JPH1170530A - Mold for molding disk - Google Patents

Mold for molding disk

Info

Publication number
JPH1170530A
JPH1170530A JP23386997A JP23386997A JPH1170530A JP H1170530 A JPH1170530 A JP H1170530A JP 23386997 A JP23386997 A JP 23386997A JP 23386997 A JP23386997 A JP 23386997A JP H1170530 A JPH1170530 A JP H1170530A
Authority
JP
Japan
Prior art keywords
compression
core
mold
guide ring
piston
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP23386997A
Other languages
Japanese (ja)
Other versions
JP3414995B2 (en
Inventor
Yuji Shibuya
裕二 渋谷
Shigeru Hatano
成 波多野
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Seikoh Giken Co Ltd
Sumitomo Heavy Industries Ltd
Original Assignee
Seikoh Giken Co Ltd
Sumitomo Heavy Industries Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Seikoh Giken Co Ltd, Sumitomo Heavy Industries Ltd filed Critical Seikoh Giken Co Ltd
Priority to JP23386997A priority Critical patent/JP3414995B2/en
Publication of JPH1170530A publication Critical patent/JPH1170530A/en
Application granted granted Critical
Publication of JP3414995B2 publication Critical patent/JP3414995B2/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

PROBLEM TO BE SOLVED: To eliminate time lag between a timing when a compression piston starts moving forward and a timing when a compression core starts moving forward. SOLUTION: The mold for molding a disk comprises a fixed side guide ring 18 having a stamper 21 mounted thereat, a movable side guide ring 23 arranged oppositely to the ring 18, a compression core 24 approachably and retractably arranged on an inner peripheral side of the ring 23, and a compression piston 37 forwarded by a driving means to forward the core 24. And, when the core 24 is disposed at a rear stopping position and the piston 37 is disposed at a retracted limit position, the core 24 is brought into contact with the piston 37. When the core 24 is forwarded to tend to compress resin, time lag between timing when the piston 37 starts moving forward and timing when the core 24 starts moving forward does not occur.

Description

【発明の詳細な説明】DETAILED DESCRIPTION OF THE INVENTION

【0001】[0001]

【発明の属する技術分野】本発明は、ディスク成形用金
型に関するものである。
BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a disk molding die.

【0002】[0002]

【従来の技術】従来、ディスク成形用の射出成形機にお
いては、加熱シリンダ内において溶融させた樹脂を、デ
ィスク成形用金型のキャビティ空間に充填(てん)し、
冷却することによってディスク基板を成形するようにし
ている。そして、前記キャビティ空間に臨ませてスタン
パが配設され、該スタンパの凹凸が前記ディスク基板の
情報面に転写されるようになっている。
2. Description of the Related Art Conventionally, in an injection molding machine for disk molding, a resin melted in a heating cylinder is filled in a cavity space of a disk molding die.
The disk substrate is formed by cooling. Then, a stamper is provided facing the cavity space, and the irregularities of the stamper are transferred to the information surface of the disk substrate.

