JPH0447736Y2 - - Google Patents
Info
- Publication number
- JPH0447736Y2 JPH0447736Y2 JP7437288U JP7437288U JPH0447736Y2 JP H0447736 Y2 JPH0447736 Y2 JP H0447736Y2 JP 7437288 U JP7437288 U JP 7437288U JP 7437288 U JP7437288 U JP 7437288U JP H0447736 Y2 JPH0447736 Y2 JP H0447736Y2
- Authority
- JP
- Japan
- Prior art keywords
- label
- heat
- container
- shrinkable
- shrinkable label
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
【考案の詳細な説明】
[産業上の利用分野]
この考案は、内容物表示、装飾目的、商品の差
別化等を目的として、液体飲料容器等の容器外面
に被着される熱収縮性ラベル及びこの熱収縮性ラ
ベルを被着した容器に関するものである。[Detailed description of the invention] [Industrial application field] This invention is a heat-shrinkable label that is applied to the outer surface of containers such as liquid beverage containers for the purpose of displaying contents, decoration, product differentiation, etc. and a container covered with this heat-shrinkable label.
[従来の技術]
商品の付加価値を高め、また同種商品から差別
化する手段として容器外面に熱収縮性ラベルを被
着することが行われている。たとえば、厚み50〜
60μのポリ塩化ビニル樹脂あるいは40〜50μのポ
リスチレン樹脂、ポリエチレンテレフタレート樹
脂等からなり、美麗で目立ち易いデザインを多色
印刷で施した熱収縮性フイルムを被着したプラス
チツク製飲料容器が市場に出回つている。[Prior Art] A heat-shrinkable label is applied to the outer surface of a container as a means of increasing the added value of a product and differentiating it from similar products. For example, thickness 50~
Plastic beverage containers made of 60μ polyvinyl chloride resin, 40-50μ polystyrene resin, polyethylene terephthalate resin, etc. and covered with a heat-shrinkable film with a beautiful and easily noticeable design printed in multiple colors are now on the market. It's on.
さらに具体例に基いて説明すると、オレンジジ
ユース、グレープフルーツ等の果実飲料、スポー
ツドリンク等の中性飲料、ウーロン茶、コーヒ
ー、紅茶、ミネラルウオーター等の清涼飲料類等
を充填するプラスチツク容器で、結晶性熱可塑性
ポリマー、例えばポリエチレンテレフタレート
(PET)等からなり、キヤツプを取付ける口部か
らサポートリング、肩部、胴部を経て底部に至る
構造で、口部は無配向に結晶化され、胴部は2軸
延伸配向の結晶を有し、透明で、ヒートセツトさ
れたプラスチツクボトルが多用されており、商品
の付加価値を高め、差別化する意図から、前記熱
収縮性ラベルが使用されている。 To explain further based on specific examples, it is a plastic container filled with fruit drinks such as orange juice and grapefruit, neutral drinks such as sports drinks, soft drinks such as oolong tea, coffee, black tea, and mineral water. It is made of a plastic polymer such as polyethylene terephthalate (PET), and has a structure that extends from the opening where the cap is attached, through the support ring, shoulders, and body to the bottom. Transparent, heat-set plastic bottles with stretch-oriented crystals are often used, and the heat-shrinkable labels are used with the intention of increasing added value and differentiating products.
前記飲料物の充填温度は、70〜95℃で、通称ホ
ツトパツク品と称され、内容物充填後、予め紫外
線あるいはエチレンオキシサイドで殺菌したキヤ
ツプでネジ締めした後、さらにはまた、キヤツプ
でネジ締め後、容器を横倒しにしてキヤツプの殺
菌を行つてから正立状態に戻し、パストライザー
を通過させて、ボトル全体を74℃前後のホツトシ
ヤワーで約15分間殺菌し、常温の水を約5分間シ
ヤワーする充填、殺菌工程がとられるのがごく一
般的な工程である。 The filling temperature of the beverage is 70 to 95°C, and it is commonly called a hot pack product. After filling the contents, it is screwed with a cap that has been sterilized with ultraviolet rays or ethylene oxide, and then screwed again with the cap. After that, turn the container on its side to sterilize the cap, then return it to an upright position, pass it through the pasteurizer, sterilize the entire bottle in a hot shower at around 74℃ for about 15 minutes, and then shower it with room temperature water for about 5 minutes. A very common process is the filling and sterilization process.
