TH14252C3 - The production process of ready-mixed concrete, pump-type waterproofing - Google Patents

The production process of ready-mixed concrete, pump-type waterproofing

Info

Publication number
TH14252C3
TH14252C3 TH1603001340U TH1603001340U TH14252C3 TH 14252 C3 TH14252 C3 TH 14252C3 TH 1603001340 U TH1603001340 U TH 1603001340U TH 1603001340 U TH1603001340 U TH 1603001340U TH 14252 C3 TH14252 C3 TH 14252C3
Authority
TH
Thailand
Prior art keywords
concrete
cement
sand
per cubic
cubic meter
Prior art date
Application number
TH1603001340U
Other languages
Thai (th)
Other versions
TH14252A3 (en
Inventor
มากุล นายณัฏฐ์
Filing date
Publication date
Application filed filed Critical
Publication of TH14252C3 publication Critical patent/TH14252C3/en
Publication of TH14252A3 publication Critical patent/TH14252A3/en

Abstract

แก้ไข 30/8/2560 กรรมวิธีการผลิตคอนกรีตผสมเสร็จชนิดงานปั๊มกันซึม มีวัตถุประสงค์เพื่อนำวัตถุดิบของการผลิต คอนกรีตสำหรับงานปั๊มกันซึมมาทำการผสมตามขั้นตอนเฉพาะโดยเครื่องผสมที่มีสมรรถนะเฉพาะ โดยเริ่มจาก การเตรียมเครื่องผสมคอนกรีตที่ภายในมีความสะอาด ชั่งหินขนาดโตสุด 6.0 มิลลิเมตร และปูนซีเมนต์ใส่ลงใน เครื่องผสมคอนกรีต จากนั้นจึงเปิดเครื่องเพื่อผสมให้หินและทรายและปูนซีเมนต์คลุกเคล้าเป้นเนื้อเดียวกันใน เครื่องผสม เมื่อส่วนผสมคลุกเคล้าเข้ากันดีแล้ว จึงเติมน้ำที่ใช้ผสมทั้งหมด เมื่อน้ำที่เติมลงผสมเข้ากันดีแล้วกับ ทราย หิน และปูนซีเมนต์ จึงเริ่มเติมน้ำยาผสมคอนกรีต ปริมาณ 1.975 ลิตรต่อลูกบาศก์เมตร พร้อมเปิด เครื่องผสมคอนกรีตเพื่อให้น้ำยาที่เติมลงไปเข้ากันได้ดีกับส่วนผสมของคอนกรีตเป็นเวลา 30 วินาที จึงเสร็จสิ้น กระบวนการผสม .......................................................................................................................................................... แก้ไข 05/01/2560 กรรมวิธีการผลิตคอนกรีตผสมเสร็จชนิดงานปั๊มกันซึม มีวัตถุประสงค์เพี่อนำวัตถุดิบของการผลิต คอนกรีตสำหรับงานปั๊มกันซึมมาทำการผสมตามขั้นตอนเฉพาะโดยเครื่องผสมที่มีสมรรถนะเฉพาะ โดยเริ่มจาก การเตรียมเครื่องผสมคอนกรีตที่ภายในมีความสะอาด ชั่งหินขนาดโตสุด 6.0 มิลลิเมตร และปูนซีเมนต์ใส่ลงใน เครื่องผสมคอนกรีต จากนั้นจึงเปิดเครื่องเพื่อผสมให้หินและทรายและปูนซีเมนต์คลุกเคล้าเป็นเนื้อเดียวกันใน เครื่องผสม เมื่อส่วนผสมคลุกเคล้าเข้ากันดีแล้ว จึงเติมน้ำที่ใช้ผสมทั้งหมด เมื่อน้ำที่เติมลงผสมเข้ากันดีแล้วกับ ทราย หิน และปูนซีเมนต์ จึงเริ่มเติมน้ำยาผสมคอนกรีต ปริมาณ 3.975 ลิตรต่อลูกบาศก์เมตร พร้อมเปิด เครื่องผสมคอนกรีตเพื่อให้น้ำยาที่เติมลงไปเข้ากันได้ดีกับส่วนผสมของคอนกรีตเป็นเวลา 30 วินาที จึงเสร็จสิ้น กระบวนการผสม ------------------------- กรรมวิธีการผลิตคอนกรีตผสมเสร็จชนิดงานปั๊มกันซึม มีวัตถุประสงค์เพื่อนำวัตถุดิบของการผลิต คอนกรีตสำหรับงานปั๊มกันซึมมาทำการผสมตามขั้นตอนเฉพาะโดยเครื่องผสมที่มีสมรรถนะเฉพาะ โดนเริ่มจาก การเตรียมเครื่องผสมคอนกรีตที่ภายในมีความสะอาด ชั่งหินขนาดโตสุด 6.0 มิลลิเมตร และปูนซีเมนต์ใส่ลงใน เครื่องผสมคอนกรีต จากนั้นจึงเปิดเครื่องเพื่อผสมให้หินและทรายและปูนซีเมนต์คลุกเคล้าเป็นเนื้อเดียวกันใน เครื่องผสม เมื่อส่วนผสมคลุกเคล้าเข้ากันดีแล้ว จึงเติมน้ำที่ใช้ผสมทั้งหมด