【0003】図2は従来のディスク成形用金型における
圧縮コアの後退状態を示す図、図3は従来のディスク成
形用金型における圧縮コアの前進状態を示す図である。
図において、31は固定プラテン、11は該固定プラテ
ン31に取り付けられた固定金型、32は可動プラテ
ン、12は該可動プラテン32に取り付けられ、前記固
定金型11に対して進退自在にかつ接離自在に配設され
た可動金型である。該可動金型12を図示しない型締機
構によって前進 (図における右方に移動)させることに
より、型閉じが行われ、固定金型11と可動金型12と
の間にキャビティ空間15が形成される。そして、前記
型締機構によって可動金型12に型締力を与えることに
より、型締めが行われ、その状態で前記キャビティ空間
15に樹脂が充填されるとともに、可動金型12の圧縮
コア24が前進させられ、圧縮が行われる。その後、前
記型締機構によって可動金型12を後退 (図における左
方に移動) させることにより、型開きが行われ、図示し
ないディスクが成形される。
FIG. 2 is a diagram showing a retracted state of a compression core in a conventional disk molding die, and FIG. 3 is a diagram showing an advanced state of a compression core in a conventional disk molding die.
In the figure, 31 is a fixed platen, 11 is a fixed mold attached to the fixed platen 31, 32 is a movable platen, and 12 is attached to the movable platen 32 so as to be able to advance and retreat with respect to the fixed mold 11 and to make contact therewith. It is a movable mold that is arranged detachably. The movable mold 12 is advanced (moved to the right in the figure) by a mold clamping mechanism (not shown) to close the mold, and a cavity space 15 is formed between the fixed mold 11 and the movable mold 12. You. The mold clamping is performed by applying a mold clamping force to the movable mold 12 by the mold clamping mechanism. In this state, the cavity space 15 is filled with resin, and the compression core 24 of the movable mold 12 is removed. It is advanced and compression takes place. Thereafter, the movable mold 12 is retracted (moved to the left in the figure) by the mold clamping mechanism, whereby the mold is opened and a disc (not shown) is formed.

【0004】前記固定金型11は、図示しない加熱シリ
ンダの射出ノズルから射出された樹脂を受けるスプルー
ブッシュ16、該スプルーブッシュ16の外周に配設さ
れた環状のインナスタンパホルダ17、該インナスタン
パホルダ17の更に外周に配設された固定側ガイドリン
グ18、前記キャビティ空間15の外周面を設定する外
周リング19、及び前記インナスタンパホルダ17によ
って固定側ガイドリング18に取り付けられたスタンパ
21から成る。なお、前記スプルーブッシュ16には、
前記射出ノズルから射出された樹脂をキャビティ空間1
5に送るためのスプルー22が形成される。
[0004] The stationary mold 11 includes a sprue bush 16 for receiving resin injected from an injection nozzle of a heating cylinder (not shown), an annular inner stamper holder 17 disposed on the outer periphery of the sprue bush 16, and an inner stamper holder. A fixed-side guide ring 18 is further provided on the outer periphery of the outer ring 17, an outer ring 19 for setting the outer peripheral surface of the cavity 15, and a stamper 21 attached to the fixed-side guide ring 18 by the inner stamper holder 17. The sprue bush 16 includes
The resin injected from the injection nozzle is transferred to the cavity 1
5 is formed.

【0005】また、前記可動金型12は、前記固定側ガ
イドリング18と対向させて配設され、環状の底部26
及び筒状部27から成る皿状の可動側ガイドリング2
3、並びに該可動側ガイドリング23の内側において、
可動側ガイドリング23に対して進退自在に配設された
圧縮コア24から成る。該圧縮コア24には、固定側ガ
イドリング18側に向けて突出させて圧縮凸部25、前
記筒状部27の内周に沿って形成された大径部34、及
び前記底部26の内周に沿って形成された小径部35が
形成されるとともに、圧縮コア24の中央には、図示し
ないカットパンチを進退させるための穴29が軸方向に
貫通させて形成される。
The movable mold 12 is disposed so as to face the fixed-side guide ring 18 and has an annular bottom 26.
And movable plate-like guide ring 2 including a cylindrical portion 27
3, and inside the movable side guide ring 23,
It is composed of a compression core 24 arranged to be able to move forward and backward with respect to the movable side guide ring 23. The compression core 24 protrudes toward the fixed guide ring 18 side, and has a compression protrusion 25, a large diameter portion 34 formed along the inner circumference of the cylindrical portion 27, and an inner circumference of the bottom 26. Is formed along with a small diameter portion 35, and at the center of the compression core 24, a hole 29 for moving a cut punch (not shown) is formed to penetrate in the axial direction.

