JPH05258663A - Manufacture of magnetron - Google Patents
Manufacture of magnetronInfo
- Publication number
- JPH05258663A JPH05258663A JP2900493A JP2900493A JPH05258663A JP H05258663 A JPH05258663 A JP H05258663A JP 2900493 A JP2900493 A JP 2900493A JP 2900493 A JP2900493 A JP 2900493A JP H05258663 A JPH05258663 A JP H05258663A
- Authority
- JP
- Japan
- Prior art keywords
- magnetron
- sealing metal
- manufacturing
- metal bodies
- plated
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
Description
【0001】[0001]
【産業上の利用分野】本発明はマグネトロンの製造方法
に関する。FIELD OF THE INVENTION The present invention relates to a method for manufacturing a magnetron.
【0002】[0002]
【従来の技術】図1は実開昭59−95557号公報等
に見られる一般的なマグネトロン本体の側面断面図であ
る。1は陽極筒体、2は該陽極筒体の内壁に放射状に固
着されたベイン、3は陽極筒体1の軸方向にベイン2の
先端に近接して立設された陰極構体、4、5は陽極筒体
1の両端開口部に夫々一端開口部が固定された略筒状の
第1及び第2封着金属体、6は第1封着金属体4の他端
開口部にろう付固着された筒状絶縁体、7は該筒状絶縁
体にろう付固着された排気管であり、該排気管を通して
陽極筒体1内の排気が行なわれる。その後、排気管7は
ベイン2から延びるアンテナ導体8を保持した状態で筒
状絶縁体6を封止している。9は第2封着金属体5の他
端開口部を封止するべくろう付固着された有底筒状の絶
縁体である。2. Description of the Related Art FIG. 1 is a side sectional view of a general magnetron body found in Japanese Utility Model Laid-Open No. 59-95557. Reference numeral 1 is an anode cylinder, 2 is a vane radially fixed to an inner wall of the anode cylinder, and 3 is a cathode assembly which is erected upright in the axial direction of the anode cylinder 1 close to the tip of the vane 2. Is a substantially cylindrical first and second sealing metal body with one end opening fixed to each end opening of the anode cylinder 1, and 6 is brazed to the other end opening of the first sealing metal body 4. The cylindrical insulator 7 is an exhaust pipe brazed and fixed to the cylindrical insulator, and the inside of the anode cylinder 1 is exhausted through the exhaust pipe. Then, the exhaust pipe 7 seals the tubular insulator 6 while holding the antenna conductor 8 extending from the vane 2. Reference numeral 9 denotes a bottomed tubular insulator that is brazed and fixed to seal the other end opening of the second sealing metal body 5.
【0003】[0003]
【発明が解決しようとする課題】ところで、第1封着金
属体4及び第2封着金属体5は、その錆発生や腐食を防
止するためにメッキ処理が施こされるが、従来は、これ
ら封着金属体4、5を所定の形に成形した後にメッキ処
理を行なっている。By the way, the first sealing metal body 4 and the second sealing metal body 5 are plated to prevent rusting or corrosion thereof. The sealing metal bodies 4 and 5 are formed into a predetermined shape and then plated.
【0004】ところが、これら封着金属体4、5は小型
であり、筒状絶縁体6及び絶縁体9とのろう付部の湾曲
部10や曲げ部11が形成されているため、これらの部分に
メッキ処理が十分に行なわれない虞れがある。この場
合、メッキ処理がなされていない部分には錆が発生した
り、腐食が生じたりし、さらに筒状絶縁体6あるいは絶
縁体9とのろう付部にメッキ処理が十分になされていな
い場合に、確実なろう付も行なわれず、製造工程におけ
る歩留が低下する。However, since these sealing metal bodies 4 and 5 are small in size and the curved portion 10 and the bent portion 11 of the brazing portion with the tubular insulator 6 and the insulator 9 are formed, these portions are formed. However, the plating process may not be performed sufficiently. In this case, if rust occurs or corrosion occurs in the non-plated part, and if the brazing part with the tubular insulator 6 or the insulator 9 is not sufficiently plated, However, reliable brazing is not performed, and the yield in the manufacturing process is reduced.
【0005】[0005]
【課題を解決するための手段】本発明は、陽極筒体の両
端開口部に夫々固定された略筒状の第1及び第2封着金
属体を有するマグネトロンの製造方法において、該第1
及び第2封着金属体を予めメッキ処理された金属板より
形成することを特徴としたマグネトロンの製造方法であ
って、さらには上記メッキ処理はNiメッキ又はCuメ
ッキであること、また上記第1及び第2封着金属体は、
筒状絶縁体及び有底筒状絶縁体とのろう付部において、
湾曲部が形成されていることを特徴とするマグネトロン
の製造方法である。The present invention provides a method for manufacturing a magnetron having substantially cylindrical first and second sealing metal bodies, which are fixed to openings at both ends of an anode cylinder, respectively.
