JPH0574662B2 - - Google Patents

Info

Publication number
JPH0574662B2
JPH0574662B2 JP62140950A JP14095087A JPH0574662B2 JP H0574662 B2 JPH0574662 B2 JP H0574662B2 JP 62140950 A JP62140950 A JP 62140950A JP 14095087 A JP14095087 A JP 14095087A JP H0574662 B2 JPH0574662 B2 JP H0574662B2
Authority
JP
Japan
Prior art keywords
adhesive
joining
recess
fitting
members
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP62140950A
Other languages
Japanese (ja)
Other versions
JPS63304857A (en
Inventor
Tomio Takahashi
Hiroshi Tejima
Tomomi Makita
Shigeo Suyama
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Toppan Inc
Original Assignee
Toppan Printing Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Toppan Printing Co Ltd filed Critical Toppan Printing Co Ltd
Priority to JP62140950A priority Critical patent/JPS63304857A/en
Publication of JPS63304857A publication Critical patent/JPS63304857A/en
Publication of JPH0574662B2 publication Critical patent/JPH0574662B2/ja
Granted legal-status Critical Current

Description

【発明の詳細な説明】 〔産業上の利用分野〕 本発明は、枠、パネルなどの組み立て部材の接
合方法に関するものである。
DETAILED DESCRIPTION OF THE INVENTION [Field of Industrial Application] The present invention relates to a method for joining assembly members such as frames and panels.

〔従来の技術〕[Conventional technology]

従来、組み立て部材の接合方法、特に隅部で部
材を突き合わせて接合する方法としては、接合端
面に接着剤を塗布しておきダボなどの部材を用い
て固定する方法、また突起と切り欠きとを設け前
記と同様に接合端面に接着剤を塗布して、前記突
起を切り欠きに嵌合させる方法がある。さらには
二部材を突き合わせることなく一部材の一部を櫛
歯状に設けて折り曲げ接着剤を用いて固定して隅
部を形成する方法も行なわれていた。
Conventionally, methods for joining assembly members, especially joining members by butting them together at corners, include applying adhesive to the joint end surfaces and fixing them using materials such as dowels, and methods that use projections and notches. There is a method of applying an adhesive to the joining end surface in the same manner as described above, and fitting the protrusion into the notch. Furthermore, there has also been a method in which a corner portion is formed by providing a part of one member in a comb-teeth shape, bending it, and fixing it using an adhesive, without abutting the two members.

〔発明が解決しようとする問題点〕[Problem that the invention seeks to solve]

しかしながら、上記した従来の二部材の接合方
法においては、接着剤の硬化までに時間がかかる
ことから、組み上げられた製品を仮固定しなけれ
ばならず、接合端面の面積が広い場合には適さな
いといつた問題点があつた。
However, in the conventional method of joining two parts described above, since it takes time for the adhesive to harden, the assembled product must be temporarily fixed, and it is not suitable when the area of the joint end surface is large. A problem arose.

〔問題点を解決するための手段〕[Means for solving problems]

本発明は、上記した従来の問題点を考慮してな
されたもので、接合部を構成する部材それぞれの
接合端面に対して直角方向に凹部を設け、該凹部
形状に対応しかつ膨脹率105〜125%の嵌合部材に
接着剤を塗布または含浸し、前記嵌合部材を凹部
それぞれに嵌合して接合端面を接合することによ
り、上記した従来の問題点を解消するものであ
る。
The present invention has been made in consideration of the above-mentioned conventional problems, and includes providing a recess in a direction perpendicular to the joining end surface of each member constituting the joining part, and having an expansion rate of 105 to 105, which corresponds to the shape of the recess. The above-mentioned conventional problems are solved by coating or impregnating 125% of the fitting members with an adhesive, fitting the fitting members into the respective recesses, and joining the joint end surfaces.

〔作用〕[Effect]

本発明においては、凹部に嵌合された嵌合部材
が膨脹して突き合わされている二部材を仮固定
し、そののち接着剤が硬化して前記二部材を接着
固定する。
In the present invention, the fitting member fitted into the recess expands to temporarily fix the two members that are butted against each other, and then the adhesive hardens to adhesively fix the two members.

〔実施例〕〔Example〕

つぎに、本発明を第1図から第3図に示す一実
施例に基づいて詳細に説明する。
Next, the present invention will be explained in detail based on an embodiment shown in FIGS. 1 to 3.

図中1は例えば枠体Aを構成する部材で、まず
この部材1の接合端面10それぞれに凹部2を切
削して設ける。前記凹部2は接合端面10に対し
て直角な面を有する多角形となつている。
In the figure, reference numeral 1 denotes a member constituting, for example, a frame body A, and first, recesses 2 are cut and provided in each of the joining end surfaces 10 of this member 1. The recess 2 has a polygonal shape with a surface perpendicular to the joint end surface 10.