【0006】そして、前記可動側ガイドリング23に対
して圧縮コア24を進退させるために、前記可動プラテ
ン32の中央にシリンダ空間33が形成され、該シリン
ダ空間33内には、前記小径部35と対向させて圧縮ピ
ストン37が進退自在に配設される。また、型締め時に
おいて固定側ガイドリング18と可動側ガイドリング2
3とをいんろう接合することができるように、固定側ガ
イドリング18の外周にテーパ面S1が、筒状部27の
内周にテーパ面S2がそれぞれ形成される。そして、圧
縮時において外周リング19と圧縮コア24とをいんろ
う接合することができるように、外周リング19の内周
にテーパ面S3が、圧縮凸部25の外周にテーパ面S4
がそれぞれ形成される。
A cylinder space 33 is formed at the center of the movable platen 32 in order to advance and retreat the compression core 24 with respect to the movable side guide ring 23. The compression piston 37 is provided so as to be able to advance and retreat in opposition. When the mold is clamped, the fixed side guide ring 18 and the movable side guide ring 2
A tapered surface S1 is formed on the outer periphery of the fixed-side guide ring 18 and a tapered surface S2 is formed on the inner periphery of the cylindrical portion 27 so that the fixed member 3 and the third member 3 can be joined. Then, a tapered surface S3 is formed on the inner periphery of the outer ring 19, and a tapered surface S4 is formed on the outer periphery of the compression convex portion 25 so that the outer ring 19 and the compression core 24 can be joined together during the compression.
Are respectively formed.

【0007】前記構成のディスク成形用金型において、
前記可動金型12を前進させ、型閉じ及び型締めを行っ
た後、キャビティ空間15に樹脂が充填されると、図2
に示すように、前記圧縮コア24は、樹脂の圧力を受け
て後退させられ、底部26の前端面S5と大径部34の
後端面S6とが当接する後方停止位置で停止させられ
る。そして、所定のタイミングで、図3に示すように、
図示しない駆動手段によって前記圧縮ピストン37を後
退限位置から前進させると、圧縮コア24は圧縮ピスト
ン37の押圧力によって前進させられ、キャビティ空間
15内の樹脂が圧縮される。なお、前記圧縮コア24の
後方停止位置は、小径部35の後端面S10が可動プラ
テン32の前端面S8より距離L2だけ前方になるよう
に設定され、前記圧縮ピストン37の後退限位置は、圧
縮ピストン37の前端面S7が可動プラテン32の前端
面S8より距離L1だけ後方になるように設定される。
In the disk molding die having the above structure,
After the movable mold 12 is advanced, the mold is closed and the mold is clamped, and the cavity space 15 is filled with resin, FIG.
As shown in (2), the compression core 24 is retracted by receiving the pressure of the resin, and is stopped at the rear stop position where the front end surface S5 of the bottom portion 26 and the rear end surface S6 of the large diameter portion 34 abut. Then, at a predetermined timing, as shown in FIG.
When the compression piston 37 is advanced from the retreat limit position by drive means (not shown), the compression core 24 is advanced by the pressing force of the compression piston 37, and the resin in the cavity space 15 is compressed. The rearward stop position of the compression core 24 is set such that the rear end surface S10 of the small diameter portion 35 is ahead of the front end surface S8 of the movable platen 32 by a distance L2. The front end face S7 of the piston 37 is set to be behind the front end face S8 of the movable platen 32 by a distance L1.

【0008】次に、キャビティ空間15内の樹脂を冷却
することによってディスク基板が成形され、前記カット
パンチを前進させることによってディスク基板に穴あけ
加工が施される。その後、前記可動金型12を後退させ
て型開きを行うと、前記ディスクを得ることができる。
なお、このとき、圧縮ピストン37は後退限位置に後退
させられる。
Next, the disc substrate is formed by cooling the resin in the cavity space 15, and the disc substrate is perforated by advancing the cut punch. Thereafter, when the movable mold 12 is retracted and the mold is opened, the disk can be obtained.
At this time, the compression piston 37 is retracted to the retreat limit position.

