JPS6466284A - エポキシ樹脂付着防止剤 - Google Patents
エポキシ樹脂付着防止剤Info
- Publication number
- JPS6466284A JPS6466284A JP22352487A JP22352487A JPS6466284A JP S6466284 A JPS6466284 A JP S6466284A JP 22352487 A JP22352487 A JP 22352487A JP 22352487 A JP22352487 A JP 22352487A JP S6466284 A JPS6466284 A JP S6466284A
- Authority
- JP
- Japan
- Prior art keywords
- adhesion
- adhesion agent
- weight
- epoxy resin
- copolymer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP22352487A JPS6466284A (ja) | 1987-09-07 | 1987-09-07 | エポキシ樹脂付着防止剤 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP22352487A JPS6466284A (ja) | 1987-09-07 | 1987-09-07 | エポキシ樹脂付着防止剤 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6466284A true JPS6466284A (ja) | 1989-03-13 |
| JPH0450356B2 JPH0450356B2 (mo) | 1992-08-14 |
Family
ID=16799493
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP22352487A Granted JPS6466284A (ja) | 1987-09-07 | 1987-09-07 | エポキシ樹脂付着防止剤 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6466284A (mo) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0249053A (ja) * | 1988-08-10 | 1990-02-19 | Daikin Ind Ltd | 付着防止剤及び付着防止方法 |
Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS55116782A (en) * | 1979-03-01 | 1980-09-08 | Daikin Ind Ltd | Antiblock agent and its use |
| JPS62149784A (ja) * | 1979-03-01 | 1987-07-03 | Daikin Ind Ltd | 付着防止剤ならびにその用途 |
-
1987
- 1987-09-07 JP JP22352487A patent/JPS6466284A/ja active Granted
Patent Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS55116782A (en) * | 1979-03-01 | 1980-09-08 | Daikin Ind Ltd | Antiblock agent and its use |
| JPS62149784A (ja) * | 1979-03-01 | 1987-07-03 | Daikin Ind Ltd | 付着防止剤ならびにその用途 |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0249053A (ja) * | 1988-08-10 | 1990-02-19 | Daikin Ind Ltd | 付着防止剤及び付着防止方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0450356B2 (mo) | 1992-08-14 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US3673099A (en) | Process and composition for stripping cured resins from substrates | |
| JPS61189693A (ja) | 電子部品の防湿コ−テイング方法 | |
| US20100193573A1 (en) | Method of Improving the Solderability of a Printed Circuit Board | |
| EP1232039B1 (en) | Composition for preventing creeping of a flux for soldering and use thereof | |
| JP2015503998A5 (mo) | ||
| CN114686885A (zh) | 一种线路板用铜面超粗化溶液、制备方法及其应用 | |
| US4657788A (en) | Process for multiple stage autodeposition of organic coatings onto metals | |
| JP2968019B2 (ja) | 樹脂付着防止剤 | |
| EP0996523B1 (en) | Composition for preventing creeping of a flux for soldering | |
| DE68913321T2 (de) | Feuchtigkeitsundurchlässige Überzugszusammensetzung. | |
| US5039472A (en) | Adhesion promoter for thermoplastic substrates and method employing same | |
| JP3710290B2 (ja) | 半田用フラックスの這い上がりを防止する組成物 | |
| JPH11217579A (ja) | 電気接点用処理剤 | |
| JP4621950B2 (ja) | 帯電防止コーティング用組成物 | |
| EP0490118A1 (en) | Photoimagable solder mask and photosensitive composition | |
| JPH0450356B2 (mo) | ||
| KR850001736B1 (ko) | 에폭시수지 부착방지제의 제조방법 | |
| JP2689496B2 (ja) | 防湿性電子部品 | |
| JPS60262812A (ja) | 付着防止剤 | |
| CN118852541A (zh) | 双离子高分子、含其的防尘丁腈橡胶手套及其制造方法 | |
| JP3391821B2 (ja) | 付着防止剤 | |
| JP2762185B2 (ja) | 付着防止剤 | |
| JPS62149784A (ja) | 付着防止剤ならびにその用途 | |
| JP7515240B2 (ja) | 電子基板、電子基板の製造方法及び電子機器 | |
| JP3529489B2 (ja) | はんだ付け用フラックス滲み防止剤 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| LAPS | Cancellation because of no payment of annual fees |