And the second sealing metal body is formed from a metal plate that has been plated in advance, and the plating treatment is Ni plating or Cu plating. And the second sealed metal body,
In the brazing part with the tubular insulator and the tubular insulator with a bottom,
A magnetron manufacturing method is characterized in that a curved portion is formed.
【0006】[0006]
【作用】本発明のマグネトロンの第1及び第2封着金属
体は、予めメッキ処理された金属板から成形されている
ため、曲げ部におけるメッキ処理がなされない部分など
が生じる虞れがない。Since the first and second sealing metal bodies of the magnetron of the present invention are formed from the metal plate which has been plated in advance, there is no possibility that the bent portion will not be plated.
【0007】[0007]
【実施例】本実施例におけるマグネトロンの構成は、上
述の構成と全く同一であるが、本発明の特徴は、第1封
着金属体4及び第2封着金属体5にある。即ち、第1封
着金属4及び第2封着金属5は、Niメッキ鋼板、Cu
メッキ鋼板あるいはAgメッキ鋼板等の予めメッキ処理
された金属板から成形されている。EXAMPLE The structure of the magnetron in this example is exactly the same as that described above, but the feature of the present invention resides in the first sealing metal body 4 and the second sealing metal body 5. That is, the first sealing metal 4 and the second sealing metal 5 are Ni-plated steel plate, Cu
It is formed from a pre-plated metal plate such as a plated steel plate or an Ag plated steel plate.
【0008】従って、従来のように、第1封着金属体4
及び第2封着金属体5の湾曲部10や曲げ部11にメッキ処
理がなされない部分が発生する虞れは全くなく、第1封
着金属体4及び第2封着金属体5はその全体にわたって
一様にメッキ処理されており、錆及び腐食の発生あるい
はろう付不良等を確実に防止することができる。Therefore, as in the conventional case, the first sealing metal body 4
Also, there is no possibility that the curved portion 10 and the bent portion 11 of the second sealing metal body 5 may be left unplated, and the first sealing metal body 4 and the second sealing metal body 5 as a whole. It is uniformly plated over the entire area, and it is possible to reliably prevent rust and corrosion, defective brazing, and the like.
【0009】[0009]
【発明の効果】本発明によれば、予めメッキ処理された
金属板から第1、第2封着金属体を形成するため、従来
のプレス加工後のメッキ処理のように曲げ部などで発生
しやすいメッキ不良が確実に防止でき、結果として錆の
発生や腐食を防止し、また筒状絶縁体及び有底筒状絶縁
体とのろう付を確実に行うことができるものである。According to the present invention, since the first and second sealing metal bodies are formed from the metal plate which has been subjected to the plating treatment in advance, it is generated in the bent portion like the conventional plating treatment after the press working. This makes it possible to reliably prevent easy plating failure, prevent rust from occurring and corrosion, and reliably braze the tubular insulator and the bottomed tubular insulator.
【0010】よって、製造工程における歩留を向上させ
ることができるとともに、マグネトロンの長寿命化を図
ることも可能とした。Therefore, it is possible to improve the yield in the manufacturing process and to extend the life of the magnetron.
【図1】マグネトロンの典型例を示す側面断面図であ
る。FIG. 1 is a side sectional view showing a typical example of a magnetron.
4 第1封着金属体 5 第2封着金属体 10 湾曲部 11 曲げ部 4 1st sealing metal body 5 2nd sealing metal body 10 Bending part 11 Bending part
Claims (3)
略筒状の第1及び第2封着金属体を有するマグネトロン
の製造方法において、該第1及び第2封着金属体を予め
メッキ処理された金属板より形成することを特徴とする
マグネトロンの製造方法。1. A method of manufacturing a magnetron having substantially cylindrical first and second sealing metal bodies fixed to opening portions at both ends of an anode cylinder, wherein the first and second sealing metal bodies are previously prepared. A method for manufacturing a magnetron, which is characterized in that the magnetron is formed from a plated metal plate.
ッキであることを特徴とする請求項1に記載のマグネト
ロンの製造方法。2. The method of manufacturing a magnetron according to claim 1, wherein the plating treatment is Ni plating or Cu plating.
縁体及び有底筒状絶縁体とのろう付部において、湾曲部
が形成されていることを特徴とする請求項1に記載のマ
グネトロンの製造方法。3. The first and second sealed metal bodies are characterized in that a curved portion is formed at a brazing portion between the tubular insulator and the bottomed tubular insulator. The method for manufacturing a magnetron according to 1.