【0009】前記構成のディスク成形用金型において
は、前記キャビティ空間15に樹脂が充填された後、所
定のタイミングで圧縮ピストン37が前進させられてキ
ャビティ空間15内の樹脂の圧力が高くされるようにな
っている。したがって、前記スタンパ21の凹凸がディ
スク基板の情報面に良好に転写される。
In the disk molding die having the above-described structure, after the cavity space 15 is filled with the resin, the compression piston 37 is advanced at a predetermined timing so that the pressure of the resin in the cavity space 15 is increased. It has become. Therefore, the irregularities of the stamper 21 are well transferred to the information surface of the disk substrate.

【0010】[0010]

【発明が解決しようとする課題】しかしながら、前記従
来のディスク成形用金型においては、圧縮コア24が後
方停止位置に置かれ、圧縮ピストン37が後退限位置に
置かれたときに、小径部35の後端面S10と圧縮ピス
トン37の前端面S7との間に距離(L1+L2)の間
隙(げき)が形成されてしまう。
However, in the above-described conventional disk molding die, when the compression core 24 is located at the rear stop position and the compression piston 37 is located at the retreat limit position, the small diameter portion 35 is not moved. A gap (gap) of a distance (L1 + L2) is formed between the rear end surface S10 and the front end surface S7 of the compression piston 37.

【0011】したがって、前記圧縮ピストン37を前進
させて樹脂を圧縮するときに、圧縮ピストン37が前進
を開始するタイミングと、圧縮ピストン37の前端面S
7が小径部35の後端面S10に当たって実際に圧縮コ
ア24が前進を開始するタイミングとの間に、わずかな
時間のずれが生じてしまう。その結果、成形条件の設定
が複雑になるだけでなく、高密度のディスクを高精度で
得ることができなくなってしまう。
Therefore, when the compression piston 37 is advanced to compress the resin, the timing at which the compression piston 37 starts to advance and the front end surface S
There is a slight time lag between the timing at which the compression core 24 starts moving forward when the rear end face S10 of the small-diameter portion 35 hits. As a result, not only the setting of molding conditions becomes complicated, but also it becomes impossible to obtain a high-density disk with high accuracy.

【0012】本発明は、前記従来のディスク成形用金型
の問題点を解決して、圧縮ピストンが前進を開始するタ
イミングと、実際に圧縮コアが前進を開始するタイミン
グとの間に、時間のずれが生じることがなく、成形条件
の設定を簡素化することができ、高密度のディスクを高
精度で得ることができるディスク成形用金型を提供する
ことを目的とする。
The present invention solves the problem of the conventional disk molding die described above, and provides a time interval between the timing when the compression piston starts to advance and the timing when the compression core actually starts to advance. It is an object of the present invention to provide a disk molding die capable of simplifying setting of molding conditions without causing displacement, and obtaining a high-density disk with high accuracy.

【0013】[0013]

【課題を解決するための手段】そのために、本発明のデ
ィスク成形用金型においては、スタンパが取り付けられ
た固定側ガイドリングと、該固定側ガイドリングと対向
させて配設された可動側ガイドリングと、該可動側ガイ
ドリングの内周側に進退自在に配設された圧縮コアと、
駆動手段によって前進させられ、前記圧縮コアを前進さ
せる圧縮ピストンとを有する。
For this purpose, in the disk molding die of the present invention, a fixed side guide ring on which a stamper is mounted and a movable side guide arranged opposite to the fixed side guide ring. A ring, a compression core disposed on the inner peripheral side of the movable side guide ring so as to be able to advance and retreat,
A compression piston which is advanced by driving means and which advances the compression core.