เมื่อน้ำที่เติมลงผสมเข้ากันดีแล้วกับ ทราย หิน และปูนซีเมนต์ จึงเริ่มเติมน้ำยาผสมคอนกรีต ปริมาณ 1.975 ลิตรต่อลูกบาศก์เมตร พร้อมเปิด เครื่องผสมคอนกรีตเพื่อให้น้ำยาที่เติมลงไปเข้ากันได้ดีกับส่วนผสมของคอนกรีตเป็นเวลา 30 วินาที จึงเสร็จสิ้น กระบวนการผสม Correction 30/8/2017 Production process of ready-mixed concrete, waterproofing pump type It is intended to bring raw materials of production. Concrete for waterproofing pump is mixed according to a specific process by a mixer with a specific performance starting from the preparation of a concrete mixer with a clean interior. Weigh the stones up to 6.0 mm. And cement into the Concrete mixer Then turn on the machine to mix the stone and sand and cement into a homogeneous mixture in the mixer. Then add all the water used to mix When the added water is mixed well with sand, stone and cement. Therefore began to add 1.975 liters of concrete admixture per cubic meter and turn on the concrete mixer to make the added solution compatible with the concrete mixture for 30 seconds, then the mixing process was completed ......... .................................................. .................................................. ............................................. Edit 05/01/2017 Production process of ready-mixed concrete with waterproofing pump type The objective is to bring raw materials of production. Concrete for waterproofing pump is mixed according to a specific process by a mixer with a specific performance starting from the preparation of a concrete mixer with a clean interior. Weigh the stones up to 6.0 mm. And cement into the Concrete mixer Then turn on the machine to mix the stone and sand and cement into a homogeneous mixture when the ingredients are thoroughly mixed. Then add all the water used to mix When the added water is mixed well with sand, stone and cement. Then started adding 3.975 liters of concrete admixture per cubic meter and turn on the concrete mixer to make the added solution compatible with the concrete mixture for 30 seconds, then the mixing process was completed --------- ---------------- The production process of ready-mixed concrete pump waterproofing type It is intended to bring raw materials of production. Concrete for waterproofing pump is mixed according to a specific process by a mixer with a specific performance starting from the preparation of a concrete mixer with a clean interior. Weigh the stones up to 6.0 mm. And cement into the Concrete mixer Then turn on the machine to mix the stone and sand and cement into a homogeneous mixture when the ingredients are thoroughly mixed. Then add all the water used to mix When the added water is mixed well with sand, stone and cement. Thus began to add 1.975 liters of concrete admixture per cubic meter and turn on the concrete mixer so that the added solution mixes well with the concrete mixture for 30 seconds, then the mixing process was completed.

