ES2063494T3 - Metodo de tratamiento superficial para botes estañados estirados y prensados. - Google Patents
Metodo de tratamiento superficial para botes estañados estirados y prensados.Info
- Publication number
- ES2063494T3 ES2063494T3 ES91903769T ES91903769T ES2063494T3 ES 2063494 T3 ES2063494 T3 ES 2063494T3 ES 91903769 T ES91903769 T ES 91903769T ES 91903769 T ES91903769 T ES 91903769T ES 2063494 T3 ES2063494 T3 ES 2063494T3
- Authority
- ES
- Spain
- Prior art keywords
- comprehensive
- cast
- xey
- general formula
- sprayed
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
SE PUEDE OBTENER UNA SUPERFICIE QUE TIENE UNA EXCELENTE ADHESIVIDAD A LA PINTURA, BUENA RESISTENCIA A LA CORROSION Y BAJA FRICCION EN ENVASES FUNDIDOS ESTAÑADOS Y FORRADOS DE HIERRO PULVERIZANDO LA SUPERFICIE DEL ENVASE DURANTE UN PERIODO DE TIEMPO COMPRENDIDO ENTRE 5 Y 60 SEGUNDOS A UNA TEMPERATURA COMPRENDIDA ENTRE 40 Y 60 (GRADOS) C CON UN LIQUIDO TRATANTE ACUOSO QUE TIENE UN PH ENTRE 4 Y 6 Y QUE COMPRENDE (I) ACIDO ORTOFOSFORICO Y/O ACIDOS FOSFORICOS CONDENSADOS Y (II) UNA CONCENTRACION DE, AL MENOS, 0,1 SIN UN OLIGOMERO SOLUBLE EN AGUA CON LA FORMULA GENERAL (I) EN DONDE N ES UN NUMERO CON UN VALOR ENTRE 10 Y 30 Y CADA X E Y REPRESENTA INDEPENDIENTEMENTE HIDROGENO O UN GRUPO Z, EN DONDE Z TIENE UNA COMPOSICION QUIMICA SEGUN LA FORMULA GENERAL (II) EN DONDE CADA R1 Y R2 ES UN ALQUILO O GRUPO HIDROXIALQUILO QUE TIENE DE 1 A 5 ATOMOS DE CARBONO, SALVO QUE, AL MENOS, EL 25% DEL TOTAL DE TODOS LOS GRUPOS X E Y DEL OLIGOMERO SON Z EN LUGAR DE HIDROGENO; Y SECANDO LA SUPERFICIE ASI PULVERIZADA, OPCIONALMENTE DESPUES DE HABER ACLARADO, EN PRIMER LUGAR, LA SUPERFICIE PULVERIZADA CON AGUA.
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP320090A JPH03207766A (ja) | 1990-01-10 | 1990-01-10 | ぶりきdi缶の表面処理方法 |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| ES2063494T3 true ES2063494T3 (es) | 1995-01-01 |
Family
ID=11550787
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| ES91903769T Expired - Lifetime ES2063494T3 (es) | 1990-01-10 | 1991-01-10 | Metodo de tratamiento superficial para botes estañados estirados y prensados. |
Country Status (8)
| Country | Link |
|---|---|
| EP (1) | EP0510105B1 (es) |
| JP (1) | JPH03207766A (es) |
| AU (1) | AU642468B2 (es) |
| BR (1) | BR9105932A (es) |
| CA (1) | CA2072258A1 (es) |
| DE (1) | DE69104825T2 (es) |
| ES (1) | ES2063494T3 (es) |
| WO (1) | WO1991010756A1 (es) |
Families Citing this family (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO1991019828A1 (en) * | 1990-06-19 | 1991-12-26 | Henkel Corporation | Liquid composition and process for treating aluminium or tin cans to impart corrosion resistance and reduced friction coefficient |
| JPH04187782A (ja) * | 1990-11-21 | 1992-07-06 | Nippon Parkerizing Co Ltd | ぶりきdi缶用表面処理液 |
| JP2771110B2 (ja) * | 1994-04-15 | 1998-07-02 | 日本パーカライジング株式会社 | アルミニウム含有金属材料用表面処理組成物および表面処理方法 |
| CA2226524A1 (en) * | 1995-07-10 | 1997-01-30 | Toshiaki Shimakura | Metal surface treatment agent and method and metallic materials treated with the same |
| JP3544761B2 (ja) * | 1995-10-13 | 2004-07-21 | 日本パーカライジング株式会社 | アルミニウム含有金属材料用表面処理組成物および表面処理方法 |
Family Cites Families (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| GB2112409B (en) * | 1981-12-22 | 1985-07-03 | Pyrene Chemical Services Ltd | Phenolic compounds and their use in metal finishing processes |
| US4433015A (en) * | 1982-04-07 | 1984-02-21 | Parker Chemical Company | Treatment of metal with derivative of poly-4-vinylphenol |