【0014】そして、前記圧縮コアが後方停止位置に置
かれ、圧縮ピストンが後退限位置に置かれたときに、圧
縮コアと圧縮ピストンとは当接させられる。
[0014] When the compression core is located at the rear stop position and the compression piston is located at the retreat limit position, the compression core and the compression piston are brought into contact with each other.

【0015】[0015]

【発明の実施の形態】以下、本発明の実施の形態につい
て図面を参照しながら詳細に説明する。図1は本発明の
実施の形態における圧縮コアの後退状態を示す図、図4
は本発明の実施の形態における圧縮コアの前進状態を示
す図である。図において、31は固定プラテン、11は
該固定プラテン31に取り付けられた固定金型、32は
可動プラテン、12は該可動プラテン32に取り付けら
れ、前記固定金型11に対して進退自在にかつ接離自在
に配設された可動金型である。該可動金型12を図示し
ない型締機構によって前進 (図における右方に移動)さ
せることにより、型閉じが行われ、固定金型11と可動
金型12との間にキャビティ空間15が形成される。そ
して、前記型締機構によって可動金型12に型締力を与
えることにより、型締めが行われ、その状態で前記キャ
ビティ空間15に樹脂が充填されるとともに、可動金型
12の圧縮コア24が前進させられ、圧縮が行われる。
その後、前記型締機構によって可動金型12を後退 (図
における左方に移動) させることにより、型開きが行わ
れ、図示しないディスクが成形される。
Embodiments of the present invention will be described below in detail with reference to the drawings. FIG. 1 is a diagram showing a retracted state of a compressed core according to an embodiment of the present invention.
FIG. 3 is a diagram showing a forward state of a compression core according to the embodiment of the present invention. In the figure, 31 is a fixed platen, 11 is a fixed mold attached to the fixed platen 31, 32 is a movable platen, and 12 is attached to the movable platen 32 so as to be able to advance and retreat with respect to the fixed mold 11 and to make contact therewith. It is a movable mold that is arranged detachably. The movable mold 12 is advanced (moved to the right in the figure) by a mold clamping mechanism (not shown) to close the mold, and a cavity space 15 is formed between the fixed mold 11 and the movable mold 12. You. Then, by applying a mold clamping force to the movable mold 12 by the mold clamping mechanism, mold clamping is performed. In this state, the cavity space 15 is filled with resin, and the compression core 24 of the movable mold 12 is removed. It is advanced and compression takes place.
Thereafter, the movable mold 12 is retracted (moved to the left in the figure) by the mold clamping mechanism, whereby the mold is opened and a disc (not shown) is formed.

【0016】前記固定金型11は、図示しない加熱シリ
ンダの射出ノズルから射出された樹脂を受けるスプルー
ブッシュ16、該スプルーブッシュ16の外周に配設さ
れた環状のインナスタンパホルダ17、該インナスタン
パホルダ17の更に外周に配設された固定側ガイドリン
グ18、前記キャビティ空間15の外周面を設定する外
周リング19、及び前記インナスタンパホルダ17によ
って固定側ガイドリング18に取り付けられたスタンパ
21から成る。なお、前記スプルーブッシュ16には、
前記射出ノズルから射出された樹脂をキャビティ空間1
5に送るためのスプルー22が形成される。
The fixed mold 11 includes a sprue bush 16 for receiving resin injected from an injection nozzle of a heating cylinder (not shown), an annular inner stamper holder 17 disposed on the outer periphery of the sprue bush 16, and an inner stamper holder. It comprises a fixed side guide ring 18 further disposed on the outer periphery of the outer ring 17, an outer ring 19 defining an outer peripheral surface of the cavity space 15, and a stamper 21 attached to the fixed side guide ring 18 by the inner stamper holder 17. The sprue bush 16 includes
The resin injected from the injection nozzle is transferred to the cavity 1
5 is formed.

