JPH03217084A - Manufacture of magnetic shield material - Google Patents
Manufacture of magnetic shield materialInfo
- Publication number
- JPH03217084A JPH03217084A JP1184990A JP1184990A JPH03217084A JP H03217084 A JPH03217084 A JP H03217084A JP 1184990 A JP1184990 A JP 1184990A JP 1184990 A JP1184990 A JP 1184990A JP H03217084 A JPH03217084 A JP H03217084A
- Authority
- JP
- Japan
- Prior art keywords
- pipe
- oxide superconductor
- magnetic shield
- cylindrical body
- pipes
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Ceased
Abstract
Description
【発明の詳細な説明】
[発明の目的]
(産業上の利用分野)
本発明は酸化物超電導体を用い、一端の閉じた筒状の磁
気シールド体を製造する方法に関する。DETAILED DESCRIPTION OF THE INVENTION [Object of the Invention] (Industrial Application Field) The present invention relates to a method of manufacturing a cylindrical magnetic shield with one end closed using an oxide superconductor.
(従来の技術)
従来、酸化物超電導体を用いて磁気シールド体を製造す
る方法としては、薄膜法、厚膜法およびバルク法などが
知られている。(Prior Art) Conventionally, known methods for manufacturing magnetic shield bodies using oxide superconductors include thin film methods, thick film methods, and bulk methods.
薄膜法としては、薄膜の形成方法で分けると、スパッタ
リング法、CvD法、MOCVD法などがあり、厚膜法
にはドクターブレード法、溶射法、スクリーン印刷法な
どがある。また、バルク法としては、粉末焼結法が代表
的な方法である。Thin film methods include sputtering, CVD, MOCVD, and the like, while thick film methods include doctor blade methods, thermal spraying, screen printing, and the like. Further, as a bulk method, a powder sintering method is a typical method.
(発明が解決しようとする問題点)
磁気シールド体は磁場の侵入をできるだけ防止する必要
があるため、一端が閉じた筒状の構造が望ましい。上記
の従来の磁気シールド体の製造方法によれば、通常、平
板状の磁気シールド体が形成されるが、これで一端の閉
じた筒状シールド体を形成しようとすると、筒の側部、
および筒側部と底部との境界部でシールド体相互をなん
らかの手段で接続する必要がある。しかし、この接続し
た継目からは磁気が漏れる恐れがある。(Problems to be Solved by the Invention) Since the magnetic shield body needs to prevent the penetration of magnetic fields as much as possible, it is desirable that the magnetic shield body has a cylindrical structure with one end closed. According to the above-mentioned conventional manufacturing method of a magnetic shield body, a flat magnetic shield body is usually formed, but when trying to form a cylindrical shield body with one end closed, the side of the cylinder,
It is also necessary to connect the shield bodies to each other by some means at the boundary between the cylinder side and the bottom. However, there is a risk that magnetism may leak from this connected joint.
また、スパッタリング法、CvD法、MOCvD法など
の薄膜法は、いずれも薄膜形成面積が小さい。また、単
結晶を基板とすることが多いことから、加工性およびコ
ストの点で問題がある。Further, thin film methods such as sputtering method, CvD method, and MOCvD method all have a small thin film formation area. In addition, since a single crystal is often used as a substrate, there are problems in terms of processability and cost.
方、ドクターブレード法、溶射法、スクリーン印刷法な
どの厚膜法は、今のところ臨界電流密度が低く、また、
大面積化時の均一性に問題がある。On the other hand, thick film methods such as doctor blade method, thermal spray method, and screen printing method currently have low critical current density, and
There is a problem with uniformity when increasing the area.
粉末焼結法が代表的な方法であるバルク法は、上記の厚
膜法の場合と同様に、今のところ臨界電流密度が低く、
また比較的薄肉で大型のシールド体を製造することは困
難であるなどの問題点がある。The bulk method, of which the powder sintering method is a typical method, currently has a low critical current density, similar to the thick film method described above.
Further, there are other problems such as the difficulty of manufacturing a relatively thin and large shield body.
本発明は磁気シールド特性に優れ、大面積、大3 ー
型化可能で、かつ継目のない一端が閉じた筒状構造の酸
化物超電導体からなる磁気シールド体を得ることを目的
とする。The object of the present invention is to obtain a magnetic shielding body made of an oxide superconductor that has excellent magnetic shielding properties, has a large area, can be made into a large three-dimensional structure, and has a seamless cylindrical structure with one end closed.
