Un metodo de reduccion de fundicion con efectividad incrementada.Info
- Publication number
- MX9601876A MX9601876A MX9601876A MX9601876A MX9601876A MX 9601876 A MX9601876 A MX 9601876A MX 9601876 A MX9601876 A MX 9601876A MX 9601876 A MX9601876 A MX 9601876A MX 9601876 A MX9601876 A MX 9601876A
- Authority
- MX
- Mexico
- Prior art keywords
- mineral
- melted bath
- gases
- charcoal
- reaction vessel
- Prior art date
Abstract
La invencion se refiere a un método para incrementar la efectividad de la reduccion de fundicion de portadores de metal oxídico, particularmente mineral de hierro, y mejorar la eficiencia térmica de los combustibles cargados en el proceso de reduccion de fundicion que tiene lugar en un recipiente de reaccion que contiene un baño derretido con una capa de escoria y donde los gases de reaccion que escapan del baño derretido son post-quemados con gases oxidantes, el calor resultante siendo transferido al baño derretido y los agentes reactivos, mineral y carbon, son alimentados al fundidor al menos en parte desde la porcion superior a través del espacio para gases del recipiente de reaccion, donde estos agentes reactivos, mineral y carbon son añadidos en una forma compacta al baño derretido como un material compuesto con o sin sustancias adicionales de escolta.
Applications Claiming Priority (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| DE19518343A DE19518343C2 (de) | 1995-05-18 | 1995-05-18 | Schmelzreduktionsverfahren mit erhöhter Effektivität |
| DE19518343.6 | 1995-05-18 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| MX9601876A true MX9601876A (es) | 1997-07-31 |
| MXPA96001876A MXPA96001876A (es) | 1997-12-01 |
Family
ID=
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN110756754A (zh) * | 2019-11-26 | 2020-02-07 | 安徽枫雅轩科技信息服务有限公司 | 一种保护渣添加装置 |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN110756754A (zh) * | 2019-11-26 | 2020-02-07 | 安徽枫雅轩科技信息服务有限公司 | 一种保护渣添加装置 |
| CN110756754B (zh) * | 2019-11-26 | 2021-06-04 | 安徽匠桥财务咨询服务有限公司 | 一种保护渣添加装置 |
Also Published As
| Publication number | Publication date |
|---|---|
| CN1053222C (zh) | 2000-06-07 |
| KR100195881B1 (ko) | 1999-06-15 |
| DE69614757T2 (de) | 2002-03-07 |
| AU678746B2 (en) | 1997-06-05 |
| RU2120476C1 (ru) | 1998-10-20 |
| AR001966A1 (es) | 1997-12-10 |
| JP3007571B2 (ja) | 2000-02-07 |
| KR960041380A (ko) | 1996-12-19 |
| CA2176798A1 (en) | 1996-11-19 |
| TW305881B (es) | 1997-05-21 |
| ATE204914T1 (de) | 2001-09-15 |
| AU678746C (en) | 2002-01-03 |
| ZA963286B (en) | 1996-07-29 |
| US5891214A (en) | 1999-04-06 |
| DE19518343A1 (de) | 1996-11-21 |
| EP0743368B1 (en) | 2001-08-29 |
| DE19518343C2 (de) | 1997-08-21 |
| JPH093514A (ja) | 1997-01-07 |
| CN1147017A (zh) | 1997-04-09 |
| EP0743368A1 (en) | 1996-11-20 |
| DE69614757D1 (de) | 2001-10-04 |
| BR9602328A (pt) | 1998-04-22 |
| AU5082096A (en) | 1997-01-09 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| RU2221053C2 (ru) | Способ прямого плавления и установка для его осуществления | |
| AR001966A1 (es) | Método de reducción por fusion de efectividad mejorada | |
| RU2189397C2 (ru) | Способ производства рафинированного железа | |
| US4601752A (en) | Method of manufacturing metals and/or generating slag | |
| AU716931B2 (en) | Direct reduction of metal oxide agglomerates | |
| CA1050765A (en) | Method for making steel | |
| RU94016951A (ru) | Способ производства чугуна | |
| MX9601216A (es) | Aparato para producir arrabio fundido mediante reduccion directa. | |
| KR950018510A (ko) | 컨버터(converter)를 이용한 철의 제조방법 | |
| DE59610981D1 (de) | Verfahren zur herstellung von flüssigem roheisen oder stahlvorprodukten sowie anlage zur durchführung des verfahrens | |
| PL334865A1 (en) | Refractory wall, metallurgical tank incorporating such wall an dmethod of using such refractory wall | |
| TW348185B (en) | Process for recovering metals from iron oxide bearing masses | |
| RU95100956A (ru) | Способ выплавки стали в мартеновской печи | |
| RU2346057C2 (ru) | Усовершенствованный способ плавки для получения железа | |
| CA2130798A1 (en) | Recovery of Non-Ferrous Metals from Dross | |
| MY116791A (en) | Protective atmosphere heating | |
| UA27012C2 (uk) | Спосіб одержаhhя розплаву заліза | |
| CA2203410A1 (en) | Process for vacuum refining molten steel and apparatus therefor | |
| DK0769125T3 (da) | Fremgangsmåde til smeltning af en metalcharge i en roterovn og roterovn til udøvelse af en sådan fremgangsmåde | |
| CA1043575A (en) | Method and device for melting metals | |
| BG102847A (en) | Method for the reduction and smelting of metal-containing compounds | |
| US5366536A (en) | Method of melting metals | |
| RU2102496C1 (ru) | Способ выплавки стали в основной мартеновской печи | |
| CZ84798A3 (cs) | Způsob tavení oxidických strusek a zbytků po spalování a zařízení pro jeho provádění | |
| WO1995035392A3 (en) | Method for reducing particulate iron ore to molten iron with hydrogen |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| FA | Abandonment or withdrawal |