【0017】また、前記可動金型12は、前記固定側ガ
イドリング18と対向させて配設され、環状の底部26
及び筒状部27から成る皿状の可動側ガイドリング2
3、並びに該可動側ガイドリング23の内側において、
可動側ガイドリング23に対して進退自在に配設された
圧縮コア24から成る。該圧縮コア24には、固定側ガ
イドリング18側に向けて突出させて圧縮凸部25、前
記筒状部27の内周に沿って形成された大径部34、及
び前記底部26の内周に沿って形成された小径部35が
形成されるとともに、圧縮コア24の中央には、図示し
ないカットパンチを進退させるための穴29が軸方向に
貫通させて形成される。
The movable mold 12 is disposed so as to face the fixed-side guide ring 18 and has an annular bottom 26.
And movable plate-like guide ring 2 including a cylindrical portion 27
3, and inside the movable side guide ring 23,
It is composed of a compression core 24 arranged to be able to move forward and backward with respect to the movable side guide ring 23. The compression core 24 protrudes toward the fixed guide ring 18 side, and has a compression protrusion 25, a large diameter portion 34 formed along the inner circumference of the cylindrical portion 27, and an inner circumference of the bottom 26. Is formed along with a small diameter portion 35, and at the center of the compression core 24, a hole 29 for moving a cut punch (not shown) is formed so as to penetrate in the axial direction.

【0018】そして、前記可動側ガイドリング23に対
して圧縮コア24を進退させるために、前記可動プラテ
ン32の中央にシリンダ空間33が形成され、該シリン
ダ空間33内には、前記小径部35と対向させて圧縮ピ
ストン37が進退自在に配設される。また、型締め時に
おいて固定側ガイドリング18と可動側ガイドリング2
3とをいんろう接合することができるように、固定側ガ
イドリング18の外周にテーパ面S1が、筒状部27の
内周にテーパ面S2がそれぞれ形成される。そして、圧
縮時において外周リング19と圧縮コア24とをいんろ
う接合することができるように、外周リング19の内周
にテーパ面S3が、圧縮凸部25の外周にテーパ面S4
がそれぞれ形成される。
A cylinder space 33 is formed in the center of the movable platen 32 in order to advance and retreat the compression core 24 with respect to the movable side guide ring 23. The compression piston 37 is provided so as to be able to advance and retreat in opposition. When the mold is clamped, the fixed side guide ring 18 and the movable side guide ring 2
A tapered surface S1 is formed on the outer periphery of the fixed-side guide ring 18 and a tapered surface S2 is formed on the inner periphery of the cylindrical portion 27 so that the fixed member 3 and the third member 3 can be joined. Then, a tapered surface S3 is formed on the inner periphery of the outer ring 19, and a tapered surface S4 is formed on the outer periphery of the compression convex portion 25 so that the outer ring 19 and the compression core 24 can be joined together during the compression.
Are respectively formed.

【0019】前記構成のディスク成形用金型において、
前記可動金型12を前進させ、型閉じ及び型締めを行っ
た後、キャビティ空間15に樹脂が充填されると、図1
に示すように、前記圧縮コア24は、樹脂の圧力を受け
て後退させられ、圧縮ピストン37の前端面S7と小径
部35の後端面S10とが当接する後方停止位置で停止
させられる。そして、所定のタイミングで、図4に示す
ように、図示しない油圧装置等の駆動手段によって前記
圧縮ピストン37を後退限位置から前進させると、圧縮
コア24は圧縮ピストン37の押圧力によって前進させ
られ、キャビティ空間15内の樹脂が圧縮される。な
お、前記圧縮コア24の後方停止位置は、小径部35の
後端面S10が可動プラテン32の前端面S8より距離
L2だけ前方になるように設定され、前記圧縮ピストン
37の後退限位置は、圧縮ピストン37の前端面S7が
可動プラテン32の前端面S8より距離L2だけ前方に
なるように設定される。
In the above-described disk molding die,
After the movable mold 12 is advanced, the mold is closed and the mold is closed, and the cavity space 15 is filled with resin, FIG.
As shown in (5), the compression core 24 is retracted by receiving the pressure of the resin, and is stopped at a rear stop position where the front end surface S7 of the compression piston 37 and the rear end surface S10 of the small diameter portion 35 abut. At a predetermined timing, as shown in FIG. 4, when the compression piston 37 is advanced from the retreat limit position by driving means such as a hydraulic device (not shown), the compression core 24 is advanced by the pressing force of the compression piston 37. Then, the resin in the cavity space 15 is compressed. The rearward stop position of the compression core 24 is set such that the rear end surface S10 of the small diameter portion 35 is ahead of the front end surface S8 of the movable platen 32 by a distance L2. The front end face S7 of the piston 37 is set to be ahead of the front end face S8 of the movable platen 32 by a distance L2.