| US4457790A (en) * | 1983-05-09 | 1984-07-03 | Parker Chemical Company | Treatment of metal with group IV B metal ion and derivative of polyalkenylphenol |
| HU29370A (es) * | 1983-08-29 |
-
1990
- 1990-01-10 JP JP320090A patent/JPH03207766A/ja active Pending
-
1991
- 1991-01-10 EP EP91903769A patent/EP0510105B1/en not_active Expired - Lifetime
- 1991-01-10 WO PCT/US1991/000202 patent/WO1991010756A1/en not_active Ceased
- 1991-01-10 AU AU72243/91A patent/AU642468B2/en not_active Ceased
- 1991-01-10 ES ES91903769T patent/ES2063494T3/es not_active Expired - Lifetime
- 1991-01-10 BR BR919105932A patent/BR9105932A/pt not_active IP Right Cessation
- 1991-01-10 CA CA002072258A patent/CA2072258A1/en not_active Abandoned
- 1991-01-10 DE DE69104825T patent/DE69104825T2/de not_active Expired - Fee Related
Also Published As
| Publication number | Publication date |
|---|---|
| EP0510105B1 (en) | 1994-10-26 |
| EP0510105A1 (en) | 1992-10-28 |
| CA2072258A1 (en) | 1991-07-11 |
| BR9105932A (pt) | 1992-11-24 |
| AU642468B2 (en) | 1993-10-21 |
| JPH03207766A (ja) | 1991-09-11 |
| DE69104825D1 (de) | 1994-12-01 |
| AU7224391A (en) | 1991-08-05 |
| WO1991010756A1 (en) | 1991-07-25 |
| DE69104825T2 (de) | 1995-05-24 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| ES8609507A1 (es) | "un metodo para inhibir la corrosion de superficies metali- cas en agua en un sistema acuoso" | |
| GB2080835B (en) | Prevention of sludge in phosphating baths | |
| ES2063494T3 (es) | Metodo de tratamiento superficial para botes estañados estirados y prensados. | |
| US4010111A (en) | Corrosion inhibitor used in brines containing oxygen | |
| DE3869605D1 (de) | Reaktives desodorierungsmittel mit korrosionsinhibierender aktivitaet. | |
| ES8604982A1 (es) | Una composicion que contiene una sal preparada por reaccion de (a) por lo menos un compuesto de un acido ditiofosforado | |
| ES530624A0 (es) | Un procedimiento para el recubrimiento de articulos ferrosos. | |
| JPS54146238A (en) | Phosphonate corrosion preventive agent | |
| MX9400176A (es) | Metodo y composicion para inhibir la corrosion de metales empleando acidos politartaricos. | |
| GB928259A (en) | Pickling bath for stainless steel | |
| GB1003705A (en) | Process for the after-treatment of phosphate coatings | |
| FI831181L (fi) | Mikroinkapslingsfoerfarande | |
| JPS5739177A (en) | Water soluble rust-resisting agent | |
| ES406358A1 (es) | Procedimiento para el pelado de frutos. | |
| Larkworthy | 670. Nitrosation, diazotisation, and deamination. Part VIII. The diazotisation of weakly basic amines in dilute perchloric acid | |
| JPS57185991A (en) | Corrosion inhibitor for stainless steel | |
| FR2158664A5 (en) | Metal surface treatment baths - additive - for addition to hydrochloric and sulphuric acid based baths | |
| Natarajan et al. | Corrosion Behaviour of Steels Used in Boiler Plants | |
| GB927576A (en) | Improvements relating to the coating of metals | |
| Vyazovoi et al. | An Industrial Study of the Anticorrosion Action of Additions(Oksidin M) to a Sulphur Mazut | |
| GB1449826A (en) | Inhibition of corrosion | |
| JPS558487A (en) | Surface treating method of copper | |
| Banas et al. | STEEL CORROSION IN GEOTHERMAL WATERS(Polish) | |
| JPS5558356A (en) | One side metal hot dipping process | |
| SU751173A1 (ru) | Способ консервации парогенератора |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| FG2A | Definitive protection |
Ref document number: 510105 Country of ref document: ES |