JPH0319190B2 - - Google Patents
Info
- Publication number
- JPH0319190B2 JPH0319190B2 JP58249113A JP24911383A JPH0319190B2 JP H0319190 B2 JPH0319190 B2 JP H0319190B2 JP 58249113 A JP58249113 A JP 58249113A JP 24911383 A JP24911383 A JP 24911383A JP H0319190 B2 JPH0319190 B2 JP H0319190B2
- Authority
- JP
- Japan
- Prior art keywords
- parts
- weight
- refractory
- silica powder
- binder
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Ceramic Products (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP24911383A JPS60141680A (ja) | 1983-12-27 | 1983-12-27 | パッチング補修用耐火物の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP24911383A JPS60141680A (ja) | 1983-12-27 | 1983-12-27 | パッチング補修用耐火物の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS60141680A JPS60141680A (ja) | 1985-07-26 |
| JPH0319190B2 true JPH0319190B2 (it) | 1991-03-14 |
Family
ID=17188143
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP24911383A Granted JPS60141680A (ja) | 1983-12-27 | 1983-12-27 | パッチング補修用耐火物の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS60141680A (it) |
Families Citing this family (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| KR100655164B1 (ko) * | 2003-08-14 | 2006-12-08 | 조선내화 주식회사 | 분철광석의 환원을 위한 유동층 환원로 내의 구조물 성형에 이용되는 내화 조성물 |
| JP7732750B2 (ja) * | 2020-12-10 | 2025-09-02 | 東京窯業株式会社 | 炉内壁面の補修方法 |
Family Cites Families (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5345214A (en) * | 1976-10-05 | 1978-04-22 | Fujitsu Ltd | Demodulation circuit of position signal for magnetic recorder |
| JPS5454114A (en) * | 1977-10-06 | 1979-04-28 | Nippon Kokan Kk | Phosphateebound* nonshaped refractory |
-
1983
- 1983-12-27 JP JP24911383A patent/JPS60141680A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS60141680A (ja) | 1985-07-26 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| KR0156553B1 (ko) | 건식 내화성 조성물 | |
| HK1007733B (en) | Dry refractory composition | |
| JPH08507282A (ja) | 耐火材組成物 | |
| CN103601517A (zh) | 一种钢包工作衬用化学结合铝镁质修补料 | |
| JPH03205376A (ja) | タンディッシュ用軽量耐火性組成物 | |
| KR19980703345A (ko) | 경량의 분무가능한 턴디쉬 라이닝 조성물 | |
| US3316083A (en) | Briquetting of foundry materials | |
| AU2008252219A1 (en) | Baking repairing material | |
| US3368010A (en) | Process for making hydration resistant refractory brick | |
| JPS60141680A (ja) | パッチング補修用耐火物の製造方法 | |
| JP2831976B2 (ja) | 湿式吹付け施工法 | |
| KR20150090225A (ko) | 분무용 부정형 내화물 | |
| JP3222709B2 (ja) | 粉末状焼付け補修材 | |
| KR100356369B1 (ko) | 고로 대풍구주변 충진용 완충모르타르 내화조성물 | |
| FI85366C (fi) | Anvaendning av en formbar, eldfast, sintermagnesitbaserad massa som en tixotropisk, sjaelvhaerdande vibrationsmassa. | |
| FI117798B (fi) | Pinnoitemassa ja menetelmä pinnoitemassan järjestämiseksi pinnoitemateriaaliksi | |
| JPH0952169A (ja) | 溶鋼容器羽口用耐火物 | |
| KR100300854B1 (ko) | 제강용기용탄소질부정형내화물 | |
| KR100240751B1 (ko) | 분무보수 내화물용 결합제 | |
| JPH032822B2 (it) | ||
| JPS6152112B2 (it) | ||
| JPS5833194B2 (ja) | 不定形耐火材 | |
| JP3037625B2 (ja) | 焼付け補修材 | |
| JPH02129079A (ja) | ハイジルコン質流し込み耐火物 | |
| JPH0321505B2 (it) |