JPH0978286A5 - - Google Patents

Info

Publication number
JPH0978286A5
JPH0978286A5 JP7-263535A JP26353595A JPH0978286A5 JP H0978286 A5 JPH0978286 A5 JP H0978286A5 JP 26353595 A JP26353595 A JP 26353595A JP H0978286 A5 JPH0978286 A5 JP H0978286A5
Authority
JP
Japan
Prior art keywords
soluble
amendment
concentration
compound
amended
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP7-263535A
Other languages
Japanese (ja)
Other versions
JP2732044B2 (en
JPH0978286A (en
Filing date
Publication date
Application filed filed Critical
Priority to JP7263535A priority Critical patent/JP2732044B2/en
Priority claimed from JP7263535A external-priority patent/JP2732044B2/en
Publication of JPH0978286A publication Critical patent/JPH0978286A/en
Application granted granted Critical
Publication of JP2732044B2 publication Critical patent/JP2732044B2/en
Publication of JPH0978286A5 publication Critical patent/JPH0978286A5/ja
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Description

【手続補正書】[Procedural Amendment Document]

【提出日】平成8年12月18日[Date of submission] December 18, 1996

【手続補正2】[Procedural Amendment 2]

【補正対象書類名】明細書[Document to be amended] Statement

【補正対象項目名】0005[Item name to be corrected] 0005

【補正方法】変更[Correction Method] Change

【補正内容】[Correction Details]

【0005】[0005]

【課題を解決するための手段】即ち、本発明白色銅合金
メッキ液は、可溶性銅シアン化物及び可溶性パラジウム
化合物に加え可溶性亜鉛化合物又は可溶性第二スズ化合
物を含有せしめ、界面活性剤0.1〜5ml/L、ピロ
リン酸塩5〜120g/L、アンモニア1〜50g/L
を添加するとともに遊離シアン濃度を40〜60g/
L、pHを11〜13に調整したことを特徴とする。
[Means for Solving the Problem] In other words, the white copper alloy plating solution of the present invention contains a soluble copper cyanide and a soluble palladium compound, in addition to a soluble zinc compound or a soluble stannic compound, and contains 0.1 to 5 ml/L of surfactant, 5 to 120 g/L of pyrophosphate, and 1 to 50 g/L of ammonia.
Add the following and increase the free cyanide concentration to 40-60 g/
The product is characterized by adjusting the L and pH to 11-13.

Claims (1)

【手続補正書】 【提出日】平成8年12月18日 【手続補正1】 【補正対象書類名】明細書 【補正対象項目名】請求項1 【補正方法】変更 【補正内容】[Procedural Amendment] [Date of Submission] December 18, 1996 [Procedural Amendment 1] [Document to be Amended] Specification [Item to be Amended] Claim 1 [Method of Amendment] Change [Content of Amendment] 【請求項1】可溶性銅シアン化物及び可溶性パラジウム
化合物に加え可溶性亜鉛化合物又は可溶性第二スズ化合
物を含有せしめ、界面活性剤0.1〜5ml/L、ピロ
リン酸塩5〜120g/L)アンモニア1〜50g/L
を添加するとともに遊離シアン濃度を40〜60g/
L、pHを11〜13に調整したことを特徴とする白色
銅合金メッキ液。
[Claim 1] A mixture containing a soluble copper cyanide and a soluble palladium compound, in addition to a soluble zinc compound or a soluble stannous compound, with a surfactant concentration of 0.1 to 5 ml/L, a pyrophosphate concentration of 5 to 120 g/L, and an ammonia concentration of 1 to 50 g/L.
Add the following and increase the free cyanide concentration to 40-60 g/
A white copper alloy plating solution characterized by having a pH adjusted to 11-13.
JP7263535A 1995-09-18 1995-09-18 White copper alloy plating solution Expired - Lifetime JP2732044B2 (en)