【0020】次に、キャビティ空間15内の樹脂を冷却
することによってディスク基板が成形され、前記カット
パンチを前進させることによってディスク基板に穴あけ
加工が施される。その後、前記可動金型12を後退させ
て型開きを行うと、前記ディスクを得ることができる。
なお、このとき、圧縮ピストン37は後退限位置に後退
させられる。
Next, the resin in the cavity space 15 is cooled to form a disk substrate, and the disk substrate is punched by advancing the cut punch. Thereafter, when the movable mold 12 is retracted and the mold is opened, the disk can be obtained.
At this time, the compression piston 37 is retracted to the retreat limit position.

【0021】前記構成のディスク成形用金型において
は、前記キャビティ空間15に樹脂が充填された後、所
定のタイミングで圧縮ピストン37が前進させられてキ
ャビティ空間15内の樹脂の圧力が高くされるようにな
っている。したがって、前記スタンパ21の凹凸がディ
スク基板の情報面に良好に転写される。ところで、圧縮
コア24が後方停止位置に置かれ、圧縮ピストン37が
後退限位置に置かれたときに、小径部35の後端面S1
0と圧縮ピストン37の前端面S7とは当接させられ
る。
In the above-described disk molding die, after the cavity space 15 is filled with resin, the compression piston 37 is advanced at a predetermined timing so that the pressure of the resin in the cavity space 15 is increased. It has become. Therefore, the irregularities of the stamper 21 are well transferred to the information surface of the disk substrate. By the way, when the compression core 24 is located at the rear stop position and the compression piston 37 is located at the retreat limit position, the rear end surface S1 of the small diameter portion 35
0 and the front end face S7 of the compression piston 37 are brought into contact with each other.

【0022】したがって、前記圧縮コア24を前進させ
て樹脂を圧縮するときに、圧縮ピストン37が前進を開
始するタイミングと、実際に圧縮コア24が前進を開始
するタイミングとの間に時間のずれが生じることがなく
なる。その結果、成形条件の設定を簡素化することがで
き、高密度のディスクを高精度で得ることができる。な
お、本発明は前記実施の形態に限定されるものではな
く、本発明の趣旨に基づいて種々変形させることが可能
であり、それらを本発明の範囲から排除するものではな
い。
Therefore, when the compression core 24 is advanced to compress the resin, there is a time lag between the timing at which the compression piston 37 starts to advance and the timing at which the compression core 24 actually starts to advance. Will not occur. As a result, setting of molding conditions can be simplified, and a high-density disk can be obtained with high accuracy. It should be noted that the present invention is not limited to the above-described embodiment, but can be variously modified based on the gist of the present invention, and they are not excluded from the scope of the present invention.

【0023】[0023]

【発明の効果】以上詳細に説明したように、本発明によ
れば、ディスク成形用金型においては、スタンパが取り
付けられた固定側ガイドリングと、該固定側ガイドリン
グと対向させて配設された可動側ガイドリングと、該可
動側ガイドリングの内周側に進退自在に配設された圧縮
コアと、駆動手段によって前進させられ、前記圧縮コア
を前進させる圧縮ピストンとを有する。
As described above in detail, according to the present invention, in the disk molding die, the fixed guide ring to which the stamper is attached and the fixed guide ring are disposed so as to face the fixed guide ring. A movable guide ring, a compression core disposed on the inner peripheral side of the movable guide ring so as to be able to advance and retreat, and a compression piston which is advanced by driving means and advances the compression core.

