JPS6071581A - 耐熱耐摺動損傷無機系構造材料 - Google Patents
耐熱耐摺動損傷無機系構造材料Info
- Publication number
- JPS6071581A JPS6071581A JP58179188A JP17918883A JPS6071581A JP S6071581 A JPS6071581 A JP S6071581A JP 58179188 A JP58179188 A JP 58179188A JP 17918883 A JP17918883 A JP 17918883A JP S6071581 A JPS6071581 A JP S6071581A
- Authority
- JP
- Japan
- Prior art keywords
- resistant
- sliding
- materials
- heat
- damage
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Valve-Gear Or Valve Arrangements (AREA)
- Cylinder Crankcases Of Internal Combustion Engines (AREA)
- Coating By Spraying Or Casting (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP58179188A JPS6071581A (ja) | 1983-09-29 | 1983-09-29 | 耐熱耐摺動損傷無機系構造材料 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP58179188A JPS6071581A (ja) | 1983-09-29 | 1983-09-29 | 耐熱耐摺動損傷無機系構造材料 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6071581A true JPS6071581A (ja) | 1985-04-23 |
| JPH059394B2 JPH059394B2 (fr) | 1993-02-04 |
Family
ID=16061473
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP58179188A Granted JPS6071581A (ja) | 1983-09-29 | 1983-09-29 | 耐熱耐摺動損傷無機系構造材料 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6071581A (fr) |
Cited By (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6257905A (ja) * | 1985-08-02 | 1987-03-13 | Asahi Chem Ind Co Ltd | 紡糸口金 |
| JPS6321748U (fr) * | 1986-07-25 | 1988-02-13 | ||
| FR2660930A1 (fr) * | 1990-04-13 | 1991-10-18 | Ceramiques Composites | Lubrifiant pour surface en ceramique et procede de lubrification. |
| JPH03260047A (ja) * | 1990-03-09 | 1991-11-20 | Agency Of Ind Science & Technol | 高温耐摩耗溶射材料及びその製造方法 |
| JPH05340212A (ja) * | 1992-06-05 | 1993-12-21 | Sumitomo Electric Ind Ltd | セラミックス製アジャスティングシム |
| EP0816698A1 (fr) * | 1996-03-07 | 1998-01-07 | SKF Nova AB | Dispositifs à contact de roulement lubrifiés, méthode pour les lubrifier et composition adaptée à une telle lubrification |
Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS58204883A (ja) * | 1982-05-20 | 1983-11-29 | 九州耐火煉瓦株式会社 | セラミツクスで構成された摺動部を有する機械部品 |
| JPS59137375A (ja) * | 1983-01-25 | 1984-08-07 | トヨタ自動車株式会社 | 摺動特性にすぐれた窒化珪素質焼結体 |
-
1983
- 1983-09-29 JP JP58179188A patent/JPS6071581A/ja active Granted
Patent Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS58204883A (ja) * | 1982-05-20 | 1983-11-29 | 九州耐火煉瓦株式会社 | セラミツクスで構成された摺動部を有する機械部品 |
| JPS59137375A (ja) * | 1983-01-25 | 1984-08-07 | トヨタ自動車株式会社 | 摺動特性にすぐれた窒化珪素質焼結体 |
Cited By (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6257905A (ja) * | 1985-08-02 | 1987-03-13 | Asahi Chem Ind Co Ltd | 紡糸口金 |
| JPS6321748U (fr) * | 1986-07-25 | 1988-02-13 | ||
| JPH03260047A (ja) * | 1990-03-09 | 1991-11-20 | Agency Of Ind Science & Technol | 高温耐摩耗溶射材料及びその製造方法 |
| FR2660930A1 (fr) * | 1990-04-13 | 1991-10-18 | Ceramiques Composites | Lubrifiant pour surface en ceramique et procede de lubrification. |
| JPH05340212A (ja) * | 1992-06-05 | 1993-12-21 | Sumitomo Electric Ind Ltd | セラミックス製アジャスティングシム |
| EP0816698A1 (fr) * | 1996-03-07 | 1998-01-07 | SKF Nova AB | Dispositifs à contact de roulement lubrifiés, méthode pour les lubrifier et composition adaptée à une telle lubrification |
| CN1082152C (zh) * | 1996-03-07 | 2002-04-03 | 斯克弗·诺瓦公司 | 润滑状态下的滚动接触装置及其润滑方法和润滑混合物 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH059394B2 (fr) | 1993-02-04 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4719074A (en) | Metal-ceramic composite article and a method of producing the same | |
| EP0139406B1 (fr) | Article composite de métal et de céramique et méthode pour sa fabrication | |
| Katz et al. | Ceramics for high performance rolling element bearings: a review and assessment | |
| US4798493A (en) | Ceramic-metal composite body | |
| JPS6071581A (ja) | 耐熱耐摺動損傷無機系構造材料 | |
| US5066547A (en) | Metal and ceramic heat-connected body | |
| Dufrane | Wear perfomance of ceramics in ring/cylinder applications | |
| Gomes et al. | Tribooxidational effects on friction and wear behavior of silicon nitride/tool steel and silicon nitride/gray cast iron contacts | |
| Sliney et al. | Tribology of selected ceramics at temperatures to 900 C | |
| Pasaribu | Friction and wear of zirconia and alumina ceramics doped with CuO | |
| EP0110488B1 (fr) | Elément de moteur | |
| EP0156484B1 (fr) | Produit composite métal-céramique et son procédé de fabrication | |
| JPH04147957A (ja) | 断熱アルミニウム系部材 | |
| Evtushok et al. | Tribological properties of composite materials based on refractory titanium compounds | |
| JPS61250161A (ja) | シリンダライナ | |
| Dufrane et al. | Performance of ceramics in ring/cylinder applications | |
| Dufrane | Wear performance of ceramics in ring/cylinder applications | |
| JPH0285519A (ja) | 摺動構造 | |
| Katz et al. | Ceramics for high performance rolling element bearings: A review and assessment | |
| Duszczyk et al. | Friction and wear of P/M Al-20Si-Al2O3 composites in kerosene | |
| Dwivedi | Friction and wear properties of a ceramic matrix composite produced by directed metal oxidation | |
| Prakash | Friction and wear characteristics of advanced ceramic composite materials | |
| Worthen et al. | Ceramic engine components | |
| Evtushok et al. | Composite materials based on titanium nitride for high-speed friction units | |
| Davis et al. | Oxidation‐induced crack healing and erosion life assessment of Ni–Mo–Al–Cr7C3–Al2O3 composite coating |