JPH0337794U - - Google Patents
Info
- Publication number
- JPH0337794U JPH0337794U JP9832489U JP9832489U JPH0337794U JP H0337794 U JPH0337794 U JP H0337794U JP 9832489 U JP9832489 U JP 9832489U JP 9832489 U JP9832489 U JP 9832489U JP H0337794 U JPH0337794 U JP H0337794U
- Authority
- JP
- Japan
- Prior art keywords
- moisture
- lamp
- absorbing film
- transparent electrode
- electroluminescent
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Description
第1図は本考案による電界発光灯の要部拡大断
面図、第2図は本考案に用いる吸湿フイルムの断
面図、第3図は従来の電界発光灯に用いられる吸
湿フイルムの断面図を示す。第4図は従来の電界
発光灯の要部拡大断面図を示す。
面図、第2図は本考案に用いる吸湿フイルムの断
面図、第3図は従来の電界発光灯に用いられる吸
湿フイルムの断面図を示す。第4図は従来の電界
発光灯の要部拡大断面図を示す。
Claims (1)
- 背面電極と透明電極により絶縁層、発光層を狭
持した電界発光素子を背面電極及び透明電極から
リードを導出して吸湿フイルムで覆い、外皮フイ
ルムで密閉封止した電界発光灯において、透明電
極上に貼り付ける吸湿フイルムの接着剤をポリオ
レフイン系接着剤としたことを特徴とする電界発
光灯。