Claims (3)

ข้อถือสิทธฺ์ (ทั้งหมด) ซึ่งจะไม่ปรากฏบนหน้าประกาศโฆษณา :แก้ไข 30 ส.ค. 2560 1. กรรมวิธีการผลิตคอนกรีตผสมเสร็จชนิดงานปั๊มกันซึมน้ำมีขั้นตอนดังนี้ ก. เตรียมเครื่องผสมคอนกรีตที่ภายในมีความสะอาดและที่ผิวภายในมีความชุ่มน้ำ (ไม่แห้งสนิท) และ มวลรวม (หินและทราย) ที่มีความชื้นอยู่ในสภาวะอิ่มตัวด้วยน้ำและผิวแห้ง (saturated surface dry) ข. ชั่งหินขนาดโตสุด 6.0 มิลลิเมตร ปริมาณเท่ากับ 1110 กิโลกรัมต่อลูกบาศก์เมตร และปูนซีเมนต์ 300 กิโลกรัมต่อลูกบาศก์เมตร ใส่ลงในเครื่องผสมคอนกรีต จากนั้นจึงเปิดเครื่องด้วยความเร็วรอบ 20 รอบ ต่อนาที เพื่อผสมให้หินและทรายและปูนซีเมนต์คลุกเคล้าเป็นเนื้อเดียวกันในเครื่องผสม เป็นเวลา 1 นาที ค. เมื่อปูนซีเมนต์ ทรายและหิน คลุกเคล้าเข้ากันดีแล้ว ให้ทำการชั่งเถ้าลอยในปริมาณ 75 กิโลกรัมต่อ ลูกบาศก์เมตร แล้วจึงเติมน้ำทั้งหมด ทั้งนี้ระหว่างเติมน้ำให้เปิดเครื่องผสมคอนกรีตเพื่อให้น้ำที่เติมลงไป เข้ากันได้ดีกับส่วนผสมของทรายและปูนซีเมนต์เป็นเวลา 25 วินาที ง. เมื่อน้ำที่เติมลงผสมเข้ากันดีแล้วกับทราย หิน และปูนซีเมนต์ จึงเริ่มเติมน้ำยาผสมคอนกรีต ปริมาณ 1.975 ลิตรต่อลูกบาศก์เมตร พร้อมเปิดเครื่องผสมคอนกรีตเพื่อให้น้ำยาที่เติมลงไปเข้ากันได้ดีกับ ส่วนผสมของคอนกรีตเป็นเวลา 30 วินาที จึงเสร็จสิ้นกระบวนการผสม 2. กรรมวิธีการผลิตคอนกรีตผสมเสร็จชนิดงานปั๊มกันซึมน้ำตามข้อถือสิทธิที่ 1 ที่ซึ่งปูนซีเมนต์ปอร์ตแลนด์ ประเภทที่ 1 มีปริมาณองค์ประกอบเคมีโดยน้ำหนัก ประกอบไปด้วย อะลูมิเนียมออกไซด์ (Al2O3) ร้อยละ 4.35 ซิลิคอนไดออกไซด์ (SiO2) ร้อยละ 20.10 โพแทสเซียมออกไซด์ (K2O) ร้อยละ 0.63 แคลเซียม ออกไซด์ (CaO) ร้อยละ 62.32 ไทเทเนียมไดออกไซด์ (TiO2) ร้อยละ 0.23 เหล็กออกไซด์ (Fe2O3) ร้อยละ 3.24 และมีค่าร้อยละการสูญเสียน้ำหนักเนื่องจากการเผาไหม้ร้อยละ 1.71 ในขณะที่มีสมบัติทางกายภาพ อันประกอบไปด้วย ขนาดเฉลี่ยเท่ากับ 623.8 ไมโครเมตร พื้นที่ผิวจำเพาะเท่ากับ 472 ตารางเมตรต่อ กิโลกรัม ความถ่วงจำเพาะเท่ากับ 3.10 และปริมาณความชื้นร้อยละ 0.12 3. คอนกรีตผสมเสร็จชนิดงานปั๊มกันซึมน้ำตามข้อถือสิทธิที่ 1 หรือ 2 มีดังต่อไปนี้ ปริมาณปูนซีเมนต์เท่ากับ 300 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณเถ้าลอยเท่ากับ 75 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณน้ำผสมคอนกรีตเท่ากับ 140 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณทรายเท่ากับ 855 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณหินขนาดโตสุด 6.0 มิลลิเมตร เท่ากับ 1110 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณน้ำยาผสมคอนกรีตเท่ากับ 1.975 ลิตรต่อลูกบาศก์เมตร ---------------------------------------------------------------------------------------------------- แก้ไข 05/01/2560 1. กรรมวิธีการผลิตคอนกรีตผสมเสร็จชนิดงานปั๊มกันซึมน้ำมีขั้นตอนดังนี้ ก. เตรียมเครื่องผสมคอนกรีตที่ภายในมีความสะอาดและที่ผิวภายในมีความชุ่มน้ำ (ไม่แห้งสนิท) และ มวลรวม (หินและทราย) ที่มีความชื้นอยู่ในสภาวะอิ่มตัวด้วยน้ำและผิวแห้ง (saturated surface dry) ข. ชั่งหินขนาดโตสุด 