PL19507B1 - A method of processing natural silicates into highly activated bleach earth. - Google Patents

A method of processing natural silicates into highly activated bleach earth. Download PDF

Info

Publication number
PL19507B1
PL19507B1 PL19507A PL1950732A PL19507B1 PL 19507 B1 PL19507 B1 PL 19507B1 PL 19507 A PL19507 A PL 19507A PL 1950732 A PL1950732 A PL 1950732A PL 19507 B1 PL19507 B1 PL 19507B1
Authority
PL
Poland
Prior art keywords
earth
acid
amount
highly activated
processing natural
Prior art date
Application number
PL19507A
Other languages
Polish (pl)
Filing date
Publication date
Application filed filed Critical
Publication of PL19507B1 publication Critical patent/PL19507B1/en

Description

Znancm jest wytwarzanie ziemi bielacej z naturalnych krzemianów przez zarobienie ich na mul zapomoca wody z dodatkiem kwasu solnego lub siarkowego, których ilosc dobierano do osiagniecia najwyzszej sily bielenia, zaleznie od rodzaju i suchosci mu¬ lu, i nastepne gotowanie materjalu, przesa¬ czenie na filtrach prasowych, przemywanie, suszenie i mielenie, podczas gdy lugi pozo¬ stawaly jako strata lub byly przerabiane dalej na cenne skladniki.Proponowano równiez przygotowywac ziemie bielaca w ten sposób, ze zamiast go¬ towac, dzialano na ziemie surowa kwasem in statu nascendi. Ziemie mieszano, naprzy- klad, z sola kuchenna i traktowano kwasem siarkowym. Znane jest ponadto wytwarza¬ nie ziemi bielacej w ten sposób, ze na ziemie surowa dzialano kwasem siarkowym lub dwusiarczanem lub mieszanina obu tych cial i mieszanine reakcyjna suszono calko¬ wicie lub prawie calkowicie. Wreszcie znane jest wytrawianie naturalnej nie przeprowa¬ dzonej w mul i nie zmielonej ziemi bielacej stezonym kwasem solnym, sola odszczepia- jaca kwas lub cialem podobnem.Wedlug tych znanych sposobów zuzywa sie, np. na 100 kg suchego surowca, w ce-lu osiagniecia mozliwie najwiekszej mocy bielenia, 28.-36 kg HCl lub 38 — 49 kg H2SO±, które ostatecznie Wydziela sie jako lugi.Proponowano równiez ziemia surowa wytrawiac wolnym kwasem, stosujac zasa¬ de przeciwpradu, w szeregu kolejno wla¬ czonych zbiorników w ten sposób, ze ziemie surowa doprowadzano z jednego konca, a potrzebna do wytrawiania ilosc kwasu z drugiego konca aparatury tak, iz ziemia i kwas byly przetlaczane przez aparature w przeciwpradzie, przyczem kwas stopniowo sie zuzywal i wylugowywal rozpuszczalne sole zawarte w ziemi surowej, wskutek cze¬ go otrzymywano ostatecznie ziemie wytra¬ wiona, która usuwano z aparatury i prze¬ rabiano dalej, podczas gdy zuzyty kwas, jako lug odpadkowy, byl stracony. Wedlug tego sposobu miano osiagnac lepsze wyko¬ rzystanie kwasu, niz w sposobach, nie sto¬ sujacych zasady przeciwpradu.Wykryto obecnie, ze mozna osiagnac nietylko calkowite zuzycie kwasu, lecz po¬ nadto mozna nawet jeszcze zaoszczedzic znaczne jego ilosci przy jednej i tej samej jakosci materjalu wyjsciowego i jednako¬ wej mocy bielenia otrzymywanej ziemi, skoro przed lub podczas gotowania w spo¬ sobie opisanym na wstepie dodac do ziemi surowej obok stosowanego dotychczas kwa¬ su wolnego jeszcze pewnych soli tegoz kwasu.Stosujac kwas solny, mozna bylo zao¬ szczedzic jedna trzecia dotychczas zuzywa¬ nej ilosci, skoro do kwasu dodano dosta¬ teczna ilosc soli kuchennej lub chlorku wap¬ niowego. Okazalo sie równiez, ze przy za¬ stosowaniu chlorków zelaza, glinu lub ziem alkalicznych mozna zaoszczedzic znaczne ilosci kwasu, których wielkosc zalezy od stezenia dodawanych za kazdym razem chlorków. Stosujac kwas siarkowy, jako srodek wytrawiajacy, nalezy dodawac siar¬ czanów odpowiednich.Wykryto ponadto, ze tego rodzaju zao¬ szczedzenie kwasu mozna osiagnac nietylko zapomoca wyzej przytoczonych soli, lecz równiez i zapomoca lugów odpadkowych otrzymywanych wedlug sposobu znanego lub sposobu wedlug wynalazku. Lugi te, za¬ leznie od wlasnosci uzytego surowca, za¬ wieraja obok nieznacznych ilosci wolnego kwasu przewaznie sole glinowe, jak rów¬ niez zmienne ilosci soli zelazowych, ziem alkalicznych i alkalicznych stosowanych w poszczególnych przypadkach kwasów.Najkorzystniej przy wytrawianiu kwa¬ sem solnym stosowac lugi odpadkowe z po¬ przedniego wytrawiania kwasem solnym, a przy uzyciu kwasu siarkowego lugi odpad¬ kowe z poprzedniego wytrawiania kwasem siarkowym, wskutek czego przy najkorzyst¬ niejszem stosowaniu sposobu mozna wy¬ tworzyc dowolnie powtarzajacy sie obieg kolowy lugów.Sposób wedlug wynalazku prowadzi sie jak nastepuje.Ziemie surowa zarabia sie badz jak do¬ tychczas woda, dodajac jednoczesnie lub pózniej jedna lub kilka ze wspomnianych soli, jeden ze wspomnianych lugów odpad¬ kowych lub odpowiednia mieszanine. Naj¬ korzystniej zarabianie na mul uskutecznia sie zapomoca samych roztworów soli lub lugów, a to w celu unikniecia niepotrzebne¬ go rozcienczania wody uzytej do zarabia¬ nia na mul.Zaleznie od rodzaju i ilosci uzytych roztworów solnych