JPS62260031A - 耐摩耗性高透磁率合金 - Google Patents
耐摩耗性高透磁率合金Info
- Publication number
- JPS62260031A JPS62260031A JP61103228A JP10322886A JPS62260031A JP S62260031 A JPS62260031 A JP S62260031A JP 61103228 A JP61103228 A JP 61103228A JP 10322886 A JP10322886 A JP 10322886A JP S62260031 A JPS62260031 A JP S62260031A
- Authority
- JP
- Japan
- Prior art keywords
- alloy
- wear
- magnetic
- fine particles
- lubricating solid
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Powder Metallurgy (AREA)
- Soft Magnetic Materials (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP61103228A JPS62260031A (ja) | 1986-05-07 | 1986-05-07 | 耐摩耗性高透磁率合金 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP61103228A JPS62260031A (ja) | 1986-05-07 | 1986-05-07 | 耐摩耗性高透磁率合金 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS62260031A true JPS62260031A (ja) | 1987-11-12 |
| JPH0447017B2 JPH0447017B2 (2) | 1992-07-31 |
Family
ID=14348613
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP61103228A Granted JPS62260031A (ja) | 1986-05-07 | 1986-05-07 | 耐摩耗性高透磁率合金 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS62260031A (2) |
Cited By (8)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO2011069318A1 (zh) * | 2009-12-10 | 2011-06-16 | 洛阳轴研科技股份有限公司 | 一种镍基轴承保持架材料及其制备方法 |
| CN103806847A (zh) * | 2014-03-04 | 2014-05-21 | 东营咸亨工贸有限公司 | 耐磨防腐抽油杆接箍 |
| CN104762500A (zh) * | 2014-12-17 | 2015-07-08 | 武汉理工大学 | 一种以MoO3板状晶体为润滑相和增强相的新型Ni3Al基自润滑材料及其制备方法 |
| CN105861879A (zh) * | 2016-03-31 | 2016-08-17 | 苏州睿昕汽车配件有限公司 | 汽车柴油机高强度活塞材料的制备方法 |
| CN107475655A (zh) * | 2016-06-03 | 2017-12-15 | 南京理工大学 | 一种活塞环表面镍铝基自润滑耐磨涂层及制备方法 |
| CN108273523A (zh) * | 2018-04-02 | 2018-07-13 | 张逸强 | 一种抗凝血药物中间体的生产方法 |
| CN109402481A (zh) * | 2018-12-11 | 2019-03-01 | 中国科学院兰州化学物理研究所 | 一种海水环境下镍硅基自润滑合金及其制备方法 |
| CN118919198A (zh) * | 2024-07-30 | 2024-11-08 | 天津三环奥纳科技有限公司 | 一种纳米晶磁芯材料及其制备方法 |
Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5061508A (2) * | 1973-10-01 | 1975-05-27 | ||
| JPS60138035A (ja) * | 1983-12-27 | 1985-07-22 | Res Inst Electric Magnetic Alloys | 磁気録音再生ヘツド用磁性合金およびその製造法 |
-
1986
- 1986-05-07 JP JP61103228A patent/JPS62260031A/ja active Granted
Patent Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5061508A (2) * | 1973-10-01 | 1975-05-27 | ||
| JPS60138035A (ja) * | 1983-12-27 | 1985-07-22 | Res Inst Electric Magnetic Alloys | 磁気録音再生ヘツド用磁性合金およびその製造法 |
Cited By (10)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO2011069318A1 (zh) * | 2009-12-10 | 2011-06-16 | 洛阳轴研科技股份有限公司 | 一种镍基轴承保持架材料及其制备方法 |
| CN103806847A (zh) * | 2014-03-04 | 2014-05-21 | 东营咸亨工贸有限公司 | 耐磨防腐抽油杆接箍 |
| CN104762500A (zh) * | 2014-12-17 | 2015-07-08 | 武汉理工大学 | 一种以MoO3板状晶体为润滑相和增强相的新型Ni3Al基自润滑材料及其制备方法 |
| CN105861879A (zh) * | 2016-03-31 | 2016-08-17 | 苏州睿昕汽车配件有限公司 | 汽车柴油机高强度活塞材料的制备方法 |
| CN107475655A (zh) * | 2016-06-03 | 2017-12-15 | 南京理工大学 | 一种活塞环表面镍铝基自润滑耐磨涂层及制备方法 |
| CN108273523A (zh) * | 2018-04-02 | 2018-07-13 | 张逸强 | 一种抗凝血药物中间体的生产方法 |
| CN108273523B (zh) * | 2018-04-02 | 2020-09-22 | 暨南大学附属第一医院 | 一种抗凝血药物中间体的生产方法 |
| CN109402481A (zh) * | 2018-12-11 | 2019-03-01 | 中国科学院兰州化学物理研究所 | 一种海水环境下镍硅基自润滑合金及其制备方法 |
| CN109402481B (zh) * | 2018-12-11 | 2021-03-26 | 中国科学院兰州化学物理研究所 | 一种海水环境下镍硅基自润滑合金及其制备方法 |
| CN118919198A (zh) * | 2024-07-30 | 2024-11-08 | 天津三环奥纳科技有限公司 | 一种纳米晶磁芯材料及其制备方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0447017B2 (2) | 1992-07-31 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP3816595B2 (ja) | スパッタリングターゲットの製造方法 | |
| US4572750A (en) | Magnetic alloy for magnetic recording-reproducing head | |
| Upadhyaya et al. | Sintering of submicron WC-10wt.% Co hard metals containing nickel and iron | |
| JPS62260031A (ja) | 耐摩耗性高透磁率合金 | |
| KR910009974B1 (ko) | 고포화 자속밀도 합금 | |
| TWI540220B (zh) | Target for magnetron sputtering and its manufacturing method | |
| JPH0790567A (ja) | 光磁気記録媒体用ターゲット材およびその製造方法 | |
| KR900007666B1 (ko) | 자기헤드용 비정질 합금 | |
| JPH06248445A (ja) | スパッタリングターゲットとそれを用いて形成した磁性薄膜および薄膜磁気ヘッド | |
| JP4218111B2 (ja) | Fe−Ni系合金粉末およびその製造方法 | |
| JPH03223444A (ja) | 高飽和磁束密度合金 | |
| JP2020202006A (ja) | 磁気記録媒体の軟磁性層用Co系合金 | |
| JP2907899B2 (ja) | 高透磁率合金成形体の製造方法およびこの製造方法により得られる成形体の部材によって構成された磁気ヘッド | |
| JPS609849A (ja) | 高強度で高耐酸化性の超硬合金 | |
| JPS6176643A (ja) | 磁気デイスク用アルミニウム基板 | |
| JPH02118056A (ja) | 磁性材料及びそれを用いた磁気ヘッド | |
| JPH07166281A (ja) | 耐摩耗性磁性合金 | |
| CA1078225A (en) | Metallurgical composition embodying hard metal carbides, and method of making | |
| JPH04131342A (ja) | 耐摩耗性に優れた焼結軟磁性材料 | |
| JPS5927371B2 (ja) | Fe↓−Co系磁性材料 | |
| JPS59145760A (ja) | 快削性耐食性高透磁率合金 | |
| JPS63307246A (ja) | 快削性高透磁率合金 | |
| JPH02153052A (ja) | 磁気記録再生ヘッド用耐摩耗性高透磁率合金の製造法ならびに磁気記録再生ヘッド | |
| JPS5927373B2 (ja) | Fe↓−Co系磁性材料 | |
| CA1054401A (en) | Metallurgical composition embodying hard metal carbides, and method of making |