaller than the inner diameter of the pipeline, and reserving grouting holes on two sides of the reinforcing ring;
Step 7: and draining accumulated water in the vertical shaft and the pipeline, disassembling the adjustable support frame, installing the reinforcing ring to the pipeline damage point, and grouting the gap between the reinforcing ring and the pipeline through the grouting hole.
The repair method for the underwater damaged pipeline in the underground excavation jacking pipe operation has at least the following beneficial effects: the hydraulic gel material meeting the underwater plugging requirement is prepared, the adjustable support frame for bearing external pressure is prepared, the repair of the damaged point is completed, the reinforcing ring is installed and grouting is carried out after the repair is completed, the repair part is further reinforced, and normal jacking operation can be continued after the reinforcement. The repair method for the underwater damaged pipeline in the underground excavation jacking pipe operation is adopted to repair the damaged point of the pipeline, so that long-term road sealing is avoided, large-scale excavation is avoided, the repair of the damaged point of the pipeline is conveniently, efficiently and cost-effectively completed, the repair structure is reliable, and the situation that the pipeline is damaged and leaked again is avoided.
According to some embodiments of the invention, after step 7, the damaged pipe is ejected out by adopting a continuous ejection mode after the repair is completed.
According to some embodiments of the invention, geological information on the jacking route is investigated before jacking the pipeline, and jacking parameters are set according to the distribution condition of the block stones.
According to some embodiments of the invention, the stroke and the jacking oil pressure of each jack in the pipe jacking machine are consistent.
According to some embodiments of the invention, in step 1, the water level of the water source communicating with the pipe break point is detected such that the water level in the shaft is 0.5m to 1m higher than the water level of the water source communicating with the pipe break point.
According to some embodiments of the invention, in step 2, the hydraulic gel material is formed by mixing cement, plugging agent, putty powder and water.
According to some embodiments of the invention, the weight ratio of cement, plugging agent, putty powder and water in the hydraulic gel material is 50:15:4:20.
According to some embodiments of the invention, the ejector rod comprises an internal thread sleeve and an external thread rod, the internal thread sleeve is in threaded fit with the external thread rod, and the whole length of the ejector rod is adjusted by screwing the external thread rod.
In step 6, according to some embodiments of the invention, cement and water glass slurries are used for grouting.
Additional aspects and advantages of the invention will be set forth in part in the description which follows, and in part will be obvious from the description, or may be learned by practice of the invention.
Drawings
The invention is further illustrated by the following examples in conjunction with the accompanying drawings:
FIG. 1 is a flow chart of a method for repairing a damaged pipeline under water in a pipe jacking operation of an embodiment of the invention;
FIG. 2 is a schematic diagram of a repair method for a damaged pipeline under water in a pipe jacking operation with an adjustable support frame for supporting the repair part;
FIG. 3 is a front view of FIG. 2;
FIG. 4 is a schematic structural view of a reinforcing ring installed in a method for repairing a damaged pipeline under water in a pipe jacking operation of the present invention;
FIG. 5 is a schematic view of the reinforcement ring of FIG. 4;
Fig. 6 is a schematic diagram of ejecting a damaged steel pipe in a repair method of a damaged pipe under water in a push pipe operation according to an embodiment of the present invention.
Reference numerals:
A shaft 100; a broken pipe 110; a pipe breakage point 111;
an adjustable support 200; an arc panel 210; a jack 220; an internally threaded sleeve 221; an external threaded rod 222;
a reinforcing ring 300; grouting holes 310.
Detailed Description
Reference will now be made in detail to the present embodiments of the present invention, examples of which are illustrated in the accompanying drawings, wherein the accompanying drawings are used to supplement the description of the written description so that one can intuitively and intuitively understand each technical feature and overall technical scheme of the present invention, but not to limit the scope of the present invention.
