PL404678A1 - Cienkowarstwowa masa tynkarska z perlitem - Google Patents
Cienkowarstwowa masa tynkarska z perlitemInfo
- Publication number
- PL404678A1 PL404678A1 PL404678A PL40467813A PL404678A1 PL 404678 A1 PL404678 A1 PL 404678A1 PL 404678 A PL404678 A PL 404678A PL 40467813 A PL40467813 A PL 40467813A PL 404678 A1 PL404678 A1 PL 404678A1
- Authority
- PL
- Poland
- Prior art keywords
- weight
- perlite
- dust
- minutes
- mass
- Prior art date
Abstract
Wynalazek dotyczy cienkowarstwowej masy tynkarskiej z perlitem, zawierającej 5-15% wagowych perlitu ekspandowanego o uziarnieniu do 4 mm. Co najmniej 5% wagowych, korzystnie 15-85% wagowych perlitu ekspandowanego stanowi granulat uzyskany z odpadowego pyłu perlitowego poprzez połączenie w warunkach ciągłego mieszania pyłu perlitowego o uziarnieniu poniżej 0,5 mm z lepiszczem w postaci wodnej dyspersji polimerowej. Stosuje się 50-150 części wagowych lepiszcza na 100 części wagowych pyłu. W początkowym etapie procesu stosuje się obroty bębna 1-20 obr/min, a następnie, w czasie 3-15 minut zwiększa się je do 50-100 obr/min i jednocześnie podgrzewa radiacyjnie masę w całej objętości promieniowaniem podczerwonym do temperatury nie wyższej niż 80°C. Mieszanie kontynuuje się przez 5-30 minut, po czym masę suszy konwekcyjnie strumieniem powietrza przez okres 60-180 minut utrzymując temperaturę nawiewu na poziomie 40-80°C, aż do uzyskania kulistych granul o wielkości 0,5-1,5 mm i zawartości wilgoci poniżej 1,5% wagowego, w ilości co najmniej 70% wagowych użytego pyłu perlitowego.
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| PL404678A PL226938B1 (pl) | 2013-07-12 | 2013-07-12 | Cienkowarstwowa masa tynkarska zperlitem |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| PL404678A PL226938B1 (pl) | 2013-07-12 | 2013-07-12 | Cienkowarstwowa masa tynkarska zperlitem |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| PL404678A1 true PL404678A1 (pl) | 2014-05-12 |
| PL226938B1 PL226938B1 (pl) | 2017-10-31 |
Family
ID=50636986
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| PL404678A PL226938B1 (pl) | 2013-07-12 | 2013-07-12 | Cienkowarstwowa masa tynkarska zperlitem |
Country Status (1)
| Country | Link |
|---|---|
| PL (1) | PL226938B1 (pl) |
-
2013
- 2013-07-12 PL PL404678A patent/PL226938B1/pl unknown
Also Published As
| Publication number | Publication date |
|---|---|
| PL226938B1 (pl) | 2017-10-31 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN101914257B (zh) | 一种高效复合调湿剂的制备方法 | |
| CN102660100B (zh) | 一种有机无机复合调湿剂的制备方法 | |
| JP2005097604A5 (pl) | ||
| JP2016104119A5 (pl) | ||
| JP2016073898A5 (pl) | ||
| JP2018090638A5 (pl) | ||
| CN104098318A (zh) | 一种生物质多孔相变调温调湿材料及其制备方法 | |
| PL406381A1 (pl) | Sposób wytwarzania lekkich proppantów ceramicznych i lekkie proppanty ceramiczne | |
| MX2018003579A (es) | Procedimiento para preparar un composite cementiceo, morteros y hormigones micro-nanoestructurados de larga vida en servicio, que comprenden dicho composite. | |
| CN109133729A (zh) | 一种负离子矿棉板及其制备方法 | |
| EA201001537A1 (ru) | Гранулированная агрохимическая композиция и способы её получения | |
| JP2015231600A5 (pl) | ||
| PL404678A1 (pl) | Cienkowarstwowa masa tynkarska z perlitem | |
| CN105732011A (zh) | 一种新型多功能硅藻土陶粒的制备方法 | |
| PL404679A1 (pl) | Sposób wytwarzania granulatu z odpadowego pylu perlitowego | |
| KR101153918B1 (ko) | 조습 및 유해물질 저감 기능이 있는 석고보드 | |
| CN104941397A (zh) | 一种硅藻土干燥剂及其生产工艺 | |
| KR20140130371A (ko) | 습기 탈취제 | |
| CN109529766A (zh) | 一种环保强吸湿pvc干燥剂及其制备方法 | |
| CN1978047A (zh) | 用凹凸棒石粘土制备食品仪器用干燥剂的方法 | |
| CN103571119B (zh) | 一种复合防虫调湿剂的制备方法 | |
| RU2013147941A (ru) | Линия производства комбикормовых добавок и премиксов | |
| CN103951339B (zh) | 一种易破碎材料人工制备的制备方法 | |
| KR101735162B1 (ko) | 천일염을 포함하는 건축 내장용 마감재 조성물 및 이의 제조 방법 | |
| RU2013141432A (ru) | Способ получения гранулированного азотного удобрения или мелиоранта из золошлаковой смеси |