[発明の構成コ
(問題点を解決するための手段)
本発明は、銀、銅あるいはそれらの合金製のパイプを多
重管構造とし、この多重管構造のパイプとパイプの間隙
に超電導体粉末を充填した後、拡管加工する。ついで円
筒の一部を切断して超電導体を金属で挟んだ構造の平板
とする。この平板を深絞り加工して、一端が閉じた継目
のない筒状体を形成する。[Structure of the Invention (Means for Solving Problems)] The present invention comprises pipes made of silver, copper, or their alloys having a multi-tube structure, and superconducting powder being applied between the pipes of the multi-tube structure. After filling, the tube is expanded. Then, a part of the cylinder is cut to create a flat plate with a structure in which the superconductor is sandwiched between metal plates. This flat plate is deep drawn to form a seamless cylindrical body with one end closed.
(作用)
以下、本発明の製造方法について図面に基づいて説明す
る。第1図は2重管構造のパイプを使用した場合の本発
明の製造方法の説明図である。パイプ1,3の材質は銀
あるいは銅あるいはそれらの合金製のものを用いる。外
径の太いパイプ1の内径は外径の細いパイプSの外径よ
りも大きい。(Function) Hereinafter, the manufacturing method of the present invention will be explained based on the drawings. FIG. 1 is an explanatory diagram of the manufacturing method of the present invention when a pipe with a double pipe structure is used. The material of the pipes 1 and 3 is silver, copper, or an alloy thereof. The inner diameter of the pipe 1 with a larger outer diameter is larger than the outer diameter of the pipe S with a smaller outer diameter.
パイプ1とパイプSを同心状に配置することによ一 4
り、外径の太いパイプ1と外径の細いパイプ3の間隙に
空間ができる。第1図の(1)のように、この空間に酸
化物超電導体2を充填する。By arranging the pipe 1 and the pipe S concentrically, a space is created between the pipe 1 having a large outer diameter and the pipe 3 having a small outer diameter. As shown in FIG. 1 (1), this space is filled with oxide superconductor 2.
その後、押しだし、引き抜き●転造●鍛造などの手段に
より、パイプを均一に拡管して、第1図(2》のような
所定の径および長さを持った円筒とする。このとき酸化
物超電導体部分の厚さとしては0.05〜1mm程度が
適し、特に0.05〜0.3mmと、比較的薄い方が加
工の効果が大きく、焼結後の臨界電流密度が高い、すな
わちシールド特性が良い磁気シールド体が得られる。ま
た、この方法によれば大面積かつ大型なシールド体を形
成できる。After that, the pipe is uniformly expanded by extrusion, drawing, rolling, forging, etc. to form a cylinder with a predetermined diameter and length as shown in Figure 1 (2).At this time, the oxide superconductor Approximately 0.05 to 1 mm is suitable for the thickness of the body part, and in particular, the relatively thinner it is, 0.05 to 0.3 mm, the greater the processing effect, and the higher the critical current density after sintering, i.e. the shielding property. A magnetic shielding body with good magnetic properties can be obtained.Furthermore, according to this method, a large-sized shielding body with a large area can be formed.
次に、円筒の一部を切断し、第1図の(3)に示すよう
な、酸化物超電導体を金属板で挟んだ構造の平板とする
。この平板を深絞り加工して一端が閉じた筒状体を形成
する。第1図の(4)は筒状体の断面図である。Next, a part of the cylinder is cut to form a flat plate having a structure in which the oxide superconductor is sandwiched between metal plates as shown in (3) in FIG. This flat plate is deep drawn to form a cylindrical body with one end closed. (4) in FIG. 1 is a sectional view of the cylindrical body.
なお、焼結処理は深絞り加工後行なうのが基本であるが
、1回に限ったことではなく、拡管後あるいは平板を形
成した後に、圧延やプレスと組合せ複数回行なってもよ
い。加工と焼結を繰り返すことにより超電導体の組織は
緻密化し、配向性が高まるために、臨界51l,流密度
が向上し、シールド特性が良好な磁気シ ルド体を得る
ことができる。The sintering treatment is basically performed after deep drawing, but it is not limited to one time, and may be performed multiple times in combination with rolling or pressing after expanding the tube or forming a flat plate. By repeating processing and sintering, the structure of the superconductor becomes denser and its orientation increases, so that the criticality 51l and the flow density are improved, and a magnetic shield body with good shielding properties can be obtained.