In the description of the present invention, it should be understood that references to orientation descriptions such as upper, lower, front, rear, left, right, etc. are based on the orientation or positional relationship shown in the drawings, are merely for convenience of description of the present invention and to simplify the description, and do not indicate or imply that the apparatus or elements referred to must have a particular orientation, be constructed and operated in a particular orientation, and thus should not be construed as limiting the present invention.
In the description of the present invention, a number means one or more, a number means two or more, and greater than, less than, exceeding, etc. are understood to not include the present number, and above, below, within, etc. are understood to include the present number. The description of the first and second is for the purpose of distinguishing between technical features only and should not be construed as indicating or implying relative importance or implicitly indicating the number of technical features indicated or implicitly indicating the precedence of the technical features indicated.
In the description of the present invention, unless explicitly defined otherwise, terms such as arrangement, installation, connection, etc. should be construed broadly and the specific meaning of the terms in the present invention can be reasonably determined by a person skilled in the art in combination with the specific contents of the technical scheme.
A repair method of a damaged pipe under water in a push bench operation according to an embodiment of the present invention will be described with reference to fig. 1 to 6.
As shown in fig. 1 to 6, the repair method for the underwater damaged pipeline in the underground excavation jacking pipe operation according to the embodiment of the invention comprises the following steps:
Step 1: increasing the pressure in the pipeline by injecting water into the vertical shaft 100, so that the water level in the vertical shaft 100 is higher than the water level of a water source communicated with the pipeline breakage point 111;
step 2: preparing a hydraulic gel material for closing the pipe breakage point 111;
Step 3: preparing an adjustable support frame 200 according to the inner diameter of the damaged pipeline 110, wherein the adjustable support frame 200 comprises an arc surface plate 210, the arc surface plate 210 is matched with the inner wall of the pipeline, and a push rod 220 with adjustable length is arranged on one side of the arc surface plate 210 away from the inner wall of the pipeline;
Step 4: repairing and plugging the pipeline breakage point 111 underwater by using a hydraulic gel material and a mould by a diver;
step 5: after the repair is completed, the cambered surface plate 210 is attached to the repair part, and the ejector rod 220 is extended, and the ejector rod 220 abuts against the inner wall of the pipeline, so that the adjustable support frame 200 forms a support for resisting external water pressure on the repair part;
Step 6: preparing a reinforcing ring 300 with a diameter slightly smaller than the inner diameter of the pipeline, and reserving grouting holes 310 on two sides of the reinforcing ring 300;
step 7: the vertical shaft 100 and the accumulated water in the pipeline are pumped out, the adjustable support frame 200 is disassembled, the reinforcing ring 300 is mounted on the pipeline breakage point 111, and the gap between the reinforcing ring 300 and the pipeline is injected through the injection holes 310.
As shown in fig. 6, after step 7, the damaged pipe 110 is ejected by continuing the ejection after the repair is completed. The damage of the pipeline generally occurs in the process of pipeline jacking, and the stone blocks on the jacking route interfere with the pipeline to damage the pipeline, so that the broken pipeline is the pipeline at the forefront end in the pipeline jacking direction, and after the damaged pipeline 110 is repaired, the pipeline jacking is continued, and the damaged pipeline 110 is jacked out at the terminal shaft 100, so that the replacement of the damaged pipeline 110 is completed, and the damaged pipeline 110 is prevented from being left underground. Compared with the pipe jacking operation without the damage of the pipeline, the pipeline at the forefront end is the damaged pipeline 110, so when the damaged pipeline 110 is jacked to the last station, a section of pipeline is jacked from the vertical shaft 100 at the starting position, the damaged pipeline 110 is jacked to the terminal vertical shaft 100, and the damaged pipeline 110 is lifted out from the terminal vertical shaft 100, therefore, the pipelines laid under the ground are all the pipelines without the damage, and the construction quality is ensured.
Geological information on the jacking route is investigated before jacking the pipeline, and jacking parameters are set according to the distribution condition of the block stones. In the jacking process, the stroke and the jacking oil pressure of each jack in the push bench are configured to be consistent.
