JPS58167447A - 腐食ガラス表面を有するセラミツクスの製造方法 - Google Patents
腐食ガラス表面を有するセラミツクスの製造方法Info
- Publication number
- JPS58167447A JPS58167447A JP4983182A JP4983182A JPS58167447A JP S58167447 A JPS58167447 A JP S58167447A JP 4983182 A JP4983182 A JP 4983182A JP 4983182 A JP4983182 A JP 4983182A JP S58167447 A JPS58167447 A JP S58167447A
- Authority
- JP
- Japan
- Prior art keywords
- metal
- ceramic
- fluoride
- filler
- glassy
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Surface Treatment Of Glass (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP4983182A JPS58167447A (ja) | 1982-03-26 | 1982-03-26 | 腐食ガラス表面を有するセラミツクスの製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP4983182A JPS58167447A (ja) | 1982-03-26 | 1982-03-26 | 腐食ガラス表面を有するセラミツクスの製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS58167447A true JPS58167447A (ja) | 1983-10-03 |
| JPH0323491B2 JPH0323491B2 (2) | 1991-03-29 |
Family
ID=12842022
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP4983182A Granted JPS58167447A (ja) | 1982-03-26 | 1982-03-26 | 腐食ガラス表面を有するセラミツクスの製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS58167447A (2) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4647477A (en) * | 1984-12-07 | 1987-03-03 | Kollmorgen Technologies Corporation | Surface preparation of ceramic substrates for metallization |
| US4885053A (en) * | 1985-07-04 | 1989-12-05 | Licentia Patent-Verwaltungs-Gmbh | Process for metal-plating an electrically poorly conducting substrate made of an inorganic material |
-
1982
- 1982-03-26 JP JP4983182A patent/JPS58167447A/ja active Granted
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4647477A (en) * | 1984-12-07 | 1987-03-03 | Kollmorgen Technologies Corporation | Surface preparation of ceramic substrates for metallization |
| US4885053A (en) * | 1985-07-04 | 1989-12-05 | Licentia Patent-Verwaltungs-Gmbh | Process for metal-plating an electrically poorly conducting substrate made of an inorganic material |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0323491B2 (2) | 1991-03-29 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4218230A (en) | Method of glass strengthening by ion exchange | |
| US4619716A (en) | Method of brazing an aluminum material | |
| DE3933976C2 (de) | Verfahren zum Bilden eines keramischen Überzugs auf einem Substrat | |
| JPH0153360B2 (2) | ||
| US4273832A (en) | Glass article strengthened by ion exchange substitution | |
| JPH07225299A (ja) | 硫酸ナトリウム含有放射性廃液の固化処理方法 | |
| JPH0323491B2 (2) | ||
| US3345194A (en) | Organic ammonium silicate coating compositions | |
| JPH0765004B2 (ja) | 耐熱耐食性塗料 | |
| JPS5590561A (en) | Manufacture of stable metal powder pigment composition | |
| JPS58130546A (ja) | 炭化珪素質基板およびその製造方法 | |
| JPS58151476A (ja) | ほうろう製品の製法 | |
| US519968A (en) | quinby | |
| JPS63745Y2 (2) | ||
| JPS58167446A (ja) | 凹凸表面セラミツクの製造方法 | |
| JPS62202005A (ja) | 多孔質金属板 | |
| JPS605525B2 (ja) | 熔剤用シリコン粉粒体の酸化皮膜形成法 | |
| JPS62290765A (ja) | 無機系塗料 | |
| Juan et al. | Inorganic fluoride materials from Solvay Fluor and their industrial applications | |
| CA1170834A (en) | Method of glass strengthening by ion exchange | |
| JP2659616B2 (ja) | 金属表面への有機樹脂層形成用下地処理剤 | |
| JP2802433B2 (ja) | レーザ照射によるセラミックス被膜の形成方法 | |
| JPS55135173A (en) | Manufacture of stable metal powder pigment composition | |
| JPH0247552B2 (ja) | Hooroobutsupinoyobisonoseizohoho | |
| JPS60195080A (ja) | セラミツク体の表面粗化法 |