JPS642206A - Composition for forming conductive film - Google Patents
Composition for forming conductive filmInfo
- Publication number
- JPS642206A JPS642206A JP15528187A JP15528187A JPS642206A JP S642206 A JPS642206 A JP S642206A JP 15528187 A JP15528187 A JP 15528187A JP 15528187 A JP15528187 A JP 15528187A JP S642206 A JPS642206 A JP S642206A
- Authority
- JP
- Japan
- Prior art keywords
- powder
- conductive film
- bismuth oxide
- particles
- composition
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE: To make it possible to form a conductive film with reduced deterioration of its junction strength with a base plate by including glass powder and/or bismuth oxide powder as surfaces of their particles are coated with Pd powder.
CONSTITUTION: In a composition, the surface of particles of glass powder and/or bismuth oxide powder are coated with Pd powder. Coating on glass powder and bismuth oxide powder with Pd powder is achieved by a mixing machine which mixes them while roughly grinding them, but if a particle diameter of the Pd powder is too large, the surface of the particles of glass powder and bismuth oxide powder can not be effectively coated, and if it is too small, the Pd powder easily coagulates, then this results in the same situation. Accordingly, deterioration of the junction strength of a conductive film with a base plate can be reduced and reliability of its junction can be enhanced.
COPYRIGHT: (C)1989,JPO&Japio
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP15528187A JPS642206A (en) | 1987-06-24 | 1987-06-24 | Composition for forming conductive film |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP15528187A JPS642206A (en) | 1987-06-24 | 1987-06-24 | Composition for forming conductive film |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH012206A JPH012206A (en) | 1989-01-06 |
| JPS642206A true JPS642206A (en) | 1989-01-06 |
| JPH0574165B2 JPH0574165B2 (en) | 1993-10-15 |
Family
ID=15602470
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP15528187A Granted JPS642206A (en) | 1987-06-24 | 1987-06-24 | Composition for forming conductive film |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS642206A (en) |
Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS59188108A (en) * | 1983-04-08 | 1984-10-25 | 富士通株式会社 | Terminal electrode paste |
-
1987
- 1987-06-24 JP JP15528187A patent/JPS642206A/en active Granted
Patent Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS59188108A (en) * | 1983-04-08 | 1984-10-25 | 富士通株式会社 | Terminal electrode paste |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0574165B2 (en) | 1993-10-15 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| NO872913D0 (en) | PREPARATION OF UNAGLOMATED PARTICLES OF METAL OXIDE WITH UNIFORM PARTICLE SIZE. | |
| CA2051361A1 (en) | Cementitious compositions and method | |
| JPS56140915A (en) | Pharmaceutical preparation for solid drug | |
| ES8500051A1 (en) | Slow-release perfume compositions and a process for the preparation of them | |
| IE900370L (en) | Water dispersible gemfibrozil compositions | |
| JPS56136838A (en) | Thermoplastic polyester resin composition | |
| JPS5435736A (en) | Carrier material for electrophotography and production of the same | |
| JPS5277136A (en) | Powdered coating composition | |
| JPS5274626A (en) | Adhesive | |
| JPS52137437A (en) | Powdered coating compositions | |
| JPS5617948A (en) | Coloring method for plate glass | |
| JPS51123256A (en) | Fluorine resin dispersions and their preparation | |
| JPS5728140A (en) | Preparation of fine particle for polyester additive | |
| JPS543953A (en) | Vibrating type particle shape controlling apparatus | |
| JPS52107033A (en) | Method of manufacturing slurry-type water dispersed paint | |
| JPS5625409A (en) | Plastic minute particle and preparation thereof | |
| JPS5776141A (en) | Electric contact meterial | |
| JPS6446767A (en) | Electrophotographic carrier | |
| Sokolov et al. | Kinetics of Compacting Glass Ceramic Materials Based on the SiO sub 2--P sub 2 O sub 5 System in the Field of Centrifugal Forces | |
| JPS57188628A (en) | Manufacture of sintered material | |
| HUA | FORMATION OF BI 4 TI 3 O 12 FROM BI 2 O 3-TIO 2 MIXTURES | |
| JPS57190040A (en) | Polyester composition | |
| JPS5226154A (en) | Scanning particles microscopes | |
| JPS5247881A (en) | Preparation of vinyl polymer particles | |
| JPS51145995A (en) | Grindstone for grinding |