【0024】そして、前記圧縮コアが後方停止位置に置
かれ、圧縮ピストンが後退限位置に置かれたときに、圧
縮コアと圧縮ピストンとは当接させられる。この場合、
前記圧縮コアが後方停止位置に置かれ、圧縮ピストンが
後退限位置に置かれたときに、圧縮コアと圧縮ピストン
とは当接させられるので、圧縮コアを前進させて樹脂を
圧縮しようとするときに、圧縮ピストンが前進を開始す
るタイミングと、実際に圧縮コアが前進を開始するタイ
ミングとの間に時間のずれが生じることがなくなる。そ
の結果、成形条件の設定を簡素化することができ、高密
度のディスクを高精度で得ることができる。
Then, when the compression core is located at the rear stop position and the compression piston is located at the retreat limit position, the compression core and the compression piston are brought into contact with each other. in this case,
When the compression core is placed at the rear stop position and the compression piston is placed at the retreat limit position, the compression core and the compression piston are brought into contact with each other, so that the compression core is advanced to compress the resin. In addition, there is no time lag between the timing when the compression piston starts moving forward and the timing when the compression core actually starts moving forward. As a result, setting of molding conditions can be simplified, and a high-density disk can be obtained with high accuracy.

【図面の簡単な説明】[Brief description of the drawings]

【図1】本発明の実施の形態における圧縮コアの後退状
態を示す図である。
FIG. 1 is a diagram illustrating a retracted state of a compression core according to an embodiment of the present invention.

【図2】従来のディスク成形用金型における圧縮コアの
後退状態を示す図である。
FIG. 2 is a view showing a retracted state of a compressed core in a conventional disk molding die.

【図3】従来のディスク成形用金型における圧縮コアの
前進状態を示す図である。
FIG. 3 is a view showing a state in which a compression core is advanced in a conventional disk molding die.

【図4】本発明の実施の形態における圧縮コアの前進状
態を示す図である。
FIG. 4 is a view showing a forward state of a compression core according to the embodiment of the present invention.

【符号の説明】[Explanation of symbols]

18 固定側ガイドリング 21 スタンパ 23 可動側ガイドリング 24 圧縮コア 37 圧縮ピストン 18 Fixed side guide ring 21 Stamper 23 Movable side guide ring 24 Compression core 37 Compression piston

Claims (1)

【特許請求の範囲】[Claims] 【請求項1】 (a)スタンパが取り付けられた固定側
ガイドリングと、(b)該固定側ガイドリングと対向さ
せて配設された可動側ガイドリングと、(c)該可動側
ガイドリングの内周側に進退自在に配設された圧縮コア
と、(d)駆動手段によって前進させられ、前記圧縮コ
アを前進させる圧縮ピストンとを有するとともに、
(e)前記圧縮コアが後方停止位置に置かれ、圧縮ピス
トンが後退限位置に置かれたときに、圧縮コアと圧縮ピ
ストンとは当接させられることを特徴とするディスク成
形用金型。
1. A fixed-side guide ring to which a stamper is attached, (b) a movable-side guide ring disposed opposite to the fixed-side guide ring, and (c) a movable-side guide ring. A compression core disposed movably on the inner peripheral side and (d) a compression piston which is advanced by a driving means and advances the compression core;
(E) The compression core and the compression piston are brought into contact with each other when the compression core is located at the rear stop position and the compression piston is located at the retreat limit position.
JP23386997A 1997-08-29 1997-08-29 Disk molding die Expired - Fee Related JP3414995B2 (en)