6.0 มิลลิเมตร ปริมาณเท่ากับ 1110 กิโลกรัมต่อลูกบาศก์เมตร และปูนซีเมนต์ 300 กิโลกรัมต่อลูกบาศก์เมตร ใส่ลงในเครื่องผสมคอนกรีต จากนั้นจึงเปิดเครื่องด้วยความเร็วรอบ 20 รอบ ต่อนาที เพื่อผสมให้หินและทรายและปูนซีเมนต์คลุกเคล้าเป็นเนื้อเดียวกันในเครื่องผสม เป็นเวลา 1 นาที ค. เมื่อปูนซีเมนต์ ทรายและหิน คลุกเคล้าเข้ากันดีแล้ว ให้ทำการชั่งเถ้าลอยในปริมาณ 75 กิโลกรัมต่อ ลูกบาศก์เมตร แล้วจึงเติมน้ำทั้งหมด ทั้งนี้ระหว่างเติมน้ำให้เปิดเครื่องผสมคอนกรีตเพื่อให้น้ำที่เติมลงไป เข้ากันได้ดีกับส่วนผสมของทรายและปูนซีเมนต์เป็นเวลา 25 วินาที ง. เมื่อน้ำที่เติมลงผสมเข้ากันดีแล้วกับทราย หิน และปูนซีเมนต์ จึงเริ่มเติมน้ำยาผสมคอนกรีต ปริมาณ 1.975 ลิตรต่อลูกบาศก์เมตร พร้อมเปิดเครื่องผสมคอนกรีตเพื่อให้น้ำยาที่เติมลงไปเข้ากันได้ดีกับ ส่วนผสมของคอนกรีตเป็นเวลา 30 วินาที จึงเสร็จสิ้นกระบวนการผสม 2. กรรมวิธีการผลิตคอนกรีตผสมเสร็จชนิดงานปั๊มกันซึมน้ำตามข้อถือสิทธิที่ 1 ที่ซึ่งปูนซีเมนต์ปอร์ตแลนด์ ประเภทที่ 1 มีปริมาณองค์ประกอบเคมีโดยน้ำหนัก ประกอบไปด้วย อะลูมิเนียมออกไซด์ (Al2O3) ร้อยละ 4.35 ซิลิคอนไดออกไซด์ (SiO2) ร้อยละ 20.10 โพแทสเซียมออกไซด์ (K2O) ร้อยละ 0.63 แคลเซียม ออกไซด์ (CaO) ร้อยละ 62.32 ไทเทเนียมไดออกไซด์ (1ไ02) ร้อยละ 0.23 เหล็กออกไซด์ (Fe2O3) ร้อยละ 3.24 และมีค่าร้อยละการสูญเสียน้ำหนักเนื่องจากการเผาไหม้ร้อยละ 1.71 ในขณะที่มีสมบัติทางกายภาพ อันประกอบไปด้วย ขนาดเฉลี่ยเท่ากับ 623.8 ไมโครเมตร พื้นที่ผิวจำเพาะเท่ากับ 472 ตารางเมตรต่อ กิโลกรัม ความถ่วงจำเพาะเท่ากับ 3.10 และปริมาณความชื้นร้อยละ 0.12 3. สูตรสัดส่วนผสมคอนกรีตชนิดงานปั๊มกันซึมน้ำตามข้อถือสิทธิที่ 1 หรือ 2 มีดังต่อไปนี้ ปริมาณปูนซีเมนต์เท่ากับ 300 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณเล้าลอยเท่ากับ 75 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณน้ำผสมคอนกรีตเท่ากับ 140 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณทรายเท่ากับ 855 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณหิน เท่ากับ 1110 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณน้ำยาผสมคอนกรีตเท่ากับ 3.975 ลิตรต่อลูกบาศก์เมตร -------------------------Disclaimer (all) which will not appear on the advertisement page: Amendment 30 Aug 2017 1. The production process of ready-mixed concrete with waterproofing pump has the following steps: a. Prepare a concrete mixer with Cleanliness and that the interior surface is wet (Not completely dry) and aggregate (rock and sand) with moisture in the state of saturated water and dry surface (saturated surface dry). B. Weighing rock size up to 6.0 mm, volume equal to 1110 kg / m3. And 300 kg of cement per cubic meter Put into the concrete mixer Then turn on the machine at a speed of 20 rpm to mix the stone and sand and cement homogeneous in the mixer for 1 minute. C. When the cement, sand and stone are mixed well. To weigh 75 kg of fly ash per