JPH03188628A - Pattern forming method - Google Patents

Pattern forming method

Info

Publication number
JPH03188628A
JPH03188628A JP32933189A JP32933189A JPH03188628A JP H03188628 A JPH03188628 A JP H03188628A JP 32933189 A JP32933189 A JP 32933189A JP 32933189 A JP32933189 A JP 32933189A JP H03188628 A JPH03188628 A JP H03188628A
Authority
JP
Japan
Prior art keywords
film
etching
resist
pattern
forming method
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Ceased
Application number
JP32933189A
Other languages
Japanese (ja)
Inventor
Kazuya Kamon
和也 加門
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Mitsubishi Electric Corp
Original Assignee
Mitsubishi Electric Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Mitsubishi Electric Corp filed Critical Mitsubishi Electric Corp
Priority to JP32933189A priority Critical patent/JPH03188628A/en
Publication of JPH03188628A publication Critical patent/JPH03188628A/en
Ceased legal-status Critical Current

Abstract

(57)【要約】本公報は電子出願前の出願データであるた
め要約のデータは記録されません。
(57) [Summary] This bulletin contains application data before electronic filing, so abstract data is not recorded.

Description

【発明の詳細な説明】 〔産業上の利用分野〕 本発明は、LSI 等の半導体デバイス製造プロセスに
おける光リソグラフィー工程で使用されるパターン形成
方法に関し、特に配線パターンの形成方法に関するもの
である。
DETAILED DESCRIPTION OF THE INVENTION [Field of Industrial Application] The present invention relates to a pattern forming method used in a photolithography step in the manufacturing process of semiconductor devices such as LSI, and particularly to a method of forming a wiring pattern.

〔従来の技術〕[Conventional technology]

従来、LSI 製造プロセスにおいて用いられているこ
の種のパターン形成方法を第2図を参照して説明する。
This type of pattern forming method conventionally used in the LSI manufacturing process will be explained with reference to FIG.

これは、その概略プロセスを第2図に示すように、S’
(シリコン)基板1上にAt(アルミ)膜2′f:蒸着
して、さらにレジスト膜3を塗布する(同図(a))。
As the schematic process is shown in Figure 2, S'
An At (aluminum) film 2'f is deposited on the (silicon) substrate 1, and then a resist film 3 is applied (FIG. 4(a)).

そして、この表面に所定の放射線11を照射して選択的
に露光し、その露光部12を形成した後(同図(b) 
) 、現像を行ってレジストパターン3a k形成する
(同図(C))。次いでこのレジストパターン3aをマ
スクにして、んt膜2のエツチングを行った後(同図(
d) ) 、レジストパターン3aを除去することによ
り、同図(e)に示すAtの配線パターン13を形成す
るものとなっている。
Then, this surface is selectively exposed by irradiating a predetermined radiation 11 to form an exposed portion 12 (see FIG. 1(b)).
), development is performed to form a resist pattern 3a k (FIG. 3(C)). Next, using the resist pattern 3a as a mask, the etching film 2 is etched (see FIG.
d)) By removing the resist pattern 3a, the At wiring pattern 13 shown in FIG. 3(e) is formed.

〔発明が解決しようとする課題〕[Problem to be solved by the invention]

しかし、このような従来のパターン形成方法では、露光
装置の解像力によって最小パターンが決まってしまい、
それ以下のパターンは形成できないという問題点があっ
た。
However, in such conventional pattern forming methods, the minimum pattern is determined by the resolution of the exposure device.
There was a problem that patterns smaller than this could not be formed.

本発明は上記のような問題点を解消するために々された
もので、従来よシも微細なパターンを形成できるパター
ン形成方法を提供することを目的とする。
The present invention has been made to solve the above-mentioned problems, and it is an object of the present invention to provide a pattern forming method that can form finer patterns than ever before.

〔線題を解決するための手段〕[Means for solving line problems]

本発明に係るパターン形成方法は、半導体基板上に金属
膜とレジスト膜を形成する工程と、前記レジスト膜を露
光し現像してパター;ングする工程と、このパターニン
グし次レジスト膜をマスクにして前記金属膜をエツチン
グするとともに、そのレジスト側壁にエツチング堆積物
を生成させる工程と、前記レジスト膜を除去してそれに
覆われ念前記金属膜を露出させる工程と、前記エツチン
グ堆積物をマスクにして前記金属膜を再びエツチングす
る工程と、このエツチング堆積物を水洗により除去する
工程とを備えている。
The pattern forming method according to the present invention includes a step of forming a metal film and a resist film on a semiconductor substrate, a step of exposing and developing the resist film for patterning, and a step of patterning and then using the resist film as a mask. a step of etching the metal film and generating an etching deposit on the resist sidewall; a step of removing the resist film to expose the metal film covered by it; and a step of etching the etching deposit using the etching deposit as a mask. The method includes a step of etching the metal film again and a step of removing this etching deposit by washing with water.

〔作 用〕[For production]

本発明においては、エツチング時に生じるレジスト側壁
に生成されるエツチング堆積物をマスクにしてパターニ
ングしているので、露光装置の解像力よりも小さいパタ
ーンが形成される。
In the present invention, since patterning is performed using etching deposits generated on the side walls of the resist during etching as a mask, a pattern smaller than the resolution of the exposure apparatus is formed.

〔実施例〕〔Example〕

以下、本発明の実施例を第1図を参照して説明する。第
1図(a)〜(e)は本発明によるパターン形成方法の
一実施例を示す概略の工程断面図である。
Embodiments of the present invention will be described below with reference to FIG. FIGS. 1(a) to 1(e) are schematic cross-sectional views showing an embodiment of the pattern forming method according to the present invention.

