JPS6473714A - Formation of semiconductor thin film - Google Patents
Formation of semiconductor thin filmInfo
- Publication number
- JPS6473714A JPS6473714A JP23156187A JP23156187A JPS6473714A JP S6473714 A JPS6473714 A JP S6473714A JP 23156187 A JP23156187 A JP 23156187A JP 23156187 A JP23156187 A JP 23156187A JP S6473714 A JPS6473714 A JP S6473714A
- Authority
- JP
- Japan
- Prior art keywords
- film
- molecular beam
- growth
- single crystal
- impurity
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE:To eliminate the hindrance of crystal growth by the presence of impurity atoms and to contrive improvement in crystallizability by a method wherein the growth of an impurity-doped single crystal silicon film by a molecular beam epitaxial method is conducted subsequent to the growth of a undoped single crystal silicon film. CONSTITUTION:A single crystal sapphire substrate, which is mirror-polished by conducting chemical and mechanical etching, is provided in the growing chamber of a molecular beam epitaxial MBE device. An electron beam is projected on the substrate 1, the surface of the substrate is cleaned, and a undoped single crystal silicon film 2 is grown on the cleaned surface by projecting a silicon molecular beam. At this time, first, a number of silicon islands are grown, the islands are linked together as their growth progresses, impurity atoms disappear, and the growth of a film 2 is facilitated. Then, after the film 2 has been made flat, an antimony molecular beam is projected together with the silicon molecular beam on the surface of the film 2 as an impurity molecular beam, and an antimony-doped single crystal silicon film 3 is formed on the film 2.
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP23156187A JPH0828325B2 (en) | 1987-09-16 | 1987-09-16 | Method for forming semiconductor thin film |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP23156187A JPH0828325B2 (en) | 1987-09-16 | 1987-09-16 | Method for forming semiconductor thin film |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6473714A true JPS6473714A (en) | 1989-03-20 |
| JPH0828325B2 JPH0828325B2 (en) | 1996-03-21 |
Family
ID=16925438
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP23156187A Expired - Fee Related JPH0828325B2 (en) | 1987-09-16 | 1987-09-16 | Method for forming semiconductor thin film |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPH0828325B2 (en) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH038331A (en) * | 1989-06-06 | 1991-01-16 | Nec Corp | Method and apparatus for forming silicon oxide |
| US8508871B2 (en) * | 2008-08-08 | 2013-08-13 | Nikon Corporation | Lens barrel and image capturing apparatus |
-
1987
- 1987-09-16 JP JP23156187A patent/JPH0828325B2/en not_active Expired - Fee Related
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH038331A (en) * | 1989-06-06 | 1991-01-16 | Nec Corp | Method and apparatus for forming silicon oxide |
| US8508871B2 (en) * | 2008-08-08 | 2013-08-13 | Nikon Corporation | Lens barrel and image capturing apparatus |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0828325B2 (en) | 1996-03-21 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS6415912A (en) | Semiconductor device | |
| CA1225571A (en) | Growth of oriented single crystal semiconductor on insulator | |
| JPS6433936A (en) | Manufacture of semiconductor device | |
| US3935040A (en) | Process for forming monolithic semiconductor display | |
| US3985590A (en) | Process for forming heteroepitaxial structure | |
| US5363793A (en) | Method for forming crystals | |
| US5463254A (en) | Formation of 3-dimensional silicon silicide structures | |
| US5142350A (en) | Transistor having cubic boron nitride layer | |
| US6955985B2 (en) | Domain epitaxy for thin film growth | |
| US5232862A (en) | Method of fabricating a transistor having a cubic boron nitride layer | |
| US5057880A (en) | Semiconductor device having a heteroepitaxial substrate | |
| JPS5493378A (en) | Manufacture for semiconductor device | |
| JPS5598823A (en) | Manufacture of single crystal element | |
| US5081053A (en) | Method for forming a transistor having cubic boron nitride layer | |
| JP2577544B2 (en) | Method for manufacturing semiconductor device | |
| JPS6427222A (en) | Manufacture of thin single crystalline film | |
| JPS6410620A (en) | Manufacture of semiconductor device | |
| EP0455981A1 (en) | Method of forming crystals | |
| JPH0828325B2 (en) | Method for forming semiconductor thin film | |
| JPS57115822A (en) | Manufacture of semiconductor device | |
| Allen | What can molecular beam epitaxy do for silicon devices? | |
| JPS5659700A (en) | Forming method for gallium nitride single crystal thin film | |
| JPH02152221A (en) | Manufacture of soi substrate | |
| JPH0513447A (en) | Field effect transistor and manufacturing method thereof | |
| JPS5768015A (en) | Manufacture of semiconductor device |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| LAPS | Cancellation because of no payment of annual fees |