lub lugów odpadkowych ilosc kwasu dodawanego mozna ograniczyc wiecej lub mniej. Dla ilosci kwasu zao¬ szczedzonego miarodajny jest w kazdym poszczególnym przypadku rodzaj materja¬ lu wyjsciowego, uzytych roztworów soli lub lugów odpadkowych. Nawet w najnieko¬ rzystniejszym przypadku wystarcza znacz¬ nie mniejsza ilosc swiezego kwasu, niz go bylo potrzeba, wedlug dotychczas stosowa¬ nych sposobów, do osiagniecia jednej i tej samej mocy bielenia.Ponadto nowy sposób wytrawiania — 2 —zwieksza dosc znacznie wydajnosc wyso- koaktywowanej ziemi bielacej, co przy ce¬ nach produktów wyjsciowych odgrywa rów¬ niez role doniosla. We wszystkich jednak przypadkach, gdzie nie kladzie sie szcze¬ gólnego nacisku na zaoszczedzenie kwasu i wieksza wydajnosc ziemi bielacej i gdzie dalej prowadzi sie prace zapomoca stoso¬ wanej dotychczas ilosci kwasu, jest pomi¬ mo to korzystnie stosowac dodatkowe ilosci roztworów soli lub lugów odpadkowych, gdyz przez to osiaga sie te korzysc, iz lugi odpadkowe otrzymuje sie w postaci stezo¬ nej i wskutek tego latwiej je mozna przera¬ biac dalej.Lugi odpadkowe, otrzymywane wedlug sposobu niniejszego, zwiekszaja stopniowo zawartosc cial w nich rozpuszczanych (sole glinu, zelaza, ziem alkalicznych i al- kaljów), wskutek czego, w celu unikniecia nadmiernego stezenia, korzystnie jest po jedno- lub wielokrotnem ich uzyciu dopro¬ wadzic je do odpowiedniego stezenia, do¬ dajac wody, otrzymywanej przy przemy¬ waniu materjalu odsaczonego.I. Przyklad w zastosowaniu do uzywa¬ nego dotychczas sposobu gotowania. 2000 kg ziemi surowej o wilgotnosci ta¬ kiej, jaka posiada po wykopaniu, zawiera¬ jacej 1140 kg suchej substancji, zarabia sie na mul 1420 1 wody, poczem zadaje sie 1250 1 kwasu solnego o 18° Be (36 kg chlo¬ rowodoru na 100 kg suchej substancji) go¬ tuje i w sposób znany przerabia dalej.Wydajnosc wynosi 78,5% w stosunku do uzytej suchej substancji.II Przyklad w wykonaniu wedlug wy¬ nalazku. 2000 kg ziemi surowej o wilgotnosci takiej, jaka posiada po wykopaniu, zawie¬ rajacej 1140 kg suchej substancji, zarabia sie na mul 1420 1 roztworu chlorku glino¬ wego o 10° Be, poczem dodaje sie 700 1 kwasu solnego o 18° Be (= 20 kg chloro¬ wodoru na 100 kg suchej substancji), gotu¬ je i przerabia dalej w sposób znany.Wydajnosc wynosi 82% uzytej suchej substancji i produkt posiada taka sama moc bielenia, jak i ziemia bielaca otrzymana w przykladzie I.III Przyklad wedlug wynalazku. 2000 kg ziemi surowej, o wilgotnosci ta¬ kiej jaka posiada po wykopaniu, która za¬ wiera 1140 kg suchej substancji zarabia sie na mul 1420 1 lugów odpadkowych o 10° Be, otrzymanych przy poprzednim procesie go¬ towania, poczem zadaje 700 1 kwasu solne¬ go o 18° Be (= 20 kg chlorowodoru na 100 kg suchej substancji), gotuje i przerabia dalej w sposób zwykly.Wydajnosc wynosi równiez 82% w sto¬ sunku do uzytej suchej substancji, przy- czem ziemia bielaca posiada taka sama moc bielenia jak i ziemia bielaca otrzymana w przykladzie I. PLIt is important to make bleaching earth from natural silicates by making them into mulch with water with the addition of hydrochloric or sulfuric acid, the amount of which was selected to achieve the highest bleaching power, depending on the type and dryness of the sludge, and then cooking the material, filtering on filters Pressing, washing, drying and grinding while the liquors remained a waste or were further processed into valuable ingredients. It was also proposed to prepare the bleaching earth in such a way that, instead of boiling, the earth was treated with raw acid in statu nascendi. The lands were mixed, for example, with table salt and treated with sulfuric acid. It is also known to produce bleaching earth in such a way that the raw earth is treated with sulfuric acid or disulphate, or a mixture of both, and the reaction mixture is dried completely or almost completely. Finally, it is known to etch natural, unmilted and unground bleaching earth with concentrated hydrochloric acid, an acid-splitting salt or the like. According to these known methods, for example, 100 kg of dry raw material is used in order to achieve the best possible effect. the highest bleaching power, 28-36 kg of HCl or 38-49 kg of H 2 SO, which eventually precipitate out as a slurry. It has also been proposed to etch the raw earth with free acid, using the principle of counter-current, in a series of tanks that were turned on in this way. that the raw earth was supplied from one end, and the amount of acid needed for etching from the other end of the apparatus, so that the earth and acid were forced through the apparatus in counter-current, because the acid was gradually consumed and the soluble salts contained in the raw earth were leached out, as a result of which eventually the etching earth which was removed from the apparatus and processed further, while the spent acid as waste liquor