PL433572A1 - Sposób spieniania asfaltu z zastosowaniem dwuskładnikowego dodatku - Google Patents
Sposób spieniania asfaltu z zastosowaniem dwuskładnikowego dodatkuInfo
- Publication number
- PL433572A1 PL433572A1 PL433572A PL43357220A PL433572A1 PL 433572 A1 PL433572 A1 PL 433572A1 PL 433572 A PL433572 A PL 433572A PL 43357220 A PL43357220 A PL 43357220A PL 433572 A1 PL433572 A1 PL 433572A1
- Authority
- PL
- Poland
- Prior art keywords
- asphalt
- temperature
- weight
- mixed until
- foaming
- Prior art date
Abstract
Przedmiotem wynalazku jest sposób spieniania asfaltu z zastosowaniem dwuskładnikowego dodatku pozwalający na obniżenie temperatury produkcji mieszanek mineralno-asfaltowych. Sposób spieniania asfaltu z zastosowaniem dwuskładnikowego dodatku polega na tym, że do zeolitu syntetycznego wymieszanego z wermikulitem w proporcjach wagowych od 1 :4 do 4: 1 dodaje się wodę w ilości od 25% do 200% wagowych suchej mieszanki i miesza się do momentu uzyskania mieszaniny o jednolitej strukturze. Następnie mieszaninę w ilości od 2% do 10% wagowo w stosunku do masy asfaltu dodaje się do gorącego asfaltu o temperaturze od 140°C do 175°C i miesza się do momentu rozpoczęcia spieniania asfaltu. W dalszej kolejności dodaje się spieniony asfalt do mieszanki mineralnej o temperaturze od 110°C do 135°C i miesza się do uzyskania całkowitego otoczenia kruszywa asfaltem po czym mieszankę mineralno-asfaltową zagęszcza w temperaturze od 105°C do 130°C.
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| PL433572A PL237068B1 (pl) | 2020-04-17 | 2020-04-17 | Sposób spieniania asfaltu z zastosowaniem dwuskładnikowego dodatku |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| PL433572A PL237068B1 (pl) | 2020-04-17 | 2020-04-17 | Sposób spieniania asfaltu z zastosowaniem dwuskładnikowego dodatku |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| PL433572A1 true PL433572A1 (pl) | 2020-09-07 |
| PL237068B1 PL237068B1 (pl) | 2021-03-08 |
Family
ID=72291478
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| PL433572A PL237068B1 (pl) | 2020-04-17 | 2020-04-17 | Sposób spieniania asfaltu z zastosowaniem dwuskładnikowego dodatku |
Country Status (1)
| Country | Link |
|---|---|
| PL (1) | PL237068B1 (pl) |
-
2020
- 2020-04-17 PL PL433572A patent/PL237068B1/pl unknown
Also Published As
| Publication number | Publication date |
|---|---|
| PL237068B1 (pl) | 2021-03-08 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| ES2753978T3 (es) | Composición ligera a base de ceniza volante | |
| PL423255A1 (pl) | Sposób spieniania asfaltu | |
| BR112019000369A2 (pt) | cimento espumoso leve, placa de cimento e métodos para produzir os mesmos | |
| PL436074A1 (pl) | Sposób wykonania mieszanki mineralno-asfaltowej mastyksowo grysowej (SMA) i mieszanka mineralno-asfaltowa mastyksowo grysowa (SMA) do budowy nawierzchni drogowej | |
| PL433575A1 (pl) | Sposób spieniania asfaltu z zastosowaniem mineralnego dodatku | |
| RU2443647C1 (ru) | Комплексная добавка для пенобетонной смеси | |
| PL433572A1 (pl) | Sposób spieniania asfaltu z zastosowaniem dwuskładnikowego dodatku | |
| PL433576A1 (pl) | Sposób spieniania asfaltu z zastosowaniem dwuskładnikowego mineralnego dodatku | |
| PL433574A1 (pl) | Sposób spieniania asfaltu z zastosowaniem dodatku mineralnego | |
| CN103964890A (zh) | 新型泡沫混凝土保温砌块及制备方法 | |
| PL433573A1 (pl) | Sposób spieniania asfaltu z zastosowaniem dodatku dwuskładnikowego | |
| RU2621250C1 (ru) | Комплексная добавка для пенобетонной смеси | |
| PL433579A1 (pl) | Sposób wytwarzania mieszanki mineralno-asfaltowej z zastosowaniem dwuskładnikowego mineralnego dodatku | |
| PL433577A1 (pl) | Sposób spieniania asfaltu z zastosowaniem dodatku dwuskładnikowego mineralnego | |
| PL423256A1 (pl) | Sposób spieniania asfaltu | |
| PL433578A1 (pl) | Sposób wytwarzania mieszanki mineralno-asfaltowej z zastosowaniem dodatku mineralnego | |
| FR2352763A1 (fr) | Revetement semi-rigide pour surfaces de circulation et procede pour sa fabrication | |
| RU2561121C2 (ru) | Сырьевая смесь для изготовления легкого бетона и способ изготовления легкого бетона из сырьевой смеси | |
| PL429523A1 (pl) | Sposób spieniania lepiszcza asfaltowego z użyciem zeolitu nasączonego wodą | |
| RU2123483C1 (ru) | Комплексная добавка для цементно-бетонных смесей | |
| PL438019A1 (pl) | Mieszanka betonu lekkiego i fibro-kompozytu cementowego dla budownictwa oraz sposób ich wytwarzania | |
| PL429521A1 (pl) | Sposób spieniania lepiszcza asfaltowego z użyciem zeolitu | |
| PL429524A1 (pl) | Sposób spieniania lepiszcza asfaltowego z użyciem zeolitu nasączonego wodą | |
| PL429522A1 (pl) | Sposób spieniania lepiszcza asfaltowego z użyciem zeolitu | |
| PL226802B1 (pl) | Sposób wytwarzania mieszanek mineralno-asfaltowych |