JPS5475585A - Aluminium terminal - Google Patents
Aluminium terminalInfo
- Publication number
- JPS5475585A JPS5475585A JP14368177A JP14368177A JPS5475585A JP S5475585 A JPS5475585 A JP S5475585A JP 14368177 A JP14368177 A JP 14368177A JP 14368177 A JP14368177 A JP 14368177A JP S5475585 A JPS5475585 A JP S5475585A
- Authority
- JP
- Japan
- Prior art keywords
- layer
- aluminium
- copper
- battlebore
- nickel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE: To reduce the corrosion of aluminium even under a corrosive condition by the procedure in which a nickel layer is provided on the junction of connection portion by an electric plating method and then a copper layer or a silver layer is provided at a place inward more than 4 mm from the outer edge of the nickel layer.
CONSTITUTION: When aluminium twisted wire is fastened with clamp to the wire insertion hole 3 formed in the cylindrical portion 4 of an aluminium terminal of a battlebore shape, and also the copper terminal of an apparatus is fastened with bolt to the battlebore-shaped portion 2, a nickel layer is electrically plated onto the junction of the battlebore-shaped portion 2, and then a copper layer or a silver layer is plated only on a nickel surface portion more than 4 mm from the outer edge of the nickel layer. Since, thus, the copper layer is isolated from the aluminium on the outside surface exposed to corrosive environment, the electrolytic corrosion between copper and aluminium can be suppressed, thus greatly reducing the corrosion at plated border portion.
COPYRIGHT: (C)1979,JPO&Japio
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP14368177A JPS583349B2 (en) | 1977-11-29 | 1977-11-29 | aluminum terminal |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP14368177A JPS583349B2 (en) | 1977-11-29 | 1977-11-29 | aluminum terminal |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5475585A true JPS5475585A (en) | 1979-06-16 |
| JPS583349B2 JPS583349B2 (en) | 1983-01-20 |
Family
ID=15344461
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP14368177A Expired JPS583349B2 (en) | 1977-11-29 | 1977-11-29 | aluminum terminal |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS583349B2 (en) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0216572U (en) * | 1989-07-12 | 1990-02-02 | ||
| CN102513637A (en) * | 2011-11-25 | 2012-06-27 | 广东电网公司电力科学研究院 | Copper-aluminum (Cu-Al) braze welding process of copper-aluminum transition wire clamp |
| WO2024056069A1 (en) * | 2022-09-16 | 2024-03-21 | 长春捷翼汽车科技股份有限公司 | Novel aluminum terminal |
-
1977
- 1977-11-29 JP JP14368177A patent/JPS583349B2/en not_active Expired
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0216572U (en) * | 1989-07-12 | 1990-02-02 | ||
| CN102513637A (en) * | 2011-11-25 | 2012-06-27 | 广东电网公司电力科学研究院 | Copper-aluminum (Cu-Al) braze welding process of copper-aluminum transition wire clamp |
| WO2024056069A1 (en) * | 2022-09-16 | 2024-03-21 | 长春捷翼汽车科技股份有限公司 | Novel aluminum terminal |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS583349B2 (en) | 1983-01-20 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US5227041A (en) | Dry contact electroplating apparatus | |
| WO1989002212A3 (en) | Improved circuit board material and electroplating bath for the production thereof | |
| IT8248633A0 (en) | BATH AND PROCEDURE FOR ELECTROPLATING A ZINC ALLOY ON A CONDUCTIVE SUBSTRATE | |
| KR830002066A (en) | How to remove copper ions from baths containing copper ions | |
| JPS5739189A (en) | Stainless steel plated with noble metal | |
| JPS53122790A (en) | Aluminum terminal and preparation | |
| JPS6486527A (en) | Ccb tape carrier | |
| AU2305483A (en) | Cyanide-free copper plating process and alloy anode | |
| ES511416A0 (en) | A METHOD OF ELECTROLYTICALLY COATING AN ELECTRICALLY CONDUCTIVE SURFACE SERVING CATHODE IN AN ELECTRICAL CIRCUIT. | |
| JPS53125222A (en) | High tensile electroconductive copper alloy | |
| JPS56119792A (en) | Electroplating method | |
| JPS5538970A (en) | Inside surface plating method of metal pipe | |
| JPS5730353A (en) | Semiconductor device | |
| JPS6486417A (en) | Contact and manufacture thereof | |
| EP0063925A1 (en) | Electro-plating process and products therefrom | |
| JPS5623297A (en) | Partial plating method | |
| KR890003937Y1 (en) | Ground rod | |
| JPS57207195A (en) | Thick plating method for copper on aluminum racket terminal | |
| JPS6358397B2 (en) | ||
| JPS57120664A (en) | Formation of nickel film | |
| JPS56142886A (en) | Tin plating method for aluminum alloy | |
| GB1461474A (en) | Electrical connectors and a method of preparing stable electro platings | |
| JPS531603A (en) | Pretreatment of cathode to be used at deposition of metal by electrolysis from solution containing metal salt | |
| JPS5399479A (en) | Copper foil fiber wire | |
| GB1394062A (en) | Semi-conductor devices |