JPS5536003A - Friction welding method - Google Patents
Friction welding methodInfo
- Publication number
- JPS5536003A JPS5536003A JP10760778A JP10760778A JPS5536003A JP S5536003 A JPS5536003 A JP S5536003A JP 10760778 A JP10760778 A JP 10760778A JP 10760778 A JP10760778 A JP 10760778A JP S5536003 A JPS5536003 A JP S5536003A
- Authority
- JP
- Japan
- Prior art keywords
- pressure
- welding
- revolution
- base metal
- high pressure
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE: To prevent break from its generation in a welding part by changing pressing force of a base metal in two stages from low pressure to high pressure, and stopping revolution of the base metal after it has been reached to high pressure when at least one of two base metals is a superalloy.
CONSTITUTION: When friction welding is carried out using for at least one of two base metals, and alloy of creep breaking strength for 700°C, 103 hrs that is not less than 20kg/mm2, or desirably, a Ni group alloy contained MC type carbide, operation is implemented as below mentioned. The above mentioned base metals were relatively revolved in N revolutions, then, are kept for T1 hr while they are pressed with the primary pressure(low pressure) P1, after that the pressure is increased to the secondary pressure(high pressure) P2 to hold them for T3 hr, there, the revolution is stopped, after revolution stop, the secondary pressure conditions P2 is maintained for a little while, and then, the pressure is released. Further, by this method, even when the welding plane of any one of the base metal inclines in a slope of 0.3W1.2° angle, welding is available.
COPYRIGHT: (C)1980,JPO&Japio
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP53107607A JPS5819393B2 (en) | 1978-09-04 | 1978-09-04 | Friction welding method |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP53107607A JPS5819393B2 (en) | 1978-09-04 | 1978-09-04 | Friction welding method |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5536003A true JPS5536003A (en) | 1980-03-13 |
| JPS5819393B2 JPS5819393B2 (en) | 1983-04-18 |
Family
ID=14463451
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP53107607A Expired JPS5819393B2 (en) | 1978-09-04 | 1978-09-04 | Friction welding method |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5819393B2 (en) |
Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5211294A (en) * | 1975-07-17 | 1977-01-28 | Teijin Ltd | Preparation of polyester elastomer |
-
1978
- 1978-09-04 JP JP53107607A patent/JPS5819393B2/en not_active Expired
Patent Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5211294A (en) * | 1975-07-17 | 1977-01-28 | Teijin Ltd | Preparation of polyester elastomer |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5819393B2 (en) | 1983-04-18 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS5536003A (en) | Friction welding method | |
| JPS526791A (en) | Process for preparing new phenolic copolymers | |
| JPS51119604A (en) | A method and apparatus for melting low melting point metals using wast e tires as fuel | |
| JPS5217308A (en) | Method for separating cermet alloy and hard metal | |
| JPS528907A (en) | Furnace for quick and continuous melting of low melting point metals | |
| JPS5587879A (en) | Accelerating method for pump | |
| JPS53146958A (en) | Rolling method of steel material at high area reduction | |
| JPS51122055A (en) | A process for isolating 7- dehydtocholesterol | |
| JPS5217314A (en) | Structural steel for heavy heat input welding | |
| JPS51143514A (en) | Process for producing manganese addition agent for iron and steel | |
| GB1387947A (en) | Method of manufacturing reaction mixtures | |
| JPS542940A (en) | Removing method for tin of tinned copper material | |
| JPS52712A (en) | Apparatus for adding low melting point metal to molten metal | |
| JPS51124767A (en) | A tapping screw and the preparation method | |
| SU1219661A1 (en) | Method of converting copper nickel-containing white matte | |
| JPS5224906A (en) | Continuous dissolving apparatus for metals | |
| JPS51151615A (en) | Method and apparatus for recovering metal in steel slag by crushing se paration | |
| JPS5270904A (en) | Method and apparatus for reventing intermingling of molten slag | |
| JPS528001A (en) | Solid fuels | |
| JPS5224103A (en) | Electrolytic cell for exfraction and separation of non-metallic impuri ties from metal | |
| JPS5245521A (en) | Low alloy high tension steel | |
| JPS5224158A (en) | Gas producer | |
| JPS5262105A (en) | Method for dismantling lining refractory material of metal mixer truck | |
| LeGall | The Metal Pack Holds Its Own | |
| JPS5268812A (en) | Addition of extremely reactive metals or alloys to molten steel |