高温充填用であるため、内容液が冷えると負圧
が掛かり、ボルトに歪み、凹み等の変形が生じ易
く、また殺菌手段として施されるホツトシヤワ
ー、クールシヤワーの熱履歴による変形等にも対
処し、さらに垂直方向からの外力にも耐えられる
ようにするため、胴部を補強する必要があり、ボ
トルの縦方向に延びるビームが設けられるととも
に、このビーム間に位置する凹みパネル部が複数
組設けられ、万一、変形しても目立たないように
工夫されている。 Because it is for high-temperature filling, negative pressure is applied when the content cools, which tends to cause deformation such as warping and denting of the bolt, and also prevents deformation due to the heat history of hot showers and cool showers used as a sterilization method. Furthermore, in order to withstand external forces from the vertical direction, it was necessary to reinforce the body, so a beam extending in the vertical direction of the bottle was installed, and multiple sets of recessed panels were installed between the beams. It is designed so that it will not be noticeable even if it is deformed.
第4図は、このようなプラスチツクボトルの一
例を示すもので、1は口部、2はサポートリン
グ、3は肩部、4は胴部、5は底部、6は胴部に
形成された補強用のビーム、7はビーム間に設け
られた凹みパネル部を示している。 Figure 4 shows an example of such a plastic bottle, where 1 is the mouth, 2 is the support ring, 3 is the shoulder, 4 is the body, 5 is the bottom, and 6 is the reinforcement formed on the body. The reference beam 7 indicates a recessed panel section provided between the beams.
[考案が解決しようとする課題]
ところで、このようなプラスチツクボトルに熱
収縮性ラベルを施す場合、ボトルの胴部ではな
く、上部の肩部に施されるのが通常であつた。[Problems to be Solved by the Invention] By the way, when heat-shrinkable labels are applied to such plastic bottles, they are usually applied not to the body of the bottle but to the upper shoulder.
その理由とするところは、次の通りである。 The reasons for this are as follows.
パストライザー通過時、ボトルはホツトシヤ
ワー、クールシヤワーを施されるが、この時、
胴部に施した熱収縮性ラベルとボトル外面との
僅かな隙間からホツトシヤワー、クールシヤワ
ーが入込み、胴部に設けた凹みパネルに水とな
つて溜り、輸送、保管時に流れ落ちて外装ダン
ボールを濡らし、損傷する問題があつた。ま
た、凹みパネルに溜つた水が長時間放置される
と腐敗して不衛生になり、消費者に不快感を与
え、販売低下につながるという問題もある。 When passing through the pasteurizer, the bottle is subjected to hot shower and cool shower, but at this time,
Hot shower and cool shower enters through the small gap between the heat-shrinkable label on the body and the outside of the bottle, collects as water in the recessed panel on the body, runs down during transportation and storage, and wets the outer cardboard. There was a problem with damage. Another problem is that if water accumulated in the recessed panels is left for a long time, it will rot and become unsanitary, causing discomfort to consumers and leading to a decline in sales.
ラベルの裏面に付着した水滴が表面から見
え、商品の外観を損なう。 Water droplets attached to the back side of the label are visible from the front side and spoil the appearance of the product.
ボトル胴部にラベルを被着した後、循環熱風
トンネルを通過させるが、胴部に設けた凹みパ
ネルに熱風エアーが溜り、ラベルに弛み、歪
み、しわ等が出易くなり、美麗さに欠けるた
め、ラベルあるいは容器の不良率が高くなる。 After the label is attached to the body of the bottle, it is passed through a circulating hot air tunnel, but hot air accumulates in the recessed panel provided on the body, making the label easy to loosen, warp, wrinkle, etc., and lack beauty. , the defective rate of labels or containers is high.
胴部に設けたビームの幅、凹みパネルの形
状、幅、深さ等の設計が適当でない場合、高温
充填時の負圧発生時ボトル自体が変形し、ラベ
ルの歪み、弛み等を生じる。 If the width of the beam provided in the body, the shape, width, depth, etc. of the recessed panel are not designed appropriately, the bottle itself will deform when negative pressure is generated during high-temperature filling, causing distortion and loosening of the label.