ついで、上記凹部2それぞれの形状に対応し凹
部2を合わせてなる空間Bを占める嵌合部材3に
接着剤4を塗布或は含浸させる。前記嵌合部材3
は接着剤4を塗布或は含浸した際に膨脹するもの
で、例えば酢酸ビニル系の水性エマルジヨンタイ
プの接着剤を塗布した時に、膨脹率105〜125%を
示すムク材や集成材が適し、凹部2の各内面に密
着するものであればよい。
Next, an adhesive 4 is applied or impregnated onto the fitting member 3 which corresponds to the shape of each of the recesses 2 and occupies the space B formed by combining the recesses 2. The fitting member 3
is a material that expands when applied or impregnated with adhesive 4. For example, solid wood or laminated wood that exhibits an expansion rate of 105 to 125% when applied with vinyl acetate-based aqueous emulsion type adhesive is suitable. Any material that comes into close contact with each inner surface of the recess 2 may be used.

そして嵌合部材3を凹部2に嵌合し部材1それ
ぞれの接合端面10を接合すればよく、前記嵌合
部材3が凹部2内で膨張して二部材1が仮固定さ
れ、接着剤4が硬化すると確実に部材1が接合固
定される。
Then, the fitting member 3 is fitted into the recess 2 and the joining end surfaces 10 of the members 1 are joined, and the fitting member 3 expands within the recess 2 to temporarily fix the two members 1, and the adhesive 4 Once cured, the member 1 is reliably bonded and fixed.

なお接着剤と部材との接着状態を良好とするた
めに、例えば接着剤を酢酸ビニル系の水性エマル
ジヨンタイプのものとすると、部材としては合
板、パーチクルボード、その他木質系の板材が適
している。しかし酢酸ビニル系の水性エマルジヨ
ンタイプの接着剤と接着が容易で切削が簡単なも
のであれば、これに限られるものではない。
In order to improve the adhesion between the adhesive and the member, for example, if the adhesive is of a vinyl acetate water-based emulsion type, plywood, particle board, or other wood-based board materials are suitable as the member. However, the material is not limited to this, as long as it can be easily bonded to a vinyl acetate-based aqueous emulsion type adhesive and can be easily cut.

〔発明の効果〕〔Effect of the invention〕

以上説明したように、本発明の方法によれば、
接合部を構成する部材それぞれの接合端面に対し
て直角方向に凹部を設け、該凹部形状に対応しか
つ膨脹率105〜125%の嵌合部材に接着剤を塗布ま
たは含浸し、前記嵌合部材を凹部それぞれに嵌合
して接合端面を接合するので、接着剤硬化までの
組み立て製品の仮固定や加圧が不要となつて製品
の製造工程が簡略化され、また接着剤のみを介し
て接合した場合に比べて強固に接合できるなど、
実用性にすぐれた効果を奏するものである。
As explained above, according to the method of the present invention,
A recess is provided in a direction perpendicular to the joint end surface of each member constituting the joint part, and an adhesive is applied or impregnated on the fitting member corresponding to the shape of the recess and having an expansion rate of 105 to 125%, and the fitting member is coated with or impregnated with an adhesive. Since the joint end faces are joined by fitting into each recess, there is no need to temporarily fix or pressurize the assembled product until the adhesive hardens, simplifying the product manufacturing process, and joining using only the adhesive. For example, it can be bonded more firmly than when
It has excellent practical effects.

【図面の簡単な説明】[Brief explanation of the drawing]

第1図は本発明に係る組み立て部材の接合方法
の一実施例の説明図、第2図は一実施例により組
み立てられた枠体の説明図、第3図は第2図−
線部における断面を示す説明図である。 1……部材、2……凹部、3……嵌合部材、4
……接着剤、10……接合端面。
FIG. 1 is an explanatory diagram of an embodiment of the method for joining assembly members according to the present invention, FIG. 2 is an explanatory diagram of a frame assembled according to the embodiment, and FIG.
It is an explanatory view showing a section at a line part. 1... member, 2... recess, 3... fitting member, 4
... Adhesive, 10 ... Joint end surface.

Claims (1)

【特許請求の範囲】[Claims] 1 接合部を構成する部材それぞれの接合端面に
対して直角方向に凹部を設け、該凹部形状に対応
しかつ膨脹率105〜125%の嵌合部材に接着剤を塗
布または含浸し、前記嵌合部材を凹部それぞれに
嵌合して接合端面を接合することを特徴とする組
み立て部材の接合方法。
1. A recess is provided in a direction perpendicular to the joining end surface of each member constituting the joint, and an adhesive is applied or impregnated on the fitting member corresponding to the shape of the recess and having an expansion rate of 105 to 125%, and the said fitting is A method for joining assembled members, characterized by fitting the members into respective recesses and joining the joining end surfaces.
JP62140950A 1987-06-05 1987-06-05 Connection of prefabricated member Granted JPS63304857A (en)