was lost. This process seeks to achieve better acid utilization than in non-countercurrent processes. It has now been found that not only total acid consumption can be achieved, but also considerable amounts of acid can be saved for one and the same quality. of the starting material and the same bleaching power of the resulting soil, since, before or during cooking in the manner described in the introduction, add to the raw soil, in addition to the previously used free acid, some salts of this acid. Using hydrochloric acid, it was possible to spare one the third amount heretofore used as sufficient salt or calcium chloride was added to the acid. It also turned out that when using iron, aluminum or alkaline earth chlorides, considerable amounts of acid can be saved, the amount of which depends on the concentration of the added chlorides each time. When sulfuric acid is used as an etching agent, suitable sulphates should be added. Moreover, it has been found that such acid preservation can be achieved not only by the abovementioned salts, but also by waste slurry obtained according to the known method or the method according to the invention. These liquors, depending on the nature of the raw material used, contain, apart from small amounts of free acid, mostly aluminum salts, as well as variable amounts of iron, alkaline earth and alkaline salts of the acids used in each case. waste liquors from previous hydrochloric acid etching, and with the use of sulfuric acid, waste liquors from previous sulfuric acid etching, as a result of which, with the most advantageous application of the method, any arbitrarily repeating cycle of liquors can be produced. The raw earth is made or, as hitherto, water, by adding simultaneously or later one or more of the aforementioned salts, one of the said waste liquors or a suitable mixture. Most preferably, the mulching is done using only salt solutions or lyes in order to avoid unnecessarily diluting the water used to make the mulch. Depending on the type and amount of salt solutions or residual lyes used, the amount of acid added may be limited more or less. The type of starting material, salt solutions or waste liquors used in each particular case is decisive for the amount of the stored acid. Even in the most unfavorable case, a much smaller amount of fresh acid than it was needed, according to the methods used hitherto, to achieve one and the same bleaching power. Moreover, the new etching method - 2 - increases quite significantly the yield of highly activated bleaching earth, which also plays an important role in the output prices. In all cases, however, where no particular emphasis is placed on saving acid and increasing the efficiency of bleaching earth, and where work is continued with the amount of acid used hitherto, it is advantageous to use additional amounts of salt solutions or waste liquors, for this has the advantage that the waste liquors are obtained in a concentrated form and can therefore be processed further more easily. The waste liquors obtained according to the present method gradually increase the content of the bodies dissolved in them (aluminum, iron, alkaline earth and alkali), so that, in order to avoid excessive concentration, it is advantageous to bring them to the appropriate concentration after one or more use, by adding water, obtained when washing the drained material. Example as applied to the cooking method used hitherto. 2,000 kg of raw soil with a moisture content of 1,140 kg of dry matter after excavation is made into 1,420 liters of water, and then 1,250 liters of hydrochloric acid at 18 ° Be are added (36 kg of hydrogen chloride per 100 kg of dry substance) is cooked and further processed in a manner known per se. The yield is 78.5% in relation to the dry substance used. II Example in an embodiment according to the invention. 2,000 kg of raw earth with a moisture content of 1140 kg of dry matter as it has after excavation, is made into a mul of 1,420 liters of aluminum chloride solution at 10 ° Be, then 700 liters of hydrochloric acid at 18 ° Be (= 20 kg of hydrogen chloride per 100 kg of dry matter), boiled and further processed in a manner known per se. The yield is 82% of the dry substance used and the product has the same bleaching power as the bleaching earth obtained in Example I.III. . 2,000 kg of raw soil, with a moisture content of 1140 kg of dry matter, is obtained for a mul of 1,420 liters of waste liquor of 10 ° Be obtained during the previous cooking process, and then 700 liters of hydrochloric acid are added. By 18 ° Be (= 20 kg of hydrogen chloride per 100 kg of dry substance), boiled and further processed as usual. The yield is also 82% of the dry substance used, but the bleaching earth has the same bleaching power as well as the bleaching earth obtained in the example of I. PL