上記のような理由によつて、熱収縮性ラベルを
被着する場合、肩部に施していたのであるが、商
品の付加価値を高め、かつ他商品と差別化する目
的からすれば、できるだけラベル面積を大きくと
り、かつラベルの仕上りが良好にできる胴部への
被着が望まれるところである。 For the reasons mentioned above, heat-shrinkable labels were applied to the shoulders, but from the standpoint of increasing the added value of the product and differentiating it from other products, it is important to attach the label as much as possible. It is desired that the label be attached to the body, which can take up a large area and give a good finish to the label.
そこで、この考案の目的とするところは、外面
に凹部を有する容器に対して被着される熱収縮性
ラベルであつて、上記のようなボトルを対象とし
た場合にも前述のような問題の生じないラベルを
提供するところにあり、さらにはこのようなラベ
ルが被着された商品価値の高い容器を提供すると
ころにある。 Therefore, the purpose of this invention is to create a heat-shrinkable label that can be attached to a container that has a concave portion on its outer surface. It is an object of the present invention to provide a label that does not cause sagging, and also to provide a container having a high commercial value to which such a label is attached.
[課題を解決するための手段]
この考案に係る熱収縮性ラベルは、上記目的達
成のため、水抜き、エアー抜きの小孔を形成した
ことを特徴とするものである。[Means for Solving the Problems] In order to achieve the above object, the heat-shrinkable label according to this invention is characterized in that small holes are formed for water and air drainage.
すなわち、ポリ塩化ビニル樹脂、ポリスチレン
樹脂、ポリエチレンテレフタレート樹脂等からな
り、容器外面に被着される熱収縮性ラベルにおい
て、容器外面に形成された凹部の下端縁位置にお
いて、複数個の小孔を形成するという手段を採用
したものである。 That is, in a heat-shrinkable label made of polyvinyl chloride resin, polystyrene resin, polyethylene terephthalate resin, etc., and attached to the outer surface of a container, a plurality of small holes are formed at the lower edge position of a recess formed on the outer surface of the container. This method was adopted.
また、この考案に係る容器は、このような熱収
縮性ラベルを被着した容器であり、凹部を有する
外面に、ポリ塩化ビニル樹脂、ポリスチレン樹
脂、ポリエチレンテレフタレート樹脂等からなる
熱収縮性ラベルを被着してなる容器において、該
熱収縮性ラベルには、前記容器外面凹部の下端縁
位置において、複数個の小孔が形成されている容
器としたものである。 Moreover, the container according to this invention is a container covered with such a heat-shrinkable label, and the outer surface having the recessed portion is covered with a heat-shrinkable label made of polyvinyl chloride resin, polystyrene resin, polyethylene terephthalate resin, etc. In the container, the heat-shrinkable label has a plurality of small holes formed at the lower edge of the recess on the outer surface of the container.
[作用]
このような熱収縮性ラベルは、凹部を有する容
器外面に被着した場合においても、小孔が水抜
き、エアー抜きの作用を果たすため、ラベル背面
に水、エアーが溜らず、前述のようなホツト充填
ボトルの胴部に被着した場合にも従来に見られる
欠点が生じない。ラベル面積を大きくとれるた
め、種々の表示、装飾を施すことができる。[Function] Even when this kind of heat-shrinkable label is attached to the outer surface of a container that has a recessed part, the small holes function to drain water and air, so water and air do not accumulate on the back of the label, and the above-mentioned problem occurs. Even when it is applied to the body of a hot-filled bottle, the disadvantages seen in the prior art do not occur. Since the label area can be increased, various indications and decorations can be applied.
また、このようなラベルを被着した容器は、ラ
ベルの高付加価値化、差別化作用が有効に生かさ
れ、商品価値が高い容器となし得る。 In addition, a container with such a label can be made into a container with high commercial value by effectively utilizing the high added value and differentiation effect of the label.
[実施例]
以下さらに、高温充填ボトルに適用した第1図
乃至第3図の実施例について説明する。[Example] Hereinafter, the example shown in FIGS. 1 to 3, which is applied to a high-temperature filling bottle, will be described.