cubic meter and then add all the water. However, while adding water, turn on the concrete mixer to allow the added water. Goes well with sand and cement mixture for 25 s. D. When the added water is mixed well with sand, stone and cement. Therefore began to add concrete admixture volume 1.975 liters per cubic meter Ready to turn on the concrete mixer so that the added solution is compatible with Mixing concrete for 30 seconds, then the mixing process is completed. 2. The production process of the ready-mixed concrete, waterproofing pump type according to claim 1, where Portland cement type 1 contains the chemical composition by weight consisting of aluminum oxide. (Al2O3) 4.35% Silicon Dioxide (SiO2) 20.10% Potassium Oxide (K2O) 0.63% Calcium Oxide (CaO) 62.32% Titanium Dioxide (TiO2) 0.23% Iron Oxide (Fe2O3) 3.24% and has The percentage of weight loss due to burning was 1.71% while having physical properties. Including The average size was 623.8 micrometers, the specific surface area was 472 square meters per kilogram, the specific gravity was 3.10 and the moisture content of 0.12 percent. 3. The pump-waterproofing ready-mixed concrete under claim 1 or 2 was as follows: The amount of cement is 300 kg / m3. Fly ash content is 75 kg / m3. The amount of water mixed with concrete is 140 kilograms per cubic meter. The amount of sand is 855 kg per cubic meter. The maximum size of stone is 6.0 mm. Is equal to 1110 kg / m3. The volume of concrete admixture is 1.975 liters per cubic meter. -------------------------------------------------- -------------------------------------------------- Edit 05/01/2017 1. The production process of ready-mixed concrete with waterproof pumping has the following steps: a. Prepare a concrete mixer that is clean inside and the inside surface is wet (Not completely dry) and aggregate (rock and sand) with moisture in the state of saturated water and dry surface (saturated surface dry). B. Weighing rock size up to 6.0 mm, volume equal to 1110 kg / m3. And 300 kg of cement per cubic meter Put into the concrete mixer Then turn on the machine at a speed of 20 rpm to mix the stone and sand and cement homogeneous in the mixer for 1 minute. C. When the cement, sand and stone are mixed well. To weigh 75 kg of fly ash per cubic meter and then add all the water. However, while adding water, turn on the concrete mixer to allow the added water. Goes well with sand and cement mixture for 25 s. D. When the added water is mixed well with sand, stone and cement. Therefore began to add concrete admixture volume 1.975 liters per cubic meter Ready to turn on the concrete mixer so that the added solution is compatible with Mixing concrete for 30 seconds, then the mixing process is completed. 