JPS6424808A - 親水性高分子重合体中の残存モノマ−の低減方法 - Google Patents
親水性高分子重合体中の残存モノマ−の低減方法Info
- Publication number
- JPS6424808A JPS6424808A JP18261187A JP18261187A JPS6424808A JP S6424808 A JPS6424808 A JP S6424808A JP 18261187 A JP18261187 A JP 18261187A JP 18261187 A JP18261187 A JP 18261187A JP S6424808 A JPS6424808 A JP S6424808A
- Authority
- JP
- Japan
- Prior art keywords
- powder
- hydrophilic polymer
- acrylamide
- weight
- dimethylaminoalkyl
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Solid-Sorbent Or Filter-Aiding Compositions (AREA)
- Compositions Of Macromolecular Compounds (AREA)
- Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP18261187A JPS6424808A (ja) | 1987-07-22 | 1987-07-22 | 親水性高分子重合体中の残存モノマ−の低減方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP18261187A JPS6424808A (ja) | 1987-07-22 | 1987-07-22 | 親水性高分子重合体中の残存モノマ−の低減方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6424808A true JPS6424808A (ja) | 1989-01-26 |
| JPH0558441B2 JPH0558441B2 (mo) | 1993-08-26 |
Family
ID=16121316
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP18261187A Granted JPS6424808A (ja) | 1987-07-22 | 1987-07-22 | 親水性高分子重合体中の残存モノマ−の低減方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6424808A (mo) |
Cited By (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5229488A (en) * | 1989-09-04 | 1993-07-20 | Nippon Shokubai Kagaku Kogyo Co., Ltd. | Method for manufacture of an absorbent resin |
| JPH06306202A (ja) * | 1993-04-23 | 1994-11-01 | Mitsubishi Petrochem Co Ltd | 高吸水性ポリマー組成物 |
| US5866678A (en) * | 1992-12-25 | 1999-02-02 | Nippon Shokubai Co., Ltd. | Absorbent and method for production of absorbent resin |
| JP2002241428A (ja) * | 2001-02-15 | 2002-08-28 | Kao Corp | (メタ)アクリル酸(共)重合体の製造法 |
| US6514615B1 (en) | 1999-06-29 | 2003-02-04 | Stockhausen Gmbh & Co. Kg | Superabsorbent polymers having delayed water absorption characteristics |
| KR100626552B1 (ko) * | 2005-04-06 | 2006-09-22 | 김수동 | 잔류단량제와 개시제 잔류물이 적게 함유된폴리아크릴아마이드 공중합체의 제조 |
| JP2006297373A (ja) * | 2005-02-15 | 2006-11-02 | Nippon Shokubai Co Ltd | 吸水剤、吸収性物品及び吸水剤の製造方法 |
Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS53141388A (en) * | 1977-05-16 | 1978-12-09 | Nitto Chem Ind Co Ltd | Preparation of acrylamide polymer |
| JPS60163956A (ja) * | 1984-02-04 | 1985-08-26 | Arakawa Chem Ind Co Ltd | 吸水性樹脂の製法 |
-
1987
- 1987-07-22 JP JP18261187A patent/JPS6424808A/ja active Granted
Patent Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS53141388A (en) * | 1977-05-16 | 1978-12-09 | Nitto Chem Ind Co Ltd | Preparation of acrylamide polymer |
| JPS60163956A (ja) * | 1984-02-04 | 1985-08-26 | Arakawa Chem Ind Co Ltd | 吸水性樹脂の製法 |
Cited By (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5229488A (en) * | 1989-09-04 | 1993-07-20 | Nippon Shokubai Kagaku Kogyo Co., Ltd. | Method for manufacture of an absorbent resin |
| US5866678A (en) * | 1992-12-25 | 1999-02-02 | Nippon Shokubai Co., Ltd. | Absorbent and method for production of absorbent resin |
| JPH06306202A (ja) * | 1993-04-23 | 1994-11-01 | Mitsubishi Petrochem Co Ltd | 高吸水性ポリマー組成物 |
| US6514615B1 (en) | 1999-06-29 | 2003-02-04 | Stockhausen Gmbh & Co. Kg | Superabsorbent polymers having delayed water absorption characteristics |
| JP2002241428A (ja) * | 2001-02-15 | 2002-08-28 | Kao Corp | (メタ)アクリル酸(共)重合体の製造法 |
| JP2006297373A (ja) * | 2005-02-15 | 2006-11-02 | Nippon Shokubai Co Ltd | 吸水剤、吸収性物品及び吸水剤の製造方法 |
| KR100626552B1 (ko) * | 2005-04-06 | 2006-09-22 | 김수동 | 잔류단량제와 개시제 잔류물이 적게 함유된폴리아크릴아마이드 공중합체의 제조 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0558441B2 (mo) | 1993-08-26 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| TWI476210B (zh) | A method for producing a water - absorbent resin | |
| EP2112172B2 (en) | Particulate water-absorbent polymer and process for production thereof | |
| US4758617A (en) | Process for preparing water-absorbing resin | |
| CN102369254B (zh) | 阻塞地层的方法 | |
| JP3417920B2 (ja) | 超吸収性ポリマー | |
| WO2007126003A1 (ja) | 吸水性樹脂の製造方法 | |
| JP2004002145A (ja) | ヒドロゲル形成性ポリマーと建築材料との混合物 | |
| JP3357093B2 (ja) | 吸水性樹脂の製造方法 | |
| AU743796B2 (en) | Method for producing cationic polyelectrolytes | |
| JPWO2016148153A1 (ja) | 吸水性樹脂および吸水剤 | |
| JPH06122708A (ja) | 吸水性樹脂の製造方法 | |
| JPH0558441B2 (mo) | ||
| JP2000038407A (ja) | 吸水性樹脂の製造方法 | |
| JP4694140B2 (ja) | 吸水性樹脂の製造方法 | |
| EP0482417A1 (en) | Emulsion composition comprising a high molecular weight anionic emulsifying agent and a low molecular weight cationic surfactant, and methods relating thereto | |
| JP5079938B2 (ja) | 吸水剤組成物 | |
| JP4275234B2 (ja) | 部分中和(メタ)アクリル酸系重合体およびその製造方法 | |
| JP4968597B2 (ja) | 複合繊維の製造方法 | |
| JP4868127B2 (ja) | 有機性汚泥の脱水方法 | |
| JP4213320B2 (ja) | 製紙白水中の有価物回収方法 | |
| JP2912683B2 (ja) | 水可溶分の少ない高吸水剤組成物 | |
| JPH05310979A (ja) | 表面グラフト重合法 | |
| US5686555A (en) | Absorbents for acids and lyes | |
| JPS6220511A (ja) | 水溶性重合体分散液の製造方法 | |
| JP3608101B2 (ja) | 水溶性重合体分散液の製造方法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| EXPY | Cancellation because of completion of term |