JPS5530367A - Vertical welding - Google Patents
Vertical weldingInfo
- Publication number
- JPS5530367A JPS5530367A JP10379578A JP10379578A JPS5530367A JP S5530367 A JPS5530367 A JP S5530367A JP 10379578 A JP10379578 A JP 10379578A JP 10379578 A JP10379578 A JP 10379578A JP S5530367 A JPS5530367 A JP S5530367A
- Authority
- JP
- Japan
- Prior art keywords
- preheating
- molten metal
- controlled
- welding
- strap
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE:To make possible controlling of penetration shapes without preheating and achieve higher quality of weld zone by providing preheating effect through utilization of part of molten metal and discharging the other molten metal to the outside in vertical welding of the material requiring preheating. CONSTITUTION:A welding wire 4 and shielding gas are supplied from a torch 3. When welding is started, the portion where molten metal pools in the groove 2b of a strap 2 and becomes deeper than the depth h is discharged from 2a. As the strap 2 is moved upward, welding progresses. The molten metal pooled in the groove 2b of the strap 2 acts as a preheating heat source for base metal 1. The amount of the metal being discharged is controlled by controlling the rate of movement and the molten metal 5 of the groove 2b is controlled of the rate of heating by arc heat, whereby preheating effect may be controlled. Further, the direct influencing power of the arc upon the base metal 1 may be controlled, thus even the materials of high heat conductivity such as steel and copper may be welded without preheating by another heating heat source.
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP10379578A JPS6021028B2 (en) | 1978-08-28 | 1978-08-28 | Vertical welding method |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP10379578A JPS6021028B2 (en) | 1978-08-28 | 1978-08-28 | Vertical welding method |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5530367A true JPS5530367A (en) | 1980-03-04 |
| JPS6021028B2 JPS6021028B2 (en) | 1985-05-24 |
Family
ID=14363325
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP10379578A Expired JPS6021028B2 (en) | 1978-08-28 | 1978-08-28 | Vertical welding method |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6021028B2 (en) |
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5722882A (en) * | 1980-07-15 | 1982-02-05 | Toshiba Corp | Welding method |
| JPS5750282A (en) * | 1980-09-08 | 1982-03-24 | Toshiba Corp | Flat mig welding method |
| US5438492A (en) * | 1993-03-26 | 1995-08-01 | Alliedsignal Inc. | End release seat belt buckle |
| JP2024006631A (en) * | 2022-07-04 | 2024-01-17 | 株式会社神戸製鋼所 | Sliding copper pad for welding and welding method |
-
1978
- 1978-08-28 JP JP10379578A patent/JPS6021028B2/en not_active Expired
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5722882A (en) * | 1980-07-15 | 1982-02-05 | Toshiba Corp | Welding method |
| JPS5750282A (en) * | 1980-09-08 | 1982-03-24 | Toshiba Corp | Flat mig welding method |
| US5438492A (en) * | 1993-03-26 | 1995-08-01 | Alliedsignal Inc. | End release seat belt buckle |
| JP2024006631A (en) * | 2022-07-04 | 2024-01-17 | 株式会社神戸製鋼所 | Sliding copper pad for welding and welding method |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6021028B2 (en) | 1985-05-24 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS5530367A (en) | Vertical welding | |
| JPS5527418A (en) | Welding or cutting method | |
| JPS6213410B2 (en) | ||
| JPS551919A (en) | Tig overlay welding method | |
| ZA807723B (en) | Process for improvement in heat utilization during steel production from solid iron materials | |
| JPS55106679A (en) | Arc welding method | |
| JPS5653889A (en) | Electroslag welding method and consumable nozzle | |
| JPS55103292A (en) | Laser cutting method | |
| JPS56144865A (en) | Surface hardening build-up welding method | |
| JPS55126381A (en) | Method and device for vertical arc spot welding | |
| JPS57158319A (en) | Partial surface hardening method using pulse tig welding machine | |
| JPS5779088A (en) | Electroslag welding method using consumable electrode | |
| JPS55130371A (en) | Welding method of stainless steel material and copper material | |
| JPS56119673A (en) | Nonconsumable electrode arc welding method | |
| Erokhin | Peculiarities of the Behavior of Oxygen During Heating of Cu--Ni Alloys in an Electric-Arc Furnace | |
| JPS57137461A (en) | Surface hardening method for stainless steel | |
| SU125324A1 (en) | Electroslag welding method | |
| JPS5428243A (en) | Welder for fine grain and high toughness | |
| JPS57152377A (en) | Controlling method for welding arc | |
| JPS5465107A (en) | Hardening method by means of plasma arc | |
| JPS56109176A (en) | Arc welding method of metal | |
| JPS5575882A (en) | Gta welding method | |
| JPS5668590A (en) | Tig welding method | |
| Loureiro | Welding by'Electroscorification' | |
| Nitkiewicz et al. | Surface Hardening of a Plate Made From 55 Grade Steel.(Retroactive Coverage) |