JPS563645A - Titanium alloy having superior vibration-damping capacity and its manufacture - Google Patents
Titanium alloy having superior vibration-damping capacity and its manufactureInfo
- Publication number
- JPS563645A JPS563645A JP7750179A JP7750179A JPS563645A JP S563645 A JPS563645 A JP S563645A JP 7750179 A JP7750179 A JP 7750179A JP 7750179 A JP7750179 A JP 7750179A JP S563645 A JPS563645 A JP S563645A
- Authority
- JP
- Japan
- Prior art keywords
- alloy
- temp
- manufacture
- vibration
- superior vibration
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE: To manufacture a Ti alloy having superior vibration-damping characteristics and effectively usable as a vibration-damping material for equipment by heating a Ti alloy contg. Al and Mo each of a predetermined percentage to a specified temp. below the β-transformation point after which it is held at the temp. and quenched at a cooling rate capable of inducing martensite transformation.
CONSTITUTION: A Ti alloy consisting of 1.0W6.0wt% Al, 1W11wt% Mo, and the balance Ti and accompanying impurities is heat treated as follows: it is heated to below a temp. 70°C below the β-transformation point, held at the temp., and quenched by water cooling or other method at a cooling rate capable of inducing martensite transformation. As a result, the metal structure is converted into martensite structure, and a Ti alloy having superior vibration-damping characteristics is obtd. By substituting Cr for 1W8.5wt% of the Ti in the starting material alloy, a Ti alloy having improved mechanical strength, workability, etc. is obtd.
COPYRIGHT: (C)1981,JPO&Japio
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP7750179A JPS563645A (en) | 1979-06-21 | 1979-06-21 | Titanium alloy having superior vibration-damping capacity and its manufacture |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP7750179A JPS563645A (en) | 1979-06-21 | 1979-06-21 | Titanium alloy having superior vibration-damping capacity and its manufacture |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| JPS563645A true JPS563645A (en) | 1981-01-14 |
Family
ID=13635707
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP7750179A Pending JPS563645A (en) | 1979-06-21 | 1979-06-21 | Titanium alloy having superior vibration-damping capacity and its manufacture |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS563645A (en) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4527146A (en) * | 1982-12-24 | 1985-07-02 | Tokyo Shibaura Denki Kabushiki Kaisha | Varistor |
| CN116144979A (en) * | 2022-12-28 | 2023-05-23 | 有研(广东)新材料技术研究院 | A medium-strength corrosion-resistant titanium alloy for coiled tubing and its preparation method |
-
1979
- 1979-06-21 JP JP7750179A patent/JPS563645A/en active Pending
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4527146A (en) * | 1982-12-24 | 1985-07-02 | Tokyo Shibaura Denki Kabushiki Kaisha | Varistor |
| CN116144979A (en) * | 2022-12-28 | 2023-05-23 | 有研(广东)新材料技术研究院 | A medium-strength corrosion-resistant titanium alloy for coiled tubing and its preparation method |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| SE8003567L (en) | PROCEDURAL KIT FOR MANUFACTURING STAINLESS, FERRITAUSTENITIC STEEL | |
| JPS5597425A (en) | Preparation of high-tensile steel with low yield ratio, low carbon and low alloy | |
| JPS56116858A (en) | Steam turbine rotor | |
| JPS56163248A (en) | Manufacture of drawn material of beryllium-copper alloy | |
| CN109594019A (en) | A kind of 9Cr martensite heat resisting cast steel and eliminate the ferritic method of δ-in the cast steel | |
| JPS57120616A (en) | Production of parts for mechanical structure | |
| JPS5623223A (en) | Production of high-young's modulus steel material | |
| JPS56169723A (en) | Treatment of reheating-omit type hot forging bar steel | |
| JPS5754252A (en) | Soft magnetic material containing chromium | |
| JPS5754249A (en) | Semihard magnet alloy and manufacture thereof | |
| JPS5538957A (en) | Austenitic stainless cast steel | |
| JPS5582739A (en) | Alloy for hearth member with improved thermal impact resistance and high temperature compressive strength | |
| JPS5635717A (en) | Production of hot-rolled steel material of superior vibration attenuating characteristic | |
| JPS5442325A (en) | Austenite stainless steel having good weldability and resistance to stress corrosion cracking in high temperature pure water | |
| JPS57123947A (en) | Magnetic alloy for magnetic recording and reproducing head and its manufacture | |
| JPS5443814A (en) | Heat treatment method for damping alloy | |
| JPS5620121A (en) | Manufacture of chromium-molybdenum steel for pressure vessel | |
| JPS552749A (en) | Manufacture of hot formed product of high toughness low alloy steel containing mo | |
| JPS5472712A (en) | Wear resistant cast steel for low temperature use | |
| JPS57164919A (en) | Production of low-carbon aluminum killed steel of high nitrate stress corrosion cracking resistance | |
| JPS55122863A (en) | Heat treating method for cr-containing ni alloy | |
| JPS57116753A (en) | High carbon steel wire rod with high toughness | |
| JPS57108220A (en) | Production of high tensile steel for welded construction | |
| JPS5684447A (en) | Parts for geothermal steam turbine | |
| JPS5579828A (en) | High tensile steel of 60kg/mm2 degree after refining having excellent cod value and manufacture thereof |