In step 1, the water level of the water source communicating with the pipe breakage point 111 is detected such that the water level in the shaft 100 is 0.5m to 1m higher than the water level of the water source communicating with the pipe breakage point 111.
In step 2, the hydraulic gel material is formed by mixing cement, plugging agent, putty powder and water. The weight ratio of cement, plugging agent, putty powder and water in the hydraulic gel material is 50:15:4:20.
The push rod 220 comprises an internal thread sleeve 221 and an external thread rod 222, wherein the internal thread sleeve 221 is in threaded fit with the external thread rod 222, and the whole length of the push rod 220 is adjusted by screwing the external thread rod 222. After the diver submerges into the water for repair, the arc panel 210 is propped against the pipeline damage point 111, so that the situation that the water pressure outside the pipeline breaks through the repair material inwards to cause the pipeline damage point 111 to continue to leak water is avoided. After the repair is completed and the water in the shaft 100 is drained, the gap between the reinforcing ring 300 and the inner wall of the pipe is injected through the injection holes 310, and cement and water glass slurry are used for the injection.
The following describes a method for repairing a damaged underwater pipeline in the underground excavation pipe jacking operation in a specific embodiment:
As shown in fig. 6, in the process of jacking from the starting vertical shaft 100 to the finishing vertical shaft 100, when the jacking of the third section pipe is completed, the first section pipe behind the machine head is burst to be perforated, and the first section pipe is in stereo cross with the finished rainwater box culvert, so that the water leakage phenomenon occurs in the pipeline, and the jacking machine head and the whole jacking equipment thereof are submerged, so that the construction cannot be continued.
And (5) researching a jacking route in the pipeline, and confirming the influence of the block stones on the jacking route on the pipe jacking construction. The combined pipe jacking machine is adopted on site and consists of 4 jacks, the on site confirmation finds that the types of the four jacks are consistent, the strokes are consistent, the jacking oil pressure is consistent, if the strokes of the 4 jacks are inconsistent, the phenomena of pipe jacking deflection, uneven local stress, concentrated stress and the like are easily caused, and the pipe joint fracture is possibly induced. And (3) confirming the condition of the underground water source around the damaged point, wherein the damaged point is in solid intersection with the rainwater box culvert, and the drainage port of the rainwater box culvert is directly communicated with the sea surface. Along with the variation of tide, the water level in the box culvert rises and falls. And pressure difference is formed with the broken point of the pipe.
After the pipe breakage causes are investigated, the repairing method is determined and implemented, firstly, the water pressure in the pipe is increased by injecting water into the vertical shaft 100, the water level in the vertical shaft 100 is kept 0.5m to 1m higher than the water level of a water source communicated with the pipe breakage point 111, the pressure difference from inside to outside is formed, and the new repairing part is prevented from bearing external pressure.
According to the weight of cement, plugging agent, putty powder and water of 50:15:4:20, and a hydraulic gel material is prepared in the proportion of 20. The adjustable support frame 200 is manufactured according to the inner diameter of the pipeline, and further helps the repair part of the pipeline bear external pressure. The adjustable support frame 200 comprises a cambered surface plate 210, wherein the cambered surface plate 210 is matched with the inner wall of the pipeline, and a push rod 220 with adjustable length is arranged on one side of the cambered surface plate 210 away from the inner wall of the pipeline; the push rod 220 comprises an internal thread sleeve 221 and an external thread rod 222, wherein the internal thread sleeve 221 is in threaded fit with the external thread rod 222, and the whole length of the push rod 220 is adjusted by screwing the external thread rod 222. The diver submerges under water to repair the damaged point 111 of the pipeline by the hydraulic gel material, and pushes the arc panel 210 against the repair-completed place, and the arc panel 210 is pressed outwards to repair the repair place by screwing the external threaded rod 222.
