JPH0625737A - 一様伸びに優れた調質ht590鋼の製造方法 - Google Patents

一様伸びに優れた調質ht590鋼の製造方法

Info

Publication number
JPH0625737A
JPH0625737A JP4184199A JP18419992A JPH0625737A JP H0625737 A JPH0625737 A JP H0625737A JP 4184199 A JP4184199 A JP 4184199A JP 18419992 A JP18419992 A JP 18419992A JP H0625737 A JPH0625737 A JP H0625737A
Authority
JP
Japan
Prior art keywords
steel
uniform elongation
less
quenching
tempered
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Ceased
Application number
JP4184199A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0625737A5 (mo
Inventor
Hidesato Mabuchi
秀里 間渕
Yokika Kawashima
善樹果 川島
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nippon Steel Corp
Original Assignee
Nippon Steel Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nippon Steel Corp filed Critical Nippon Steel Corp
Priority to JP4184199A priority Critical patent/JPH0625737A/ja
Publication of JPH0625737A publication Critical patent/JPH0625737A/ja
Publication of JPH0625737A5 publication Critical patent/JPH0625737A5/ja
Ceased legal-status Critical Current

Links

Landscapes

  • Heat Treatment Of Steel (AREA)
JP4184199A 1992-07-10 1992-07-10 一様伸びに優れた調質ht590鋼の製造方法 Ceased JPH0625737A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP4184199A JPH0625737A (ja) 1992-07-10 1992-07-10 一様伸びに優れた調質ht590鋼の製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP4184199A JPH0625737A (ja) 1992-07-10 1992-07-10 一様伸びに優れた調質ht590鋼の製造方法

Publications (2)

Publication Number Publication Date
JPH0625737A true JPH0625737A (ja) 1994-02-01
JPH0625737A5 JPH0625737A5 (mo) 1996-10-08

Family

ID=16149094

Family Applications (1)

Application Number Title Priority Date Filing Date
JP4184199A Ceased JPH0625737A (ja) 1992-07-10 1992-07-10 一様伸びに優れた調質ht590鋼の製造方法

Country Status (1)

Country Link
JP (1) JPH0625737A (mo)

Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS6468421A (ja) * 1987-09-10 1989-03-14 住友金属工業株式会社 建設用高張力鋼板の製造方法
JPH0452225A (ja) * 1990-06-19 1992-02-20 Sumitomo Metal Ind Ltd 低降伏比高張力鋼板の製造法

Patent Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS6468421A (ja) * 1987-09-10 1989-03-14 住友金属工業株式会社 建設用高張力鋼板の製造方法
JPH0452225A (ja) * 1990-06-19 1992-02-20 Sumitomo Metal Ind Ltd 低降伏比高張力鋼板の製造法

Similar Documents

Publication Publication Date Title
CN109943771B (zh) 一种高韧性可焊接细晶粒结构钢板及其生产方法
CN109898024A (zh) 低屈强比TMCP型屈服345MPa建筑钢及生产方法
JP3873540B2 (ja) 高生産性・高強度圧延h形鋼の製造方法
JPH0563525B2 (mo)
JPH0452225A (ja) 低降伏比高張力鋼板の製造法
KR100370584B1 (ko) 저항복비를 가진 고강도 후강판의 제조방법
JP2706159B2 (ja) 溶接性の良好な低降伏比高張力鋼の製造方法
JP3756291B2 (ja) 高強度鉄筋の製造方法
JPS5952687B2 (ja) 低温靭性のすぐれた調質型高張力鋼板の製造法
JPS6152317A (ja) 低温靭性にすぐれた熱延鋼板の製造方法
JPH0681032A (ja) 一様伸びに優れた調質ht590鋼及びその製造方法
JPH06128630A (ja) 一様伸びの優れたht690以上の調質高張力鋼の製造方法
JPH03207814A (ja) 低降伏比高張力鋼板の製造方法
KR940008057B1 (ko) 저항복비 건축용 고장력강의 제조방법
JPH0920921A (ja) セパレーションを利用する高靱性鋼板の製造方法
JPH0670249B2 (ja) 靭性に優れた調質型高張力鋼板の製造方法
JPH04224623A (ja) 板厚方向の硬度差が小さい板厚60mm以上の50キロ級低降伏比厚肉高張力鋼板の製造方法
JPH02301517A (ja) 低降伏比高張力鋼板の製造方法
JPH06128629A (ja) 一様伸びの優れたht690以上の調質高張力鋼の製造方法
JPS6324012A (ja) 直接焼入れ焼戻し法による低降伏比高張力鋼板の製造方法
JPH03162521A (ja) 抵温靭性の優れた高張力鋼板の製造法
JPH0143006B2 (mo)
JPH04354823A (ja) 降伏比80%以下の抗張力 60kgf/mm2級鋼の製造方法
JPH06264144A (ja) 冷間成形による建築用低降伏比鋼管の製造法
JPH04321A (ja) 降伏点伸びを有し、降伏比が低く、かつ低温靭性に優れた鋼管の製造方法

Legal Events

Date Code Title Description
A02 Decision of refusal

Free format text: JAPANESE INTERMEDIATE CODE: A02

Effective date: 19980324