PL403394A1 - Method for preparing a modified anatase - Google Patents

Method for preparing a modified anatase

Info

Publication number
PL403394A1
PL403394A1 PL403394A PL40339413A PL403394A1 PL 403394 A1 PL403394 A1 PL 403394A1 PL 403394 A PL403394 A PL 403394A PL 40339413 A PL40339413 A PL 40339413A PL 403394 A1 PL403394 A1 PL 403394A1
Authority
PL
Poland
Prior art keywords
nickel
anatase
titanium dioxide
preparing
ammonia
Prior art date
Application number
PL403394A
Other languages
Polish (pl)
Other versions
PL232138B1 (en
Inventor
Antoni Waldemar Morawski
Diana Dolat
Beata Tryba
Beata Michalkiewicz
Jacek Przepiórski
Sylwia Mozia
Zofia Lendzion-Bieluń
Original Assignee
Zachodniopomorski Uniwersytet Technologiczny W Szczecinie
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zachodniopomorski Uniwersytet Technologiczny W Szczecinie filed Critical Zachodniopomorski Uniwersytet Technologiczny W Szczecinie
Priority to PL403394A priority Critical patent/PL232138B1/en
Publication of PL403394A1 publication Critical patent/PL403394A1/en
Publication of PL232138B1 publication Critical patent/PL232138B1/en

Abstract

Sposób otrzymywania fotokatalitycznego anatazu, wykorzystujący proces kalcynacji, charakteryzuje się tym, że wysuszony amorficzny ditlenek tytanu impregnuje się roztworem soli niklu, suszy przez noc w temperaturze 100°C, uciera w moździerzu do postaci proszku i następnie kalcynuje w temperaturze do 700°C w atmosferze amoniaku. Jako sól niklu stosuje się azotan niklu (II), siarczan niklu (II), chlorek niklu (II) w ilości odpowiadającej zawartości niklu od 1% mas. do 10% masowych w stosunku do ditlenku tytanu. Kalcynację prowadzi się w atmosferze amoniaku przez 4 godziny w temperaturze poniżej przemiany anatazu w rutyl, to jest poniżej 700°C.The method of obtaining photocatalytic anatase, using the calcination process, is characterized by the fact that the dried amorphous titanium dioxide is impregnated with a nickel salt solution, dried overnight at 100 ° C, triturated in a mortar to form a powder and then calcined at up to 700 ° C in the atmosphere ammonia. The nickel salt used is nickel (II) nitrate, nickel (II) sulfate, and nickel (II) chloride in an amount corresponding to 1% by weight of nickel. up to 10% by mass in relation to titanium dioxide. Calcination is carried out in an ammonia atmosphere for 4 hours at a temperature below the conversion of anatase to rutile, i.e. below 700 ° C.

PL403394A 2013-04-02 2013-04-02 Method for preparing a modified anatase PL232138B1 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
PL403394A PL232138B1 (en) 2013-04-02 2013-04-02 Method for preparing a modified anatase

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
PL403394A PL232138B1 (en) 2013-04-02 2013-04-02 Method for preparing a modified anatase

Publications (2)

Publication Number Publication Date
PL403394A1 true PL403394A1 (en) 2014-10-13
PL232138B1 PL232138B1 (en) 2019-05-31

Family

ID=51662777

Family Applications (1)

Application Number Title Priority Date Filing Date
PL403394A PL232138B1 (en) 2013-04-02 2013-04-02 Method for preparing a modified anatase

Country Status (1)

Country Link
PL (1) PL232138B1 (en)

Also Published As

Publication number Publication date
PL232138B1 (en) 2019-05-31

Similar Documents

Publication Publication Date Title
CL2015000279A1 (en) Conversion process of plaster fgd into ammonium sulfate and calcium carbonate.
MY194298A (en) Titanium stannate silicate, method of preparation and use thereof
PE20150186A1 (en) CATALYST
EP2757068C0 (en) Synthesis process of a LiM1-x-y-zNyQzFexPO4 compound and its use as electrode material for a lithium battery
WO2015188016A3 (en) Energy-efficient real-time task scheduler
PL403394A1 (en) Method for preparing a modified anatase
DE112014002496A5 (en) Process for the preparation of a powdery precursor material, powdery precursor material and its use
Li et al. Thermodynamic assessment of the Co–Fe–Sb system
PL413966A1 (en) Method for producing TiO2-SnO2 nanocomposites
PL403392A1 (en) Method for preparing a modified rutile
PL403391A1 (en) Method for preparing a modified rutile
PL406503A1 (en) Method for obtaining self-cleaning cement mortars
RU2011100194A (en) METHOD FOR PROCESSING URANIUM HEXAFLUORIDE
PL403556A1 (en) Bed of the photocatalytic removal of hydrogen sulphide from the air and a method for preparing the bed for photocatalytic removal of hydrogen sulphide from the air
JP2009196854A5 (en)
PL409691A1 (en) Method for obtaining photocatalyst based on TiO2 active in the visible light, modified with guanidine carbonate and the application of the photocatalyst based on TiO2 active in the visible light
PL423028A1 (en) Method for producing silicon-modified titanium dioxide
PL403557A1 (en) Method for producing the nanocrystalline titanium dioxide
PL402459A1 (en) Method for photocatalytic reduction of carbon dioxide to methanol
PL411608A1 (en) Method for producing a biocidal product
PL397133A1 (en) Method of purifying aqueous solutions from organic impurities and a photocatalytic contribution for purification of aqueous solutions from organic impurities
JP2016155986A5 (en)
PL406272A1 (en) Method for obtaining cement mortars
Wang et al. Design of monitoring and scheduling system for a large-scale reverse osmosis desalination plant
Lapushkin et al. OPPORTUNITIES AND CHALLENGES IN THE ABSORPTION OF SMALL ENTERPRISES OF А HOLDING