2. The production process of the ready-mixed concrete, waterproofing pump type according to claim 1, where Portland cement type 1 contains the chemical composition by weight consisting of aluminum oxide. (Al2O3) 4.35% Silicon Dioxide (SiO2) 20.10% Potassium Oxide (K2O) 0.63% Calcium Oxide (CaO) 62.32% Titanium Dioxide (1 02) 0.23% Iron Oxide (Fe2O3) 3.24% And the percentage of weight loss due to burning was 1.71% while the physical properties. Including The average size is 623.8 micrometers, the specific surface area is 472 square meters per kilogram, specific gravity is 3.10 and the moisture content of 0.12%. The amount of cement is 300 kg / m3. The volume of the coop is 75 kilograms per cubic meter. The amount of water mixed with concrete is 140 kilograms per cubic meter. The amount of sand is 855 kilograms per cubic meter, the rock volume is 1110 kilograms per cubic meter. The volume of concrete admixture is 3.975 liters per cubic meter. ------------------------- 1. กรรมวิธีการผลิตคอนกรีตผสมเสร็จมีขั้นตอนดังนี้ ก. เตรียมเครื่องผสมคอนกรีตที่ภายในมีความสะอาดและที่ผิวภายในมีความชุ่มน้ำ (ไม่แห้งสนิท) และ มวลรวม (หินและทราย) ที่มีความชื้นอยู่ในสภาวะอิ่มตัวด้วยน้ำผละผิวแห้ง (saturated surface dry) ข. ชั่งหินขนาดโตสุด 6.0 มิลลิเมตร ปริมาณเท่ากับ 1110 กิโลกรัมต่อลูกบาศก์เมตร และปูนซีเมนต์ 300 กิโลกรัมต่อลูกบาสเมตร ใส่ลงในเครื่องผสมคอนกรีต จากนั้นจึงเปิดเครื่องด้วยความเร็วรอบ 20 รอบ ต่อนาที เพื่อผสมให้หินและทรายและปูนซีเมนต์คลุกเคล้าเป็นเนื้อเดียวกันในเครื่องผสม เป็นเวลา 1 นาที ค. เมื่อปุนซีเมนต์ ทรายและหิน คลุกเคล้าเข้ากันดีแล้ว ให้ทำการชั่งเถ้าลอยในปริมาณ 75 กิโลกรัมต่อ ลูกบาศก์เมตร แล้วจึงเติมน้ำทั้งหมด ทั้งนี้ระหว่างเติมน้ำให้เปิดเครื่องผสมคอนกรีตเพื่อให้น้ำที่เติมลงไป เข้ากันได้ดีกับส่วนผสมของทรายและปูนซีเมนต์เป็นเวลา 25 วินาที ง. เมื่อน้ำที่เติมลงผสมเข้ากันดีแล้วกับทราย หิน และปูนซีเมนต์ จึงเริ่มเติมน้ำยาผสมคอนกรีต ปรืมาณ 1.975 ลิตรต่อลูกบาศก์เมตร พร้อมเปิดเครื่องผสมคอนกรีตเพื่อให้น้ำยาที่เติมลงไปเข้ากันได้ดีกับ ส่วนผสมของคอนกรีตเป็นเวลา 30 วินาที จึงเสร็จสิ้นกระบวนการผสม1. The production process of ready-mixed concrete has the following steps: a. Prepare a concrete mixer that is clean inside and that the inside surface is wet (Not completely dry) and aggregates (rock and sand) with moisture in a state saturated with water and dry surface (saturated surface dry). B. Weigh rock size up to 6.0 mm, volume equal to 1110 kg per cubic meter. And 300 kg of cement per ball. Put into the concrete mixer Then turn on the machine at a speed of 20 rpm to mix the stone and sand and cement homogeneous in the mixer for 1 minute. C. When the mortar, cement, sand and stone