第1図において第2図と同一の部分には同一の符号を付
してあシ、4は第1のアルミエツチング時に生成しレジ
スト側壁に堆積するAtct8膜、6は第2のアルミエ
ツチングに生成し側壁に堆積するhtct8 膜である
。
In Fig. 1, the same parts as in Fig. 2 are given the same reference numerals, 4 is the Atct8 film produced during the first aluminum etching and deposited on the resist sidewall, and 6 is the Atct8 film produced during the second aluminum etching. htct8 film deposited on the sidewalls.

すなわちこの実施例は、第1図に示すように、まずSt
基板1上にU膜2.レジスト膜3を順次形成し念のち、
このレジスト膜3を露光し現像してパターニングする(
同図(&))。次いで、このパターニングされ次レジス
ト膜つまジレジストハターン3aをマスクにして、エツ
チングガスBCt8+CZ、によシAt膜2をエツチン
グする(同図(b))。
That is, in this embodiment, as shown in FIG.
A U film 2 on the substrate 1. After sequentially forming the resist film 3,
This resist film 3 is exposed, developed, and patterned (
Same figure(&)). Next, using the patterned resist film 3a as a mask, the At film 2 is etched with an etching gas BCt8+CZ (FIG. 4(b)).

この時、そのレジスト側壁にはhtct8 膜4がエツ
チング堆積物として堆積する。次に、CF、処理により
Atct8 膜4のCtをFに置換してAtF8膜5を
形成し、しかる後レジスト3を除去する(同図(C))
。次いでこのAtF8膜5をマスクにして、再びAt膜
2をエツチングガスBCl34−C1゜によシエッチン
グする(同図(d))。この時、んグ。
At this time, the htct8 film 4 is deposited as an etching deposit on the side walls of the resist. Next, Ct of the Atct8 film 4 is replaced with F by CF treatment to form an AtF8 film 5, and then the resist 3 is removed ((C) in the same figure).
. Next, using this AtF8 film 5 as a mask, the At film 2 is etched again with etching gas BCl34-C1° (FIG. 4(d)). At this time, ng.

膜5には再び*tct8 が堆積して、Atct8膜6
が生成される。次に、CF、処理により htct8 
膜6のCtをFに置換してAlF2膜を形成した後、そ
のAlF2膜を水処理により除去することにより(同図
(e) ) 、同図(&)にみられるパターン3aに比
べて、半分の微小パターンつま、QAtの配線パターン
Tを形成することができる。
*tct8 is deposited on the film 5 again, forming the Atct8 film 6.
is generated. Next, by CF, processing htct8
By replacing Ct in the film 6 with F to form an AlF2 film, and then removing the AlF2 film by water treatment ((e) in the same figure), compared to pattern 3a seen in (&) in the same figure, It is possible to form a wiring pattern T of half the minute pattern, that is, QAt.

なお、上記実施例ではAt配線について述べたが、鉄な
ど他の金属配線でもよい。
Note that although At wiring was described in the above embodiment, other metal wiring such as iron may also be used.

〔発明の効果〕〔Effect of the invention〕

以上のように本発明によれば、エツチングに伴う堆積物
を利用してパターニングするので、露光装置の解像力よ
りも%小さいパターンが形成できる効果がある。
As described above, according to the present invention, since patterning is performed using deposits accompanying etching, it is possible to form a pattern that is % smaller than the resolution of the exposure apparatus.

【図面の簡単な説明】[Brief explanation of drawings]

第1図(、)〜(・)は本発明によるパターン形成方法
の一実施例を示す工程断面図、第2図(a)〜(a)は
従来のパターン形成方法の一例を示す工程断面図である
。 1・・・・St基板、2・・・・At膜、3・・  ・
レジストMl’、3m  ・・・・レジストパターン、
4,6・・・・htct8 膜、5・ ・・・Aぴ。 膜、7・・・・配線パターン。
Figures 1 (,) to (•) are process cross-sectional views showing an example of the pattern forming method according to the present invention, and Figures 2 (a) to (a) are process cross-sectional views showing an example of the conventional pattern forming method. It is. 1... St substrate, 2... At film, 3... ・
Resist Ml', 3m...Resist pattern,
4,6...htct8 membrane, 5...Api. Membrane, 7... Wiring pattern.

Claims (1)

【特許請求の範囲】[Claims] 半導体基板上に金属膜とレジスト膜を形成する工程と、
前記レジスト膜を露光し現像してパターニングする工程
と、このパターニングしたレジスト膜をマスクにして前
記金属膜をエッチングするとともに、そのレジスト側壁
にエッチング堆積物を生成させる工程と、前記レジスト
膜を除去してそれに覆われた前記金属膜を露出させる工
程と、前記エッチング堆積物をマスクにして前記金属膜
を再びエッチングする工程と、このエッチング堆積物を
水洗により除去する工程とを備えることを特徴とするパ
ターン形成方法。
a step of forming a metal film and a resist film on the semiconductor substrate;
a step of exposing and developing the resist film to pattern it; a step of etching the metal film using the patterned resist film as a mask and generating etching deposits on the side walls of the resist; and a step of removing the resist film. The method is characterized by comprising the steps of exposing the metal film covered with the metal film, etching the metal film again using the etching deposit as a mask, and removing the etching deposit by washing with water. Pattern formation method.
JP32933189A 1989-12-18 1989-12-18 Pattern forming method Ceased JPH03188628A (en)