JPH01126226A - 酸化物微粒子原料の合成法 - Google Patents
酸化物微粒子原料の合成法Info
- Publication number
- JPH01126226A JPH01126226A JP28464387A JP28464387A JPH01126226A JP H01126226 A JPH01126226 A JP H01126226A JP 28464387 A JP28464387 A JP 28464387A JP 28464387 A JP28464387 A JP 28464387A JP H01126226 A JPH01126226 A JP H01126226A
- Authority
- JP
- Japan
- Prior art keywords
- soln
- raw material
- dielectric constant
- water
- solvent
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Inorganic Compounds Of Heavy Metals (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP28464387A JPH01126226A (ja) | 1987-11-11 | 1987-11-11 | 酸化物微粒子原料の合成法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP28464387A JPH01126226A (ja) | 1987-11-11 | 1987-11-11 | 酸化物微粒子原料の合成法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPH01126226A true JPH01126226A (ja) | 1989-05-18 |
| JPH0574529B2 JPH0574529B2 (mo) | 1993-10-18 |
Family
ID=17681122
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP28464387A Granted JPH01126226A (ja) | 1987-11-11 | 1987-11-11 | 酸化物微粒子原料の合成法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPH01126226A (mo) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH01226721A (ja) * | 1988-03-04 | 1989-09-11 | Hakusui Chem Ind Ltd | 超伝導体製造用安定溶液及び超導薄膜の製造方法 |
| JPH03140472A (ja) * | 1989-10-27 | 1991-06-14 | Agency Of Ind Science & Technol | 酸化物微粒子堆積膜の製法 |
| KR100374704B1 (ko) * | 2000-04-07 | 2003-03-04 | 한국기계연구원 | 나노 Cu-Al₂O₃복합분말 제조방법 |
-
1987
- 1987-11-11 JP JP28464387A patent/JPH01126226A/ja active Granted
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH01226721A (ja) * | 1988-03-04 | 1989-09-11 | Hakusui Chem Ind Ltd | 超伝導体製造用安定溶液及び超導薄膜の製造方法 |
| JPH03140472A (ja) * | 1989-10-27 | 1991-06-14 | Agency Of Ind Science & Technol | 酸化物微粒子堆積膜の製法 |
| KR100374704B1 (ko) * | 2000-04-07 | 2003-03-04 | 한국기계연구원 | 나노 Cu-Al₂O₃복합분말 제조방법 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0574529B2 (mo) | 1993-10-18 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US3514252A (en) | Process for the preparation of stabilized zirconia powders | |
| US5468427A (en) | Process for making ultra-fine ceramic particles | |
| JPS63295405A (ja) | 微粉砕された粉末状組成物を製造するための方法 | |
| US5523065A (en) | Process for making ultra-fine barium titanate particles | |
| US5660774A (en) | Process for making a sintered body from ultra-fine superconductive particles | |
| US5716565A (en) | Process for making ultra-fine stabilized zirconia particles | |
| DE112006000294B4 (de) | Verfahren zur Herstellung von Pulverteilchen mit Nanogröße | |
| US5660773A (en) | Process for making ultra-fine yttrium-iron-garnet particles | |
| TWI902974B (zh) | 草酸鈦氧基鋇的製造方法及鈦酸鋇的製造方法 | |
| US5660772A (en) | Process for making ultra-fine barium hexaferrite particles | |
| JPH0574530B2 (mo) | ||
| JPH0574529B2 (mo) | ||
| JPH0572332B2 (mo) | ||
| JPH0572331B2 (mo) | ||
| JPH03141115A (ja) | 酸化イットリウム微粉末の製造方法 | |
| Ando et al. | Preparation of Pb (Mg1/3Nb2/3) O3-PbTiO3 powder by a wet chemical process | |
| JPH01294527A (ja) | Abo↓3型ペロブスカイト型金属酸化物の製造方法 | |
| JPH0784348B2 (ja) | サマリウムを含む誘電体セラミックスの製造方法 | |
| JPH01164709A (ja) | 複合酸化物前駆体の製造方法 | |
| JPH0328109A (ja) | 複合酸化物粉末の製造方法 | |
| JPS6284B2 (mo) | ||
| JPH05116943A (ja) | チタン酸バリウム粉末の製造方法 | |
| JPH0427166B2 (mo) | ||
| JP2589179B2 (ja) | 鉛系セラミックス粉末の製造方法 | |
| JPH05306121A (ja) | チタン酸バリウム系磁器原料粉末の製造方法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| EXPY | Cancellation because of completion of term |