are mixed well. To weigh 75 kg of fly ash per cubic meter and then add all the water. However, while adding water, turn on the concrete mixer to allow the added water. Goes well with sand and cement mixture for 25 sec. D. When the added water is mixed well with sand, stone and cement. Therefore began to add concrete admixture at 1.975 liters per cubic meter Ready to turn on the concrete mixer to make the added solution compatible with Concrete mixture for 30 seconds to complete the mixing process. 2. กรรมวิธีการผลิตคอนกรีตผสมเสร็จตามข้อถือสิทธิที่ 1 ที่ศึ่งปูนซีเมนต์ปอร์ตแลนด์ประเภทที่ 1 มีปริมาณ องคื์ประกอบเคมีโดยน้ำหนัก ประกอบไปด้วย อะละมิเนียมออกไซด์ (Al2O3) ร้อลละ 4.35 ซิลิคอนได ออกไซด์ (SiO2) ร้อยละ 20.10 โพแทสเซียมออกไซด์ (K2O) ร้อยละ 0.63 แคลเซียมออกไซด์ (CaO) ร้อลละ 62.32 ไทเทเนียมไดออกไซด์ (TiO2) ร้อยละ 0.23 เหล็กออกไซด์ (Fe2O3) ร้อลละ 3.24 และมีค่า ร้อลละการสูญเสียน้ำหนักเนื่งจากการเผาไหม้ร้อยละ 1.71 ในขณะที่มีสมบัติทางกายภาพอันประกอบไป ด้วย ขนาดเฉลี่ยเท่ากับ 623.8 ไมโคลเมตร พื้นที่ผิวจำเพาะเท่ากับ 472 ตารางเมตรต่อกิโลกรัม ความถ่วงจำเพาะเท่ากับ 3.10 ปละปิมาณความชื้นร้อยละ 0.122. Production process for ready-mixed concrete according to claim No. 1, in Portland Cement Type 1, there are chemical compositions by weight, consisting of Al-Aluminum Oxide (Al2O3) and 4.35 Silicon Dioxide ( 20.10% SiO2, 0.63% potassium oxide (K2O), 62.32% calcium oxide (CaO), 0.23% titanium dioxide (TiO2), 3.24% iron oxide (Fe2O3) and 3.24% percentage. Loss of weight due to combustion of 1.71% while having physical properties comprising average size of 623.8 μm, specific surface area of 472 sq m / kg. Specific gravity is 3.10 ypp. At 0.12% moisture. 3. สูตรสัดส่วนผสมคอนกรีตตามข้อถือสิทธิที่ 1 และ 2 มีดังต่อไปนี้ ปรมาณปูนซีเมนต์เท่ากับ 300 กิโลกรัมต่อลูกบาศก์เมตร ปรมาณเถ้าลอยเท่ากับ 75 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณน้ำผสมคอนกรีตเท่ากับ 140 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณทรายเท่ากับ 855 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณหิน เท่ากับ 1110 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณน้ำยาผสมคอนกรีตเท่ากับ 1.975 ลิตรต่อลูกบาศก์เมตร3. The concrete mix proportion formula according to claim 1 and 2 are as follows. The amount of cement is 300 kilograms per cubic meter. The amount of fly ash is 75 kilograms per cubic meter. The amount of water mixed with concrete is 140 kilograms per cubic meter. The amount of sand is 855 kilograms per cubic meter, the rock volume is 1110 kilograms per cubic meter. The volume of concrete admixture is 1.975 liters per cubic meter.
TH1603001340U 2016-08-01 The production process of ready-mixed concrete, pump-type waterproofing TH14252A3 (en)