Because the strength of the repair part is weaker, in order to avoid the repair part from being broken down again in the subsequent jacking process, the reinforcing ring 300 is prepared according to the inner diameter of the pipeline, the outer diameter of the reinforcing ring 300 is 1.33m, a space with the thickness of 1cm is reserved between the reinforcing ring 300 and the inner diameter of the pipeline of 1.35 for grouting, and grouting holes 310 are reserved at two sides of the reinforcing ring 300.
And draining accumulated water in the vertical shaft 100, disassembling the adjustable support frame 200, installing the reinforcing ring 300, and injecting cement and water glass slurry between the gap between the reinforcing ring 300 and the inner wall of the pipeline through the grouting holes 310 to finish repairing.
And after the repair is finished, the first section of damaged pipeline 110 behind the machine head is ejected out in a continuous ejection mode, so that the construction quality is ensured.
In summary, the hydraulic gel material meeting the underwater plugging requirement is prepared, the adjustable supporting frame 200 for bearing the external pressure is prepared, the repair of the damaged point is completed, the reinforcing ring 300 is installed and grouting is performed after the repair is completed, the repaired point is further reinforced, and normal jacking operation can be continued after the reinforcement. The repair method for the underwater damaged pipeline in the underground excavation jacking pipe operation is adopted to repair the damaged point 111 of the pipeline, long-term road sealing is avoided, large-scale excavation is avoided, the repair of the damaged point 111 of the pipeline is conveniently, efficiently and cost-effectively completed, the repair structure is reliable, and the situation that the pipeline is damaged and leaked again is avoided.
The embodiments of the present invention have been described in detail with reference to the accompanying drawings, but the present invention is not limited to the above embodiments, and various changes can be made within the knowledge of one of ordinary skill in the art without departing from the spirit of the present invention.

Claims (9)

1.一种暗挖顶管作业中水下破损管道的修补方法,其特征在于,包括:1. A method for repairing a damaged underwater pipeline in a dark excavation pipe jacking operation, characterized by comprising: 步骤1:通过向竖井内注水的方式增加管道内压力,使竖井内水位高度高于与管道破损点连通的水源的水位高度;Step 1: Increase the pressure in the pipeline by injecting water into the shaft so that the water level in the shaft is higher than the water level of the water source connected to the damaged point of the pipeline; 步骤2:调配用于封闭管道破损点的水硬性凝胶材料;Step 2: preparing a hydraulic gel material for sealing the damaged point of the pipe; 步骤3:根据破损管道的内径制备可调支撑架,可调支撑架包括弧面板,弧面板与管道内壁相吻合,弧面板远离管道内壁的一侧设置有长度可调的顶杆;Step 3: Prepare an adjustable support frame according to the inner diameter of the damaged pipe, the adjustable support frame includes a curved panel, the curved panel matches the inner wall of the pipe, and a length-adjustable mandrel is provided on the side of the curved panel away from the inner wall of the pipe; 步骤4:由潜水员使用水硬性凝胶材料和模具在水下对管道破损点进行修补封堵;Step 4: Divers use hydraulic gel materials and molds to repair and seal the damaged points of the pipeline underwater; 步骤5:修补完成后将弧面板与修补处贴合并伸长顶杆,顶杆与管道内壁相抵,使可调支撑架对修补处形成对抗外部水压的支撑;Step 5: After the repair is completed, fit the arc panel to the repaired part and extend the top rod, so that the top rod abuts against the inner wall of the pipe, so that the adjustable support frame can support the repaired part against external water pressure; 步骤6:制备直径略小于管道内径的加固环,加固环两侧预留有注浆孔;Step 6: Prepare a reinforcement ring with a diameter slightly smaller than the inner diameter of the pipe, with grouting holes reserved on both sides of the reinforcement ring; 步骤7:将竖井及管道积水抽干,拆卸可调支撑架,将加固环安装到管道破损点,通过注浆孔向加固环与管道的间隙注浆。