A method involves tempering of blanks from the intercritical temperatures interval of As1-As3, cold forming of threading and tempering. Tempering is carried out from the temperature by 50-70°C exceeding Curie point of blank material at a cooling rate of 45-70°, degrees/s.
UA4422647A1988-04-041988-04-04METHOD For production of strengthening threaded articles from mild steel