JPS6127067A - 鉛蓄電池 - Google Patents
鉛蓄電池Info
- Publication number
- JPS6127067A JPS6127067A JP59148288A JP14828884A JPS6127067A JP S6127067 A JPS6127067 A JP S6127067A JP 59148288 A JP59148288 A JP 59148288A JP 14828884 A JP14828884 A JP 14828884A JP S6127067 A JPS6127067 A JP S6127067A
- Authority
- JP
- Japan
- Prior art keywords
- lead
- acid
- acid resistant
- heating
- thermosetting
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/64—Carriers or collectors
- H01M4/66—Selection of materials
- H01M4/68—Selection of materials for use in lead-acid accumulators
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Cell Electrode Carriers And Collectors (AREA)
- Connection Of Batteries Or Terminals (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP59148288A JPS6127067A (ja) | 1984-07-16 | 1984-07-16 | 鉛蓄電池 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP59148288A JPS6127067A (ja) | 1984-07-16 | 1984-07-16 | 鉛蓄電池 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6127067A true JPS6127067A (ja) | 1986-02-06 |
| JPH0363178B2 JPH0363178B2 (2) | 1991-09-30 |
Family
ID=15449415
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP59148288A Granted JPS6127067A (ja) | 1984-07-16 | 1984-07-16 | 鉛蓄電池 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6127067A (2) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO2022196566A1 (ja) | 2021-03-16 | 2022-09-22 | 株式会社Gsユアサ | 鉛蓄電池 |
Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS52151331U (2) * | 1976-05-13 | 1977-11-16 | ||
| JPS57143266A (en) * | 1981-02-27 | 1982-09-04 | Shin Kobe Electric Mach Co Ltd | Plate for lead acid battery |
-
1984
- 1984-07-16 JP JP59148288A patent/JPS6127067A/ja active Granted
Patent Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS52151331U (2) * | 1976-05-13 | 1977-11-16 | ||
| JPS57143266A (en) * | 1981-02-27 | 1982-09-04 | Shin Kobe Electric Mach Co Ltd | Plate for lead acid battery |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO2022196566A1 (ja) | 2021-03-16 | 2022-09-22 | 株式会社Gsユアサ | 鉛蓄電池 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0363178B2 (2) | 1991-09-30 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN101510609B (zh) | 蓄电池正板栅的合金材料及其制备方法 | |
| CN107881356B (zh) | 一种铅酸蓄电池用正极板栅合金及其制备方法 | |
| JPS6020455B2 (ja) | 鉛−酸蓄電池用の鉛合金 | |
| JPS6127067A (ja) | 鉛蓄電池 | |
| ATE72612T1 (de) | Vorrichtung zum verbinden von polbruecken und polen mit den fahnenableitern eines plattensatzes fuer eine akkumulatorenzelle. | |
| CN108172839A (zh) | 铅酸蓄电池正极板栅高锡合金及其制备方法 | |
| CN107841653A (zh) | 一种阀控铅酸蓄电池用正极板栅合金及其制备方法 | |
| Feliu et al. | The effect of ageing on the anodic corrosion of Pb-Sb alloys | |
| JP2001185206A (ja) | 鉛蓄電池及びその製造方法 | |
| JPS6127069A (ja) | 鉛蓄電池 | |
| JP3397076B2 (ja) | 鉛蓄電池用正極板 | |
| JP3413930B2 (ja) | 鉛蓄電池極板群の製造法 | |
| JPS632253A (ja) | 鉛蓄電池及びその製造法 | |
| US2820079A (en) | Battery grid alloy | |
| JPH0213425B2 (2) | ||
| Cattaneo et al. | Continuous casting of lead-antimony alloys | |
| US10637044B2 (en) | Corrosion resistant positive grid for lead-acid batteries | |
| Mao et al. | Study of Lithium‐Lead Alloys as Grid Material for Lead‐Acid Batteries | |
| JPS6113565A (ja) | 鉛蓄電池 | |
| Caldwell et al. | Effect of Base Lead Composition on Metallurgical Properties of Maintenance‐Free Battery Alloys | |
| DE2412322A1 (de) | Akkumulatorengitter | |
| JPS6180756A (ja) | 鉛蓄電池用格子体の製造法 | |
| JP2008266739A (ja) | 鉛蓄電池用鉛合金及び鉛蓄電池 | |
| Skołuda et al. | The influence of different factors on the kinetics of potentiostatic forming of pasted positive lead electrodes | |
| JPH04358035A (ja) | 蓄電池用鉛基合金 |