図面において、ボトルの構造は従来と同様であ
り、同一部分は同一符号で示す。すなわち、1は
口部、2はサポートリング、3は肩部、4は胴
部、5は底部、6は胴部に形成された補強用のビ
ーム、7はビーム間に設けられた凹みパネル部で
ある。8は、胴部4の全体(A部からB部)に掛
けて、さらには底部5に掛けて被着された熱収縮
性ラベルで、多色印刷による美麗で目立ち易いデ
ザインが施されている。9は、凹みパネル部7の
凹部下端縁位置においてラベル8に形成された複
数個の小孔で、格別目立たず、また、ラベルに損
傷を誘発しない程度の大きさ並びに間隔で形成す
るものとする。ビームとビーム間は、第2図のよ
うに適度な張力によつて張り渡された状態となつ
ている。 In the drawings, the structure of the bottle is the same as the conventional bottle, and the same parts are designated by the same reference numerals. That is, 1 is a mouth part, 2 is a support ring, 3 is a shoulder part, 4 is a body part, 5 is a bottom part, 6 is a reinforcing beam formed in the body part, and 7 is a concave panel part provided between the beams. It is. 8 is a heat-shrinkable label that is attached to the entire body part 4 (from part A to B) and also to the bottom part 5, and has a beautiful and easily noticeable design printed in multiple colors. . Reference numeral 9 denotes a plurality of small holes formed in the label 8 at the lower edge position of the recess of the recessed panel portion 7, which are not particularly noticeable and are formed at such a size and interval that they do not cause damage to the label. . As shown in FIG. 2, the beams are stretched with appropriate tension.
なお、上記実施例は高温充填ボトルへの適用例
を示しているが、要するに外面に凹部を有する容
器においては同様の問題が予測されるため、これ
らへの適用も除外するものではない。 In addition, although the above-mentioned example shows an example of application to a hot-filled bottle, in short, a similar problem is expected in a container having a concave portion on the outer surface, so application to these containers is not excluded.
[考案の効果]
この考案の熱収縮性ラベルは以上の通りであ
り、外面に凹部を有する容器であつても、この凹
部上面を覆う形態でラベルを被着した場合にも、
ラベル背面に水滴やエアーが残存せず、これによ
つて生起される問題を排除し得るものであり、ラ
ベル面積を大幅に拡大可能で、有効な表示、装飾
を施し得るラベルとなし得たのである。[Effects of the invention] The heat-shrinkable label of this invention is as described above, and even when the container has a recess on the outer surface, the label can be attached to cover the upper surface of the recess.
There are no water droplets or air remaining on the back of the label, which eliminates the problems caused by this, and the label area can be greatly expanded, making it possible to create a label that can be used for effective display and decoration. be.
従つて、このようなラベルを被着した容器は、
凹部を外してラベルを被着したものと比較して、
飛躍的に商品価値を高めることができるという利
点を有している。 Therefore, containers with such labels are
Compared to the one where the recess was removed and the label was attached,
It has the advantage of dramatically increasing product value.
第1図は、この考案に係る熱収縮性ラベルを被
着した高温充填ボトルを示す正面図で、ラベルの
み断面にて示す。第2図は、凹みパネル部におけ
るラベルの被着状態を示す断面図、第3図は、熱
収縮性ラベルのみの正面図、第4図は、高温充填
ボトルの説明図である。
8……熱収縮性ラベル、9……小孔。
FIG. 1 is a front view showing a hot-filling bottle covered with a heat-shrinkable label according to the invention, and only the label is shown in cross section. FIG. 2 is a cross-sectional view showing how the label is attached to the concave panel portion, FIG. 3 is a front view of only the heat-shrinkable label, and FIG. 4 is an explanatory view of the hot-filled bottle. 8...Heat-shrinkable label, 9...Small hole.
Claims (1)
リエチレンテレフタレート樹脂等からなり、容
器外面に被着される熱収縮性ラベルにおいて、
容器外面に形成された凹部の下端縁位置におい
て、複数個の小孔を形成したことを特徴とする
熱収縮性ラベル。 (2) 凹部を有する外面に、ポリ塩化ビニル樹脂、
ポリスチレン樹脂、ポリエチレンテレフタレー
ト樹脂等からなる熱収縮性ラベルを被着してな
る容器において、該熱収縮性ラベルには、前記
容器外面凹部の下端縁位置において、複数個の
小孔が形成されている容器。[Scope of claims for utility model registration] (1) A heat-shrinkable label made of polyvinyl chloride resin, polystyrene resin, polyethylene terephthalate resin, etc. and applied to the outer surface of a container,
A heat-shrinkable label characterized in that a plurality of small holes are formed at the lower edge position of a recess formed on the outer surface of a container. (2) Polyvinyl chloride resin,
In a container covered with a heat-shrinkable label made of polystyrene resin, polyethylene terephthalate resin, etc., a plurality of small holes are formed in the heat-shrinkable label at the lower edge position of the recess on the outer surface of the container. container.