さらに上述した拡径加工および焼結を繰り返すことによ
り超電導体の組織の緻密化や配同性が高まるために、さ
らに臨界電流密度が高い、すなわちシールド特性が良い
磁気シールド体を製造することができる。Furthermore, by repeating the above-mentioned diameter expanding process and sintering, the structure of the superconductor becomes denser and the alignment property is improved, so that it is possible to manufacture a magnetic shielding body with even higher critical current density, that is, better shielding properties.
上記の製造方法の例では、超電導体が一層である磁気シ
ールド体が作られるが、第2図に示すように多重管を用
いて、同様な製造方法により、超電導体層を多層とした
磁気シールド体を作ることができる。こうすることによ
り、シールド効果をさらに高めることができる。In the example of the manufacturing method described above, a magnetic shield with a layer of superconductor is manufactured, but as shown in Figure 2, a magnetic shield with multiple layers of superconductor is manufactured using a similar manufacturing method using multiple tubes. You can make a body. By doing so, the shielding effect can be further enhanced.
[発明の効果コ
本発明の製造方法によれば、臨界電流密度が高く、継目
のない、大型の、一端が閉じた酸化物超電導体を用いた
筒状磁気シールド体を形成することができる。[Effects of the Invention] According to the manufacturing method of the present invention, it is possible to form a cylindrical magnetic shield body using a large, seamless oxide superconductor with a high critical current density and one end closed.
第1図は2重管構造のパイプを用いた本発明の製造方法
の実施例の説明図、第2図は4重管構造のパイプを用い
た本発明の製造方法の実施例の説明図である。
1,3.4・・・パイプ、2,5・・・酸化物超電導体
。
−了一FIG. 1 is an explanatory diagram of an embodiment of the manufacturing method of the present invention using a pipe with a double-pipe structure, and FIG. 2 is an explanatory diagram of an embodiment of the manufacturing method of the present invention using a pipe with a quadruple-pipe structure. be. 1,3.4...pipe, 2,5...oxide superconductor. −Ryoichi
Claims (3)
法において、複数のパイプからなる多重管構造体の隣接
するパイプの間隙に酸化物超電導体を充填し、前記多重
管構造体を拡管加工により所定の径の筒状体とした後、
前記筒状体の一部を切断し、平板状にして焼結処理する
ことを特徴とする酸化物超電導体を用いた磁気シールド
体の製造方法。(1) In a method for manufacturing a magnetic shield using an oxide superconductor, an oxide superconductor is filled into the gap between adjacent pipes of a multi-tube structure consisting of a plurality of pipes, and the multi-tube structure is expanded. After making a cylindrical body with a predetermined diameter by
A method for manufacturing a magnetic shield body using an oxide superconductor, characterized in that a part of the cylindrical body is cut, flattened, and sintered.
法において、複数のパイプからなる多重管構造体の隣接
するパイプの間隙に酸化物超電導体を充填し、前記多重
管構造体を拡管加工により所定の径の筒状体とした後、
前記筒状体の一部を切断して平板状とし、深絞り加工に
よりー端が閉じた筒状体を形成し、焼結処理することを
特徴とする酸化物超電導体を用いた磁気シールド体の製
造方法。(2) In a method for manufacturing a magnetic shield using an oxide superconductor, an oxide superconductor is filled into gaps between adjacent pipes of a multi-tube structure consisting of a plurality of pipes, and the multi-tube structure is expanded. After making a cylindrical body with a predetermined diameter by
A magnetic shield using an oxide superconductor, characterized in that a part of the cylindrical body is cut into a flat plate shape, a cylindrical body with a closed end is formed by deep drawing, and the cylindrical body is sintered. How the body is manufactured.
金製パイプであることを特徴とする請求項1および2記
載の磁気シールドの製造方法。(3) The method for manufacturing a magnetic shield according to Claims 1 and 2, wherein the pipe is made of silver, copper, or an alloy thereof.