Step 7: Drain the water from the shaft and pipeline, remove the adjustable support frame, install the reinforcement ring to the damaged point of the pipeline, and inject grout into the gap between the reinforcement ring and the pipeline through the grouting hole. 2.根据权利要求1所述的暗挖顶管作业中水下破损管道的修补方法,其特征在于,在步骤7后,修补完成后采用继续顶进的方式,将破损管道顶出。2. The method for repairing underwater damaged pipes in dark excavation and pipe jacking operations according to claim 1 is characterized in that, after step 7, the damaged pipe is pushed out by continuing to jack up after the repair is completed. 3.根据权利要求2所述的暗挖顶管作业中水下破损管道的修补方法,其特征在于,在顶进管道前调查顶进路线上的地质信息,根据块石分布情况进行顶进参数的设置。3. The method for repairing underwater damaged pipes in dark excavation and pipe jacking operations according to claim 2 is characterized in that the geological information on the jacking route is investigated before jacking the pipe, and the jacking parameters are set according to the distribution of rocks. 4.根据权利要求3所述的暗挖顶管作业中水下破损管道的修补方法,其特征在于,配置顶管机中各个千斤顶的行程、施顶油压一致。4. The method for repairing underwater damaged pipes in dark excavation and pipe jacking operations according to claim 3 is characterized in that the stroke and the jacking oil pressure of each jack in the pipe jacking machine are configured to be consistent. 5.根据权利要求1所述的暗挖顶管作业中水下破损管道的修补方法,其特征在于,在步骤1中,检测与管道破损点连通的水源的水位高度,使竖井内水位比与管道破损点连通的水源的水位高度高0.5m至1m。5. The method for repairing underwater damaged pipes in dark excavation and pipe jacking operations according to claim 1 is characterized in that, in step 1, the water level of the water source connected to the damaged point of the pipe is detected, so that the water level in the shaft is 0.5m to 1m higher than the water level of the water source connected to the damaged point of the pipe. 6.根据权利要求1所述的暗挖顶管作业中水下破损管道的修补方法,其特征在于,在步骤2中,水硬性凝胶材料由水泥、堵漏灵、腻子粉和水混合形成。6. The method for repairing underwater damaged pipes in dark excavation and pipe jacking operations according to claim 1 is characterized in that, in step 2, the hydraulic gel material is formed by mixing cement, leak-proof agent, putty powder and water. 7.根据权利要求6所述的暗挖顶管作业中水下破损管道的修补方法,其特征在于,水硬性凝胶材料中水泥、堵漏灵、腻子粉和水的重量配比为50:15:4:20。7. The method for repairing underwater damaged pipes in dark excavation and pipe jacking operations according to claim 6 is characterized in that the weight ratio of cement, leak-proof agent, putty powder and water in the hydraulic gel material is 50:15:4:20. 8.根据权利要求1所述的暗挖顶管作业中水下破损管道的修补方法,其特征在于,顶杆包括内螺纹套筒和外螺纹杆,内螺纹套筒与外螺纹杆螺纹配合,通过拧动外螺纹杆调整顶杆整体长度。8. The method for repairing underwater damaged pipes in dark excavation and pipe jacking operations according to claim 1 is characterized in that the push rod includes an internal threaded sleeve and an external threaded rod, the internal threaded sleeve is threadedly matched with the external threaded rod, and the overall length of the push rod is adjusted by twisting the external threaded rod. 9.根据权利要求1所述的暗挖顶管作业中水下破损管道的修补方法,其特征在于,在步骤6中,注浆采用水泥和水玻璃浆。9. The method for repairing underwater damaged pipes in dark excavation and pipe jacking operations according to claim 1, characterized in that in step 6, cement and water glass slurry are used for grouting.
CN202410806673.XA 2024-06-21 Repair method for underwater damaged pipeline in underground excavation pipe jacking operation Active CN118564762B (en)