Claims (5)

Zastrzezenia patentowe. 1. Sposób przeróbki naturalnych krze¬ mianów na wysokoaktywowana ziemie bie¬ laca, wedlug którego zarabia sie ziemie su¬ rowa na mul i gotuje ja z czynnikiem wy¬ trawiajacym w pradzie jednokierunkowym, znamienny tern, ze obok stosowanych do¬ tychczas kwasów wolnych stosuje sie do¬ datkowo odpowiednie, rozpuszczalne w wo¬ dzie sole tych kwasów, a wiec przy wytra¬ wianiu kwasem solnym stosuje sie chlorki, przy wytrawianiu zas kwasem siarkowym— siarczany.Patent claims. 1. The method of processing natural silicates into highly activated bleach earth, according to which raw earth is made into mulch and boiled with an etching agent in a unidirectional current, characterized by the fact that apart from the free acids used so far, in addition, suitable water-soluble salts of these acids, such as chlorides in the digestion with hydrochloric acid, and sulfates in the digestion with sulfuric acid. 2. Sposób wedlug zastrz. 1, znamienny tern, ze obok lub zamiast stosowanych soli rozpuszczalnych w wodzie stosuje sie lugi odpadkowe, jakie otrzymuje sie przy spo¬ sobie wytrawiania na sucho lub na mo¬ kro.2. The method according to claim The method according to claim 1, characterized in that, in addition to or instead of the water-soluble salts used, waste liquors as obtained with a dry or wet etching process are used. 3. Sposób wedlug zastrz. 1 i 2, zna¬ mienny tern, ze na jedna i te sama ilosc ziemi surowej, w celu otrzymania ziemi o jednej i tej samej mocy bielenia, dziala sie zamiast stosowana dotychczas iloscia kwa¬ su tylko czescia tej ilosci. — 3 —3. The method according to p. 1 and 2, the significant point that on one and the same amount of crude earth, in order to obtain a soil of one and the same bleaching power, only a part of this amount is acted upon instead of the amount of acid used hitherto. - 3 - 4. Sposób wedlug zastrz. 1 — 3, zna¬ mienny tern, ze zarabianie na mul ziemi su¬ rowej uskutecznia sie lugami odpadkowe- mi, otrzymanemi przy poprzednim sposobie wytrawiania, lub odpowiedniemi roztwora¬ mi soli.4. The method according to p. 1 to 3, the significant point in which working on a mule of crude soil results in waste slurries obtained in the previous etching method, or with suitable salt solutions. 5. Sposób wedlug zastrz. 1 — 4, zna¬ mienny tern, ze lugi odpadkowe, wykazuja¬ ce po jedno lub wielokrotnem uzyciu zbyt wysokie stezenie, odpowiednio sie rozcien¬ cza i dopiero wtedy stosuje ponownie do wytrawiania. Bayerische Aktiengesellschaft f ii r chemische und Landwirtschaftlich- chemische Fabrikate. Zastepca: K. Czempinski, rzecznik patentowy. Druk L. Boguslawskiego i Ski, Warszawa. PL5. The method according to p. 1-4, the significant trough, which shows too high a concentration after one or more uses, is suitably diluted and only then reused for pickling. Bayerische Aktiengesellschaft f ii r chemische und Landwirtschaftlich- chemische Fabrikate. Deputy: K. Czempinski, patent attorney. Printing by L. Boguslawski and Ski, Warsaw. PL
PL19507A 1932-09-02 A method of processing natural silicates into highly activated bleach earth. PL19507B1 (en)